Research on Texture Evolution of TA15 Titanium Alloy during Thermal Compression AITranslate

College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Texture evolution of TA15 titanium alloy during thermal compression deformation was studied by Gleeble--3500 thermal simulation machine and EBSD. The results show that there are significant changes in morphology and orientation of the primary a phase with increased strain rate during deformation: the equal axis shape of the grain is elongated to long strip shape in the direction perpendicular to the compression direction, orientation change region firstly forms in the grain, and then slip deformation occurs to some extent resulting in plastic deformation. At the same time, the strength of a phase texture weakens with increased strain rate, and the texture component is continually transformed from {1120}(1120) to {0001 } (1126).

KeyWords AITranslate

TA15 titanium alloy texture grain orientation thermal compression EBSD

1许国栋.TA15钛合金的热压缩变形性能[J].金属学报,2002(z1):230-232. 被引量:5

2王洋,尤逢海,朱景川,来忠红,刘勇.TA15合金热变形行为研究[J].机械工程材料,2006,30(11):63-65. 被引量:33

3张旺峰,王玉会,马济民.TA15钛合金大锻件热处理强化及机制[J].稀有金属,2010,34(1):1-5. 被引量:21

4陈慧琴,曹春晓,郭灵,林海.Hot deformation mechanism and microstructure evolution of TC11 titanium alloy in β field[J].中国有色金属学会会刊:英文版,2008,18(5):1021-1027. 被引量:13

5Sander B, Raabe D. Texture inhomogeneity in a Ti-Nb based β-titanium alloy after warm rolling and recrystalli- zation[J]. Materials Science and Engineering A, 2008, 479(1-2) :236-247.

6李萍,段园培,薛克敏,王晓溪,甘国强.TB8钛合金的热变形组织与织构[J].中国有色金属学报,2010,20(5):872-877. 被引量:14

7李成铭,李萍,赵蒙,薛克敏.TA15钛合金高温压缩变形行为与组织研究[J].航空材料学报,2013,33(3):25-29. 被引量:14

8徐文臣,单德彬,李春峰,吕炎.TA15钛合金的动态热压缩行为及其机理研究[J].航空材料学报,2005,25(4):10-15. 被引量:71

9贺飞,陈海峰,王玉会.显微组织对TA15合金高温拉伸性能的影响[J].材料工程,2012,40(2):13-15. 被引量:11

10郜阳,孙志超,杨合.TA15钛合金等温近β变形行为及微观组织演化[J].稀有金属材料与工程,2013,42(5):951-956. 被引量:17

1张治民,任璐英,薛勇,吴耀金,王强,徐健,张慧芳.热等静压Ti-6Al-4V钛合金热变形微观组织演变[J].稀有金属材料与工程,2019,48(3):820-826. 被引量:5

2苏连朋,刘汉源,王文先,于振涛,周廉.EBSD技术及其在钛合金织构分析中的研究进展[J].热加工工艺,2019,48(22):1-6. 被引量:8

1柯佳龙,王丽娜,张玉磊,郑波,程佳浩.“材料分析方法”在大学生创新实践平台中的探索与应用[J].创新创业理论研究与实践,2020(22):140-141.

2刘鸿羽,柴皓,娄延春,金磊,赵军,刘时兵,倪嘉.ZTA15大型钛合金熔模精密铸件界面反应研究[J].稀有金属材料与工程,2020,49(3):890-896. 被引量:6

3马兰,杨绍利,李俊翰,朱钰玲.钨对TiH2粉末冶金高温钛合金高温塑性的影响[J].钢铁钒钛,2020,41(4):41-47.

4詹美燕,李春明.电子背散射衍射的制样方法和影响花样质量的因素[J].物理测试,2021,39(1):31-36. 被引量:5

5王辉,夏明许,曾龙,李建国.金属/氧化物界面形成机理原位研究[J].失效分析与预防,2021,16(1):15-27.

6冯瑞,王克鲁,鲁世强,李鑫,欧阳德来,崔霞,周璇,钟明君.BT25钛合金β相区动态再结晶行为及数值模拟[J].稀有金属材料与工程,2021,50(3):894-901. 被引量:3

7左玉婷,王书明,李聪,张丽民,朱言言.激光增材制造钛合金织构跨尺度分析[J].稀有金属材料与工程,2021,50(4):1365-1370. 被引量:4

8赵海涛,姜彤.电子背散射衍射技术在热模拟压缩研究中的应用[J].沈阳理工大学学报,2021,40(2):61-66.

