Preparation of New Ag-SnO_2 Contact Material and Its Effectson the Material's Properties AITranslate
Abstract AITranslate
The new AgSnO_2 contact material is developed by chemical co-precipitation and powder hot forging.Analysis and testing is made of its structure and physical properties such as density,hardness and resistivity,etc.
KeyWords AITranslate
1邵文柱,崔玉胜,杨德庄.电接触材料的发展与现状[J].电工合金,1999(1):11-15. 被引量:60
2堵永国,白书欣,张家春,易阳,王乃千.一种全新AgSnO_2触点材料的设计与制备[J].电工合金,2000(1):15-22. 被引量:44
3堵永国,张为军.常用触点材料的物理性能[J].电工材料,2002(1):35-39. 被引量:15
1陈晓华,贾成厂,刘向兵.粉末冶金技术在银基触点材料中的应用[J].粉末冶金工业,2009,19(4):41-47. 被引量:10
2乔秀清,申乾宏,陈乐生,贺庆,樊先平,杨辉.AgSnO2电接触材料的研究进展[J].材料导报,2013,27(1):1-6. 被引量:27
3刘松涛,郭敏,王俊勃,师浩军,杨凯,游义博.纳米Ag/SnO2电接触材料的化学沉积制备工艺及耐电弧烧蚀性能[J].纺织高校基础科学学报,2020,33(4):45-50.
1王景芹,朱艳彩,王海涛,赵军.添加物Bi对AgSnO_2触头材料的影响[J].电工技术学报,2011,26(1):29-33. 被引量:15
2乔秀清,申乾宏,陈乐生,贺庆,樊先平,杨辉.AgSnO2电接触材料的研究进展[J].材料导报,2013,27(1):1-6. 被引量:27
3贾成厂,王欣平.烧结金属触点材料[J].金属世界,2013(2):9-15. 被引量:3
4王塞北,谢明,刘满门,杨有才,陈永泰,张吉明.AgNi电触头材料研究进展[J].稀有金属材料与工程,2013,42(4):875-880. 被引量:21
5乔秀清,陈骋,娄湘虹,孙继扬,申乾宏,陈乐生,杨辉.载银SnO_2复合微球的制备及表征[J].材料科学与工程学报,2013(5):641-644. 被引量:2
6王松,陈永泰,杨有才,张吉明,刘满门,王塞北,谢明.AgSnO_2电接触材料的研究进展[J].贵金属,2013,34(S01):102-107. 被引量:10
7溥存继,谢明,杜文佳,杨云峰,赵明,王塞北,张吉明,杨有才,陈永泰.贵金属基电接触材料的研究进展[J].材料导报,2014,28(7):22-25. 被引量:23
8刘方方.材料变形量对反应合成AgSnO2材料电接触性能的影响[J].中国科技纵横,2014(16):219-219.
9于朝清,刘雪梅,任小梅,徐永红,章应,田茂江,周晓荣.AgSnO_2电接触材料制造技术的研究进展[J].贵金属,2014,35(A01):93-99. 被引量:8
10陶麒鹦,周晓龙,周允红,樊勇军,张浩.AgCuO电触头材料的接触电阻及电弧侵蚀形貌分析[J].稀有金属材料与工程,2015,44(5):1219-1223. 被引量:19
1郑晶,郭天福,付翀.含微量元素的Ag-SnO2触头材料的研究进展[J].中国材料科技与设备,2015,11(5):52-54.
2甘卫平,周兆锋,林炳,李晶.粉末内氧化法制备AgCuO(10)触头材料工艺研究[J].材料导报,2005,19(F05):308-309. 被引量:4
3思芳,王俊勃,刘松涛,杨敏鸽,杨尔慧.Ag-SnO_2触头材料制备工艺的研究现状与发展趋势[J].电子元件与材料,2015,34(9):31-34. 被引量:8
Basic Information:
DOI:
Chinese Library Classification Number:TM241[一般工业技术—材料科学与工程]
Citation Information:
The new AgSnO_2 contact material is developed by chemical co-precipitation and powder hot forging.Analysis and testing is made of its structure and physical properties such as density,hardness and resistivity,etc.
quote
| GB/T 7714-2015 | [1] ZHOU Zhao-feng, GAN Wei-ping, LIN Bing. Preparation of New Ag-SnO_2 Contact Material and Its Effectson the Material's Properties[J]. Rare Metals and Cemented Carbides, 2004(3): 22-24. |
| MLA | [1] ZHOU Zhao-feng, et al., "Preparation of New Ag-SnO_2 Contact Material and Its Effectson the Material's Properties." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 22-24. |
| APA | [1] ZHOU Zhao-feng, GAN Wei-ping, & LIN Bing. (2004). Preparation of New Ag-SnO_2 Contact Material and Its Effectson the Material's Properties. Rare Metals and Cemented Carbides(3), 22-24. |
| IEEE | [1] ZHOU Zhao-feng, GAN Wei-ping, and LIN Bing, "Preparation of New Ag-SnO_2 Contact Material and Its Effectson the Material's Properties," Rare Metals and Cemented Carbides, no. 3, pp. 22-24, 2004. keywords: {AgSnO_2 contact material;chemical co-precipitation;powder hot forging} |