Influences of Particle Size and Single Sample Weight of W Powders on the Properties of W-10Cu Composite Materials for Electronic Packing AITranslate

13th Research Institute of China Electronic Technology Group Corporation;13th Research Institute of China Electronic Technology Group Corporation;13th Research Institute of China Electronic Technology Group Corporation;13th Research Institute of China Electronic Technology Group Corporation
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Abstraet..W-10Cu composite materials were prepared by high velocity compaction-cold forging-copper infil tration. Meanwhile,investigation was made on the influences of particle size and single sample weight of W powders on the microstructure and properties of the materials. The results show that the relative density of W skeleton decreases with the increase of single sample weight before and after cold forging. Upon compaction of the mixed powders,W skeleton has the greatest relative density,yet it is not satisfactory to W-10Cu composite material,of which the relative density should be no less than 81%. By cold forging,the maximum relative density of all the types o{ W skeletons can reach 81%, and among them W skeleton com- pacted with medium-grained powders has the greatest relative density. The W-10Cu composite materials with dense and uniform microstructure can be prepared by high velocity compaction-cold forging-copper in- filtration with three types of powders and they can also meet the performance requirement for electronic packaging materials. Keywords : W-10Cu ; W powders ; particle size; single sample weight; W skeleton; electronic packing

KeyWords AITranslate

W-10Cu W powders particle size single sample weight W skeleton electronic packing

1黄强,顾明元,金燕萍.电子封装材料的研究现状[J].材料导报,2000,14(9):28-32. 被引量:59

2童志义.高密度封装技术现状及发展趋势[J].电子工业专用设备,2000,29(2):1-9. 被引量:14

3陶应启,王祖平,方宁象,吴仲春.钨铜复合材料的制造工艺[J].粉末冶金技术,2002,20(1):49-51. 被引量:34

4Carl Zweben. Advances in composite materials or thermal management in electronic packaging[J]. JOM, 1998,50(6) : 47-51.

5Sethi G, Hauck E, German R M. High velocity compaction compared with conventional compaction [J]. Materials Science and Technology, 2006,22 (8) 955-959.

6王志法,姜国圣,刘正春.钨的超高压成型与低温烧结[J].稀有金属材料与工程,1998,27(5):290-293. 被引量:13

1郑锋.几种金属元素对W粉粒度的影响[J].硬质合金,1995,12(3):143-145. 被引量:10

2张棉绒,李均明.W粉粒度对CuW/Cu整体触头结合强度的影响[J].热加工工艺,2005,34(10):18-18. 被引量:3

3王庆相,梁淑华,杨怡,范志康.W粉粒度对Ti-20%W合金组织和力学性能的影响[J].粉末冶金技术,2010,28(1):26-30. 被引量:7

4阳冬元,周春成.W粉球磨时间对W粉、WC粉及其制备的合金性能的影响[J].硬质合金,2016,33(5):322-328. 被引量:2

5谷成玲.粉末高速压制成形坯孔隙度的分形研究[J].煤矿机械,2013,34(4):62-63.

6郑玉凯,蔡一湘,陈峰,闫志巧,罗兵辉.烧结温度对10TiB/Ti-4.5Al-6.8Mo-1.5Fe复合材料组织与性能的影响[J].粉末冶金材料科学与工程,2013,18(4):546-551.

7郑洲顺,王爽,郑珊,曲选辉.基于离散单元法的粉末高速压制流动过程模拟[J].稀有金属材料与工程,2010,39(12):2132-2136. 被引量:15

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

Abstraet..W-10Cu composite materials were prepared by high velocity compaction-cold forging-copper infil tration. Meanwhile,investigation was made on the influences of particle size and single sample weight of W powders on the microstructure and properties of the materials. The results show that the relative density of W skeleton decreases with the increase of single sample weight before and after cold forging. Upon compaction of the mixed powders,W skeleton has the greatest relative density,yet it is not satisfactory to W-10Cu composite material,of which the relative density should be no less than 81%. By cold forging,the maximum relative density of all the types o{ W skeletons can reach 81%, and among them W skeleton com- pacted with medium-grained powders has the greatest relative density. The W-10Cu composite materials with dense and uniform microstructure can be prepared by high velocity compaction-cold forging-copper in- filtration with three types of powders and they can also meet the performance requirement for electronic packaging materials. Keywords : W-10Cu ; W powders ; particle size; single sample weight; W skeleton; electronic packing

quote

GB/T 7714-2015 [1] LIU Yong-wang, JIANG Guo-sheng, GU Yi, et al. Influences of Particle Size and Single Sample Weight of W Powders on the Properties of W-10Cu Composite Materials for Electronic Packing[J]. Rare Metals and Cemented Carbides, 2013(5): 32-35.
MLA [1] LIU Yong-wang, et al., "Influences of Particle Size and Single Sample Weight of W Powders on the Properties of W-10Cu Composite Materials for Electronic Packing." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 32-35.
APA [1] LIU Yong-wang, JIANG Guo-sheng, GU Yi, & WANG Zhi-fa. (2013). Influences of Particle Size and Single Sample Weight of W Powders on the Properties of W-10Cu Composite Materials for Electronic Packing. Rare Metals and Cemented Carbides(5), 32-35.
IEEE [1] LIU Yong-wang, JIANG Guo-sheng, GU Yi, and WANG Zhi-fa, "Influences of Particle Size and Single Sample Weight of W Powders on the Properties of W-10Cu Composite Materials for Electronic Packing," Rare Metals and Cemented Carbides, no. 5, pp. 32-35, 2013. keywords: {W-10Cu;W powders;particle size;single sample weight;W skeleton;electronic packing}