Determination of Potassium in Tantalum Powder by Flame Atomic Emission Spectrometry AITranslate
Abstract AITranslate
Potassium content in tantalum powder was determined by flame atomic emission spectrometry, the flame conditions were optimized, and the reagent dosages were selected. The detection limit is 2. 375 μg/g of the above method for the potassium content in tantalum powder under the selected conditions,its standard addition recovery rate is 94.0%- 104.5%, and the relative standard derivation is not more than 7.31%. There is no significant difference on analytical results between the above method and the national standard analytical method of atomic absorption spectrometry.
KeyWords AITranslate
1寿曼立,姜桂兰.原子光谱分析(第二版)[M].北京:地贸出版社,1994.
2郝红梅,王安禄,王秋迎.火焰原子吸收光谱法测定铌中微量锌和镉的实验[J].钽铌工业进展,2003,(2):25-26.
1刘煜.原子发射光谱法直接测定仲钨酸铵中杂质钙元素[J].中国科技信息,2008(14):54-54.
2杜姗,黄伟华,胡贵祥.火焰原子发射光谱法测定奶粉中的钠和钾含量[J].中国卫生检验杂志,2008,18(3):449-450. 被引量:4
3宋金华,戴和平,廖丹.电感耦合等离子质谱法测定钽粉中杂质[J].稀有金属与硬质合金,2012,40(2):68-71. 被引量:6
4陈立华,陆小娟,王敏蕾,张颖,迟爱玲.火焰原子发射光谱法测定矿石中的钾和钠[J].有色矿冶,2012,28(5):45-47. 被引量:5
5张旭,肖玉萍,刘磊,曹宏杰.Z2000火焰原子发射光谱法测定卤水中钾、钠和锂的干扰[J].光谱实验室,2013,30(6):3069-3072. 被引量:2
6张颖.电感耦合等离子体发射光谱法测定氟钽酸钾中十四种杂质元素[J].硬质合金,2002,19(2):107-111. 被引量:4
7孙建之.锂的测定方法的进展[J].理化检验:化学分册,2009,45(10):1240-1244. 被引量:14
8张曼,孙建之.火焰原子发射光谱法测定磷酸锂中的钙[J].光谱实验室,2013,30(2):967-968. 被引量:1
9黄冬兰,潘丽君.火焰原子发射光谱法测定电解质饮料中钾钠的含量[J].韶关学院学报,2015,36(2):29-32. 被引量:2
10唐德胜,刘英,童坚.磷钼酸铵-孔雀绿-PVA分光光度法测定钽粉中磷[J].分析试验室,2006,25(9):96-98. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:O657.31[理学—分析化学]
Citation Information:
Potassium content in tantalum powder was determined by flame atomic emission spectrometry, the flame conditions were optimized, and the reagent dosages were selected. The detection limit is 2. 375 μg/g of the above method for the potassium content in tantalum powder under the selected conditions,its standard addition recovery rate is 94.0%- 104.5%, and the relative standard derivation is not more than 7.31%. There is no significant difference on analytical results between the above method and the national standard analytical method of atomic absorption spectrometry.
quote
| GB/T 7714-2015 | [1] ZHANG Zhong, HAO Hong-mei. Determination of Potassium in Tantalum Powder by Flame Atomic Emission Spectrometry[J]. Rare Metals and Cemented Carbides, 2014(5): 65-67. |
| MLA | [1] ZHANG Zhong, and HAO Hong-mei. "Determination of Potassium in Tantalum Powder by Flame Atomic Emission Spectrometry." Rare Metals and Cemented Carbides, no. 5, 2014, pp. 65-67. |
| APA | [1] ZHANG Zhong, & HAO Hong-mei. (2014). Determination of Potassium in Tantalum Powder by Flame Atomic Emission Spectrometry. Rare Metals and Cemented Carbides(5), 65-67. |
| IEEE | [1] ZHANG Zhong and HAO Hong-mei, "Determination of Potassium in Tantalum Powder by Flame Atomic Emission Spectrometry," Rare Metals and Cemented Carbides, no. 5, pp. 65-67, 2014. keywords: {potassium content;tantalum powder;flame atomic emission spectrometry} |