Silicon Determination from Chloride Potassium inthe Presence of Hydrofluoric Acid AITranslate
Abstract AITranslate
Soluble silicate is dissolved in hot water from the trial sample,then hydrofluoric acid is added to dissolve insoluble silicate.At pH=1.5~2.0,silicate ion and ammonium molybdate becomes the yellow silicon-molybdenum heteropoly acid and is reduced into silico-molybdenum blue by the reductant.The resultant material shows maximum absorption peak at 810 nm,the apparent mol light absorption coefficient is 1.2×10~4 L/(mol·cm ),content ranges 0~100 μg/50 ml, as conforms to Beer's Law.The method can be directly used for total silicon determination from commercial and reagent chloride potassium.
KeyWords AITranslate
1王永奉.分析化学(下册)[M].北京:地质出版社,1996.71.
2王肇信 幸良佐 曾芳屏.钽铌冶金学[M].北京:稀有金属冶金学会,1998.232-254.
3李俊义.分析化学[M].北京:高等教育出版社,1981.121.
1阎永胜,魏家友,史克全,周晓光,谭振江.SiO_3^(2-)存在下ARS-Cr(Ⅲ)显色体系测定Cr(Ⅲ)[J].理化检验:化学分册,1995,31(2):98-98. 被引量:1
2王淑琴,徐淑研,张万玲.火焰原子吸收法测定催化剂中铁的含量[J].化学工程师,2000,14(6):46-47.
3王翠萍,董世哲,李琳,贺美英.ICP-AES法测定铀铌锆合金中的铌和锆[J].原子能科学技术,2003,37(z1):169-172. 被引量:8
4齐荣,杨国武,韩美,胡净宇.电感耦合等离子体原子发射光谱法测定钛合金中镧铈钇[J].冶金分析,2014,34(2):53-57. 被引量:14
5王晶.火焰原子吸收法测定催化剂中镍的含量[J].化学工程师,2002,16(6):34-34. 被引量:2
6胡秋娈.钼蓝试法鉴定SiO^2—3实验探讨与改进[J].洛阳师专学报:自然科学版,1993,7(1):78-78.
7梁文君,杨泽彪,王齐光,虞光禹.吸光光度法测定金属硅中的磷、锰[J].云南冶金,2002,31(1):51-52. 被引量:3
8周恺,孙宝莲,李波,杨平平.火焰原子吸收光谱法测定红土镍矿中锌[J].冶金分析,2011,31(10):57-61. 被引量:15
9魏恩双.EGTA络合滴定法测定锆铁合金中钙[J].莱钢科技,2016,0(5):44-45.
10陈小兰.原子吸收分光光度法测定磷酸锆银钠中的银[J].广东有色金属学报,2003,13(1):73-75.
Basic Information:
DOI:
Chinese Library Classification Number:O657.3[理学—分析化学]
Citation Information:
Soluble silicate is dissolved in hot water from the trial sample,then hydrofluoric acid is added to dissolve insoluble silicate.At pH=1.5~2.0,silicate ion and ammonium molybdate becomes the yellow silicon-molybdenum heteropoly acid and is reduced into silico-molybdenum blue by the reductant.The resultant material shows maximum absorption peak at 810 nm,the apparent mol light absorption coefficient is 1.2×10~4 L/(mol·cm ),content ranges 0~100 μg/50 ml, as conforms to Beer's Law.The method can be directly used for total silicon determination from commercial and reagent chloride potassium.
quote
| GB/T 7714-2015 | [1] ZHANG Tao, ZHOU Li. Silicon Determination from Chloride Potassium inthe Presence of Hydrofluoric Acid[J]. Rare Metals and Cemented Carbides, 2004(3): 27-28. |
| MLA | [1] ZHANG Tao, and ZHOU Li. "Silicon Determination from Chloride Potassium inthe Presence of Hydrofluoric Acid." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 27-28. |
| APA | [1] ZHANG Tao, & ZHOU Li. (2004). Silicon Determination from Chloride Potassium inthe Presence of Hydrofluoric Acid. Rare Metals and Cemented Carbides(3), 27-28. |
| IEEE | [1] ZHANG Tao and ZHOU Li, "Silicon Determination from Chloride Potassium inthe Presence of Hydrofluoric Acid," Rare Metals and Cemented Carbides, no. 3, pp. 27-28, 2004. keywords: {hydrofluoric acid;photometry;chloride potassium;total silicon} |