Microstructure and Thermodynamic Analysis of Ti-Nb-Cr-C Doped Molybdenum Alloy AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The Ti-Nb-Cr-C doped molybdenum alloy was prepared by powder metallurgy, and its microstructure, particle size and composition were analyzed. Thermodynamics was discussed of oxide generation during ball milling and carbide formation during sintering. The results show that the second phase particles are mainly distributed on the grain boundary, and also distributed inside the grain when Nb content is eno- ugh. The second phase mainly contains Nb,Ti and C,possibly being composite carbides of Nb and Ti based on the thermodynamics analysis. The second phase particles can refine the grains of molybdenum alloy, and the effect of grain refinement is strongest with Nb content of 3 %. Cr exists in molybdenum alloy mainly in the form of solid solution.

KeyWords AITranslate

molybdenum alloy Ti-Nb-Cr-C doping carbide the second phase particle morphology thermodynamics

1冯鹏发,孙军.钼及钼合金粉末冶金技术研究现状与发展[J].中国钼业,2010,34(3):39-45. 被引量:25

2卢明园,范静莲,成会朝,等.微量合金元素Ti、zr对Mo合金性能和显微组织的影响[J].稀有金属材料与工程,20lO,39(6):985-988.

3GB/T6394-2002.金属平均晶粒度测定方法[S].[S].,..

4梁静,奚正平,汤慧萍,李来平.TZM合金中碳化物生成机制分析[J].稀有金属材料与工程,2011,40(S2):210-214. 被引量:3

5朱心昆,赵昆渝,程抱昌,林秋实,张修庆,陈铁力,苏云生,雍岐龙.高能球磨制备纳米TiC粉末[J].中国有色金属学报,2001,11(2):269-272. 被引量:10

1谢瑞广,李长久,崔红.基于冷喷涂制备ZrC掺杂NiAl热障涂层粘结层[J].表面技术,2016,45(10):1-6. 被引量:4

2王彦峰,李争显,华云峰,王宝云,杜继红.C掺杂方式对TiAlSiN膜层组织及性能的影响[J].表面技术,2013,42(4):32-34. 被引量:7

3韩宁,马春伟,侯雪玲,徐培全,贾涵浩,薛允.C掺杂对La-Fe-Si合金中NaZn_(13)型相形成及磁热性能的影响[J].材料导报,2016,30(8):104-108. 被引量:1

4王彦峰,李争显,杜继红,王宝云.C掺杂硬质膜层的组织及性能研究[J].稀有金属材料与工程,2012,41(S2):178-181.

5刘国庆,熊晓梅,王庆阳,闫果,刘春芳,卢亚锋,杨烨,蒲明华,赵勇.C掺杂对MgB_2超导体水解行为的影响[J].稀有金属材料与工程,2007,36(7):1291-1294. 被引量:1

6谢瑞广,李长久,崔红.冷喷涂制备ZrC改性NiAl粘结层的高温氧化行为[J].材料导报,2016,30(12):6-9. 被引量:2

7Chao Yuan,Ji-heng Li,Wen-lan Zhang,Xiao-qian Bao,Xue-xu Gao.Microstructure and magnetostrictive performance of NbC-doped <100>oriented Fe-Ga alloys[J].矿物冶金与材料学报:英文版,2015,0(1):52-58.

8孙昱艳,张平祥,白质明,陈思华.无定形C掺杂对MgB_2微结构和超导电性的影响[J].东北大学学报:自然科学版,2010,31(8):1153-1156.

9向鑫,陈长安,蒋春丽.XRD研究Fe、C掺杂对He离子注入Al表面晶格畸变的影响[J].稀有金属材料与工程,2011,40(9):1610-1615. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]

Citation Information:

The Ti-Nb-Cr-C doped molybdenum alloy was prepared by powder metallurgy, and its microstructure, particle size and composition were analyzed. Thermodynamics was discussed of oxide generation during ball milling and carbide formation during sintering. The results show that the second phase particles are mainly distributed on the grain boundary, and also distributed inside the grain when Nb content is eno- ugh. The second phase mainly contains Nb,Ti and C,possibly being composite carbides of Nb and Ti based on the thermodynamics analysis. The second phase particles can refine the grains of molybdenum alloy, and the effect of grain refinement is strongest with Nb content of 3 %. Cr exists in molybdenum alloy mainly in the form of solid solution.

quote

GB/T 7714-2015 [1] ZHANG Pan-long, NI Feng, ZHAO Jing-jing, et al. Microstructure and Thermodynamic Analysis of Ti-Nb-Cr-C Doped Molybdenum Alloy[J]. Rare Metals and Cemented Carbides, 2013(5): 19-24.
MLA [1] ZHANG Pan-long, et al., "Microstructure and Thermodynamic Analysis of Ti-Nb-Cr-C Doped Molybdenum Alloy." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 19-24.
APA [1] ZHANG Pan-long, NI Feng, ZHAO Jing-jing, XU Liu-jie, & WEI Shi-zhong. (2013). Microstructure and Thermodynamic Analysis of Ti-Nb-Cr-C Doped Molybdenum Alloy. Rare Metals and Cemented Carbides(5), 19-24.
IEEE [1] ZHANG Pan-long, NI Feng, ZHAO Jing-jing, XU Liu-jie, and WEI Shi-zhong, "Microstructure and Thermodynamic Analysis of Ti-Nb-Cr-C Doped Molybdenum Alloy," Rare Metals and Cemented Carbides, no. 5, pp. 19-24, 2013. keywords: {molybdenum alloy;Ti-Nb-Cr-C doping;carbide;the second phase particle;morphology;thermodynamics}