Research on Milling Performance of YT-typed Carbide Shaped Tool Coated with Diamond Films for High Volume Fraction SiC_P/Al Composite AITranslate
Abstract AITranslate
Micron diamond film was prepared by hot filament chemical vapor deposition on B212-typed YT15 carbide shaped milling blade,and then milling experiments were performed with 65% SiC particle reinforced aluminum-based composite as the specimen material. Compared with uncoated carbide tool, the coating effect of diamond film coated tool was evaluated. The results show that under the same milling conditions, each milling force of diamond film coated tool is reduced by 50%-65% compared with the uncoated tool. The diamond film exhibits a good adhesion strength on the matrix during milling. The coated tool with acid-alkali pretreatment is more suitable for roughing of the above composite,and the coated tool with alcohol-alkali pretreatment is more suitable for its semi-finishing. Besides, the workpiece surface quality obtained by continuous machining with the coated tool is better and more stable than that with the uncoated tool, and the shaped precision of the groove milled with the coated tool is increased by about 30 % compared with the uncoated tool.
KeyWords AITranslate
1郑喜军,米国发.碳化硅颗粒增强铝基复合材料的研究现状及发展趋势[J].热加工工艺,2011,40(12):92-96. 被引量:52
2孙方宏,陈明,张志明,沈荷生.高性能CVD金刚石薄膜涂层刀具的制备和试验研究[J].机械工程学报,2003,39(7):101-106. 被引量:25
3向道辉.基于内涨鼓泡法定量评价金刚石薄膜综合力学性能理论模型及其实现[D].上海:上海交通大学,2007.
4马志斌,汪建华,王传新.在WC-TiC-Co硬质合金基体上制备金刚石薄膜的试验研究[J].工具技术,2002,36(2):18-20. 被引量:4
5吴震宇,王学根,孙方宏,陈明.SiC颗粒增强铝基复合材料高速铣削工艺研究[J].工具技术,2004,38(3):15-18. 被引量:17
6赵忠,丁仁亮,周而康.金属材料及热处理(第3版)[M].北京:机械工业出版社,2004.
1张而耕,黄彪,陈强.金刚石涂层立铣刀与PCD立铣刀切削铝合金性能研究[J].表面技术,2016,45(5):149-153. 被引量:3
1张而耕,黄彪,周琼.TaC涂层的研究现状及应用[J].陶瓷学报,2017,38(1):8-12. 被引量:6
2张而耕,黄彪,何澄,周琼.新型Ta-C涂层铣刀切削性能研究[J].表面技术,2017,46(6):125-130. 被引量:4
3邵伟平,张韬,彭广盼,薛喆.不同材质刀具在7075铝合金高速铣削中的磨损研究[J].宇航材料工艺,2022,52(5):96-102. 被引量:1
1张晓辉,许幸新,张春林,向道辉,郑友益.YT15硬质合金成形铣刀的金刚石涂层制备及应用研究[J].制造技术与机床,2014(10):107-111. 被引量:2
2许幸新,张晓辉,张春林,郑友益.YT类硬质合金成形铣刀的金刚石涂层工艺研究[J].河南理工大学学报:自然科学版,2014,33(4):472-477. 被引量:2
3许幸新,张晓辉,张春林,郑友益.硬质合金成形铣刀的金刚石涂层热应力分析[J].金刚石与磨料磨具工程,2013,33(5):48-52. 被引量:4
4许幸新,张晓辉,张春林,郑友益.复杂形状硬质合金刀具金刚石涂层的制备及铣削特性研究[J].稀有金属与硬质合金,2014,42(3):63-68. 被引量:1
5牛文莉,马跃林,张永宏,严国英.GLC涂层刀具干切削性能研究[J].陕西理工学院学报:自然科学版,2016,32(1):6-9. 被引量:1
6庄大明,刘家浚,朱宝亮,罗振壁,苗赫濯.陶瓷刀具切削304不锈钢时的磨损性能[J].材料研究学报,1997,11(2):163-168.
7李刚,王扬渝,周浩东.拼接淬硬钢铣削特性有限元模拟[J].工具技术,2014,48(5):24-27.
8阎开印,孟廷会,于军慧.添加稀土元素对硬质合金物理机械性能和切削性能的影响[J].西南交通大学学报,1995,30(1):46-52. 被引量:6
9周铭熙,汤美,于晓见.不铲磨硬质合金成形铣刀[J].机械工人:冷加工,1999(8):12-13.
10高爱华,张建新.硬质合金成形铣刀切削性能的试验研究[J].中国钨业,2004,19(2):37-38.
Basic Information:
DOI:
Chinese Library Classification Number:TG711[金属学及工艺—刀具与模具]
Citation Information:
Micron diamond film was prepared by hot filament chemical vapor deposition on B212-typed YT15 carbide shaped milling blade,and then milling experiments were performed with 65% SiC particle reinforced aluminum-based composite as the specimen material. Compared with uncoated carbide tool, the coating effect of diamond film coated tool was evaluated. The results show that under the same milling conditions, each milling force of diamond film coated tool is reduced by 50%-65% compared with the uncoated tool. The diamond film exhibits a good adhesion strength on the matrix during milling. The coated tool with acid-alkali pretreatment is more suitable for roughing of the above composite,and the coated tool with alcohol-alkali pretreatment is more suitable for its semi-finishing. Besides, the workpiece surface quality obtained by continuous machining with the coated tool is better and more stable than that with the uncoated tool, and the shaped precision of the groove milled with the coated tool is increased by about 30 % compared with the uncoated tool.
quote
| GB/T 7714-2015 | [1] ZHANG Xiao-hui, XU Xing-xin, ZHANG Chun-lin, et al. Research on Milling Performance of YT-typed Carbide Shaped Tool Coated with Diamond Films for High Volume Fraction SiC_P/Al Composite[J]. Rare Metals and Cemented Carbides, 2014(5): 60-64. |
| MLA | [1] ZHANG Xiao-hui, et al., "Research on Milling Performance of YT-typed Carbide Shaped Tool Coated with Diamond Films for High Volume Fraction SiC_P/Al Composite." Rare Metals and Cemented Carbides, no. 5, 2014, pp. 60-64. |
| APA | [1] ZHANG Xiao-hui, XU Xing-xin, ZHANG Chun-lin, XIANG Dao-hui, & ZHENG You-yi. (2014). Research on Milling Performance of YT-typed Carbide Shaped Tool Coated with Diamond Films for High Volume Fraction SiC_P/Al Composite. Rare Metals and Cemented Carbides(5), 60-64. |
| IEEE | [1] ZHANG Xiao-hui, XU Xing-xin, ZHANG Chun-lin, XIANG Dao-hui, and ZHENG You-yi, "Research on Milling Performance of YT-typed Carbide Shaped Tool Coated with Diamond Films for High Volume Fraction SiC_P/Al Composite," Rare Metals and Cemented Carbides, no. 5, pp. 60-64, 2014. keywords: {YT15 carbide sh fraction SiCp/Al composite aped tool;diamond coating;hot filament chemical vapor deposition;high volume;milling performance} |