9刘超,王鑫,门月,张浩宇,张思倩,周舸,陈立佳,刘海建.Ti-6Al-4V合金热压缩过程中的动态再结晶[J].材料研究学报,2021,35(8):583-590. 被引量:2

10陆子川,孙亚超,姚草根,李圣刚,候智敏,张绪虎,纪玮,张海洋.一种新型Ti-Al-V-Zr-Mo-Nb低温钛合金组织与性能研究[J].稀有金属材料与工程,2022,51(1):217-224. 被引量:2

1牟世娟,芦明霞.等径角挤压时铝材料显微组织演化研究[J].中国高新技术企业,2009(6):123-124.

2高颖颖.Cu-Cr-Zr-Ag合金高温流变行为及织构演化研究[J].上海有色金属,2016,37(1):20-23.

3刘彦章,Hyun-Gil Kim,Jeong-Yong Park,Yong-Hwan Jeong.冷加工过程中Zr-1Nb板材组织演化研究(英文)[J].稀有金属材料与工程,2013,42(4):667-672. 被引量:1

4刘洪涛,王若超,周吉学,陈燕飞,庄海华.AZ31B镁合金焊接头显微组织及织构演化研究[J].铸造技术,2017,38(4):906-909. 被引量:5

5赵婷,邓磊,王新云.2024铝合金板材高温拉伸流变行为和微观组织演化研究[J].精密成形工程,2015,7(3):37-42. 被引量:7

6蒲春雷,项利,仇圣桃,宋宁.50W600正常晶粒长大过程中再结晶织构演化研究[J].钢铁钒钛,2012,33(5):89-95. 被引量:1

7曾怡丹,郝新,李艳芬,许萍.铝合金半固态浆料保温过程中组织演化研究[J].热加工工艺,2015,44(5):28-31. 被引量:1

8罗睿,姜新华,王秀静,吴军,柳鑫龙,张三平.碳钢大气腐蚀机制及锈层演化研究[J].腐蚀科学与防护技术,2013,25(5):433-436. 被引量:2

9罗睿,吴军,柳鑫龙,周学杰,郑鹏华,张三平.Q235和09CuPCrNi-A钢在两种不同大气环境中腐蚀早期锈层演化研究[J].中国腐蚀与防护学报,2014,34(6):566-573. 被引量:4

10孙兵,张英波,权高峰,李彬.AZ80镁合金半固态组织的等温演化研究[J].特种铸造及有色合金,2014,0(9):928-932. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

Texture evolution of TA15 titanium alloy during thermal compression deformation was studied by Gleeble--3500 thermal simulation machine and EBSD. The results show that there are significant changes in morphology and orientation of the primary a phase with increased strain rate during deformation: the equal axis shape of the grain is elongated to long strip shape in the direction perpendicular to the compression direction, orientation change region firstly forms in the grain, and then slip deformation occurs to some extent resulting in plastic deformation. At the same time, the strength of a phase texture weakens with increased strain rate, and the texture component is continually transformed from {1120}(1120) to {0001 } (1126).

quote

GB/T 7714-2015 [1] WEN Yao, XUE Ke-min, LI Ping, et al. Research on Texture Evolution of TA15 Titanium Alloy during Thermal Compression[J]. Rare Metals and Cemented Carbides, 2014(5): 55-59.
MLA [1] WEN Yao, et al., "Research on Texture Evolution of TA15 Titanium Alloy during Thermal Compression." Rare Metals and Cemented Carbides, no. 5, 2014, pp. 55-59.
APA [1] WEN Yao, XUE Ke-min, LI Ping, & GAN Guo-qiang. (2014). Research on Texture Evolution of TA15 Titanium Alloy during Thermal Compression. Rare Metals and Cemented Carbides(5), 55-59.
IEEE [1] WEN Yao, XUE Ke-min, LI Ping, and GAN Guo-qiang, "Research on Texture Evolution of TA15 Titanium Alloy during Thermal Compression," Rare Metals and Cemented Carbides, no. 5, pp. 55-59, 2014. keywords: {TA15 titanium alloy;texture;grain orientation;thermal compression;EBSD}