Study of Vacuum Canned Hot Extrusion of High-Si Al Alloy Powder AITranslate
Abstract AITranslate
High-Si aluminum alloy is fabricated by air-atomization water cooling and vacuum canned hot extrusion.The powder has gone through morphology SEM,density test、microstructure analysis and mechanical property testing.Experimental results have shown that,compared to the as-cast sample,the resultant material is characterized by very uniform,dispersed and fine Si initial crystal,obviously higher tensile strength.With the increase of extrusion temperature and Si content and the primary silicon crystal was fined and evenly distributed.Otherwise,with the increasing extrusion temperature,the particle size of initial Si crystalline phase becomes larger and the tensile strength drops.
KeyWords AITranslate
1张大童,李元元,罗宗强,邱诚.快速凝固高硅铝合金粉末的热挤压过程[J].中国有色金属学报,2001,11(1):6-9. 被引量:22
2张大童,李元元,罗宗强.快速凝固过共晶铝硅合金材料的研究进展[J].轻合金加工技术,2001,29(2):1-6. 被引量:35
3沈军,谢壮德,董寅生,周彼德,李庆春.快速凝固铝硅合金的性能、应用及发展方向[J].粉末冶金技术,2000,18(3):208-213. 被引量:18
1周朝辉,蒲治军,腾文华,江学强.真空包套锻造成形有限元模拟及试验[J].热加工工艺,2011,40(13):72-73.
2解立川,彭超群,王日初,王小锋,蔡志勇,刘兵.高硅铝合金电子封装材料研究进展[J].中国有色金属学报,2012,22(9):2578-2587. 被引量:44
3刘孝飞,刘彦强,樊建中,魏少华,马自力,左涛.热等静压制备Si_p/Al-Cu复合材料的组织与性能[J].中国有色金属学报,2012,22(11):3059-3065. 被引量:4
4王荣旗,谢敬佩,吴文杰,王爱琴.SiC颗粒预处理对SiC_p/Al-Si复合材料组织及性能的影响[J].粉末冶金工业,2014,24(6):33-36. 被引量:9
1童国庆,杨伟锋,申文浩,仲洪海,蒋阳.Sip/Al功能梯度材料的粉末冶金热压工艺制备及性能研究[J].粉末冶金工业,2014,24(1):39-43. 被引量:3
2王合利,徐达,常青松,王志会.铝合金封装中陶瓷基板的可靠性优化设计研究[J].电子元件与材料,2014,33(3):73-76.
3马如龙,彭超群,王日初,张纯,解立川.电子封装用diamond/Al复合材料研究进展[J].中国有色金属学报,2014,24(3):689-699. 被引量:11
4解立川,彭超群,王日初,蔡志勇.快速凝固过共晶铝硅合金粉末的形貌与显微组织[J].中国有色金属学报,2014,24(1):130-136. 被引量:8
5陈寰贝,庞学满,胡进,程凯.航空航天用电子封装材料及其发展趋势[J].电子与封装,2014,14(5):6-9. 被引量:13
6徐志伟,王振亚.T/R组件封装用铝硅合金高速铣削试验研究[J].电子机械工程,2018,34(6):43-46. 被引量:2
7孔亚茹,郭强,张荻.颗粒增强铝基复合材料界面性能的研究[J].材料导报,2015,29(9):34-43. 被引量:34
8李多生,吴文政,QIN Qing-hua,周贤良,左敦稳,鲁世强,郜友彬.石墨烯/Al复合材料的微观结构及力学性能[J].中国有色金属学报,2015,25(6):1498-1504. 被引量:42
9郎利辉,喻思,姚松,王刚,布国亮,续秋玉.热等静压法制备TC11钛合金及其粉-固扩散连接件的组织与性能[J].粉末冶金材料科学与工程,2015,20(4):548-554. 被引量:1
10喻思,郎利辉,姚松,王刚,黄西娜,续秋玉.热等静压制备CF/Al复合材料的微观结构及性能[J].中国有色金属学报,2015,25(10):2745-2751. 被引量:4
1杨伏良,甘卫平,陈招科.硅含量对高硅铝合金材料组织及性能的影响[J].材料导报,2005,19(2):98-100. 被引量:28
2张伟,杨伏良,甘卫平,刘泓.电子封装用高硅铝合金热膨胀性能的研究[J].材料导报,2006,20(F05):348-350. 被引量:17
3杨伏良,甘卫平,陈招科.挤压温度对高硅铝合金材料力学性能的影响[J].材料导报,2005,19(7):127-129. 被引量:2
4徐玉松,刘颖,胡陈.粉末热挤压法制备ZrO_2/Cu复合材料及性能研究[J].热加工工艺,2014,43(2):121-124. 被引量:1
5解立川,彭超群,王日初,王小锋,蔡志勇,刘兵.高硅铝合金电子封装材料研究进展[J].中国有色金属学报,2012,22(9):2578-2587. 被引量:44
6路王珂,谢敬佩,王爱琴,李继文,张银娣.退火温度对铜铝铸轧复合板界面组织和力学性能的影响[J].机械工程材料,2014,38(3):14-17. 被引量:12
7姜秀凤,娄勇健,王锐,刘海艳,陈晓红,周宇杭.玻璃钢包装筒结构设计及成形工艺[J].精密成形工程,2014,6(2):60-62. 被引量:3
8廖文俊,刘新宽,王宇鑫.高性能铜/铝复合排的制备及界面机理[J].同济大学学报:自然科学版,2012,40(8):1234-1238. 被引量:12
9邓朝飞,安宁.热处理对铸造ZL102合金组织和性能的影响[J].热加工工艺,2011,40(24):216-217. 被引量:5
10柳大敏.国内外空调致冷铜管的技术发展[J].上海有色金属,1997,18(4):183-190.
Basic Information:
DOI:
Chinese Library Classification Number:TB376.2[一般工业技术—材料科学与工程]
Citation Information:
High-Si aluminum alloy is fabricated by air-atomization water cooling and vacuum canned hot extrusion.The powder has gone through morphology SEM,density test、microstructure analysis and mechanical property testing.Experimental results have shown that,compared to the as-cast sample,the resultant material is characterized by very uniform,dispersed and fine Si initial crystal,obviously higher tensile strength.With the increase of extrusion temperature and Si content and the primary silicon crystal was fined and evenly distributed.Otherwise,with the increasing extrusion temperature,the particle size of initial Si crystalline phase becomes larger and the tensile strength drops.
quote
| GB/T 7714-2015 | [1] GAN Wei-ping, CHEN Zhao-ke, YANG Fu-liang. Study of Vacuum Canned Hot Extrusion of High-Si Al Alloy Powder[J]. Rare Metals and Cemented Carbides, 2004(3): 18-21. |
| MLA | [1] GAN Wei-ping, et al., "Study of Vacuum Canned Hot Extrusion of High-Si Al Alloy Powder." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 18-21. |
| APA | [1] GAN Wei-ping, CHEN Zhao-ke, & YANG Fu-liang. (2004). Study of Vacuum Canned Hot Extrusion of High-Si Al Alloy Powder. Rare Metals and Cemented Carbides(3), 18-21. |
| IEEE | [1] GAN Wei-ping, CHEN Zhao-ke, and YANG Fu-liang, "Study of Vacuum Canned Hot Extrusion of High-Si Al Alloy Powder," Rare Metals and Cemented Carbides, no. 3, pp. 18-21, 2004. keywords: {rapid solidification;vacuum canned;hot extrusion;Al-Si alloy} |