Rapid Determination of Trace Germanium in Zinc ElectrolyteSolution by Oscillopolarography AITranslate
Abstract AITranslate
An oscillopolarographic method for the rapid determination of trace germanium in the medium of gallic acid-V(Ⅳ)-EDTA was presented.The peak potential was at-0.60 V,the linear range of the determination was 5×10-8~2×10-6 g/L,and the detection limit was 4×10-9 g/L.The method is directly used for the rapid determination of trace germanium in zinc electrolyte solution with satisfactory results.
KeyWords AITranslate
1北京矿冶研究院分析室.矿石及有色金属分析手册[M].北京:冶金工业出版社,1989.170.
2杨逸萍,胡明辉.示差脉冲极谱法测定海水中痕量锗[J].海洋学报,1991,13(2):277-281. 被引量:5
3刘翰晟.高阻镍合金中锗的连苯三酚方波极谱测定[J].理化检验:化学分册,1983,19(2):20-20.
4张月霞,吴永明.锗(Ⅳ)-没食子酸示波极谱电流增敏机理研究Ⅰ.高温合金中锗的测定及有关研究[J].冶金分析,1997,17(3):8-11. 被引量:4
1陈新焕,江正瑾,李益恒.锗(Ⅳ)-没食子酸-钒(Ⅳ)-EDTA 体系极谱吸附催化波的研究[J].长沙水电师院学报:自然科学版,1997,12(3):313-315.
2王晴晴,杨新安,张王兵.鲁米诺-EDTA体系测定水样中超痕量镉[J].安徽工业大学学报:自然科学版,2015,32(2):143-146.
3刘建,李建.P_(204)-kerosene-EDTA体系萃取分离钨钼[J].中国钼业,2007,31(4):26-29. 被引量:10
4李伟,黄新建,邓海强,王立世.基于二氧化钛纳米管的电化学发光传感器及其对铅离子的测定研究[J].上海师范大学学报:自然科学版,2010,39(3):284-289.
5李益恒,朱志伟.锗(Ⅳ)-3,4-二羟基苯甲酸-钒(Ⅴ)-EDTA体系极谱吸附催化波的研究[J].分析科学学报,1995,11(1):51-54. 被引量:4
6刘爱骅,王瑾,杨孙楷.水样及生物体内微量锌、锰、硒的极谱催化波同时测定[J].台湾海峡,1996,15(3):270-274. 被引量:1
7孙元喜.硫离子-荧光素-抗坏血酸吸附催化波研究及应用[J].分析化学,1993,21(6):742-742. 被引量:3
8刘建,王秀山,杨子超,阎居梅.萃淋树脂CL-P507吸附分离钨、钼的研究——Ⅰ.树脂的吸附及分离性能[J].应用化学,1990,7(4):37-41. 被引量:11
9江正瑾,陈新焕,李益恒.锗(Ⅳ)-没食子酸-钒(Ⅴ)-EDTA体系极谱吸附催化波的研究[J].分析试验室,1998,17(5):63-66. 被引量:8
10杨芳,郑文杰,胡学旺,冯德雄.M^(2+)(Zn^(2+)、Cu^(2+))-BR-OH^- -EDTA 水溶液体系的发光特征[J].暨南大学学报:自然科学与医学版,2002,23(5):52-55. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:O657.14[理学—分析化学]
Citation Information:
An oscillopolarographic method for the rapid determination of trace germanium in the medium of gallic acid-V(Ⅳ)-EDTA was presented.The peak potential was at-0.60 V,the linear range of the determination was 5×10-8~2×10-6 g/L,and the detection limit was 4×10-9 g/L.The method is directly used for the rapid determination of trace germanium in zinc electrolyte solution with satisfactory results.
quote
| GB/T 7714-2015 | [1] JIANG Xin-yu. Rapid Determination of Trace Germanium in Zinc ElectrolyteSolution by Oscillopolarography[J]. Rare Metals and Cemented Carbides, 2004(3): 25-26. |
| MLA | [1] JIANG Xin-yu. "Rapid Determination of Trace Germanium in Zinc ElectrolyteSolution by Oscillopolarography." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 25-26. |
| APA | [1] JIANG Xin-yu. (2004). Rapid Determination of Trace Germanium in Zinc ElectrolyteSolution by Oscillopolarography. Rare Metals and Cemented Carbides(3), 25-26. |
| IEEE | [1] JIANG Xin-yu, "Rapid Determination of Trace Germanium in Zinc ElectrolyteSolution by Oscillopolarography," Rare Metals and Cemented Carbides, no. 3, pp. 25-26, 2004. keywords: {zinc electrolyte solution;oscillopolarography;trace germanium;determination} |