Effect of Solid Solution-Aging on Microstructure and Performance of TC4 Titanium Alloy AITranslate
Abstract AITranslate
The investigation was made of the effect of solid solution-aging process on the microstructure, mechanical properties and tensile fracture morphology at room temperature of TC4 titanium alloy. The results show that through solid solution-aging process, acicular martensite α' phase and metastable β phase are broken down into dispersive stable α+β phase, increasing the hardness and strength of TC4 titanium alloy. When the solid solution temperature is constant,the hardness and strength of the TC4 titanium alloy gradually decrease, while its plasticity gradually increases with the aging temperature increasing. Under the conditions of solid solution temperature 940 ~C and aging temperature 500 ℃, the TC4 titanium alloy can be obtained with higher strength and better plasticity. After solid solution-aging treatment, TC4 titanium alloy has better plasticity at room temperature,and its tensile fracture is characterized by ductile fracture.
KeyWords AITranslate
1卢斌,杨锐.热处理对650℃短时用Ti650板材显微组织和力学性能的影响[J].宇航材料工艺,2007,37(6):77-81. 被引量:9
2曹春晓.一代材料技术,一代大型飞机[J].航空学报,2008,29(3):701-706. 被引量:123
3王亮,史鸿培.高性能钛合金粉末冶金技术研究[J].宇航材料工艺,2003,33(3):42-44. 被引量:24
4刘莹,曲周德,王本贤.钛合金TC4的研究开发与应用[J].兵器材料科学与工程,2005,28(1):47-50. 被引量:121
5赵永庆.高温钛合金研究[J].钛工业进展,2001,18(1):33-39. 被引量:97
6马玲,赵双群,王战宏,买学锋,赵玉林.热等静压温度对铍铝合金显微组织及力学性能的影响[J].飞航导弹,2006(8):57-59. 被引量:10
7李承受.空间环境条件下材料的失效[J].材料科学与工程,1991,9(1):1-7. 被引量:7
8王悔改,冷文才,李双晓,等.热处理工艺对TC4钛合金组织和性能的影响[J].材料热处理技术,2011,40(10):181-183.
9王新英,谢成木.改善ZTi6Al4V合金性能的热处理工艺[J].特种铸造及有色合金,2001(6):16-17. 被引量:10
1谭国寅,吴云峰,杨钢,孙彦华,岳有成.固溶时效工艺对TC4钛合金冲击性能的影响[J].铸造技术,2016,37(5):902-903. 被引量:4
2丁辉,曹占元,张玉勤,周荣.高速线材轧制工艺对Ti-6Al-4V合金小规格棒材组织与性能的影响[J].热加工工艺,2016,45(11):47-50. 被引量:3
3魏鑫,赵兴东,李昌永,王健妍.热处理制度对TC4钛合金风扇盘组织和性能的影响研究[J].中国材料进展,2017,36(7):588-593. 被引量:4
4张峰,黄文克,李远征,徐凯,杨晓龙,郭丹,薛康利.钛合金油井管应用研究现状及进展[J].焊管,2017,40(11):7-11. 被引量:8
5王琛,刘文博,李涛.热处理对航空用TC4合金组织与性能的影响[J].金属热处理,2018,43(8):107-110. 被引量:5
6刘冀尧,王文焱,谢敬佩,赵轩玮,李长银,张玉林,胡玉水.固溶时效对Ti-6Al-4V-1.5Mn合金组织与性能的影响[J].金属热处理,2018,43(9):106-111. 被引量:1
7徐楷昕,雷振,黄瑞生,尹立孟,方乃文,邹吉鹏,曹浩.40mm厚TC4钛合金窄间隙激光填丝焊接头组织及性能[J].材料导报,2022,36(2):158-163. 被引量:5
8高学敏,王晗,王可迪,何宇鹏,程东松.固溶时效处理对Ti-6Al-4V ELI钛合金准静态和动态力学性能的影响[J].金属热处理,2022,47(11):87-91. 被引量:1
9朱宁远,陈世豪,廖强,陈秋明,赖文坤,左寿彬.固溶时效处理对TC11钛合金显微组织和硬度的影响[J].金属热处理,2022,47(12):62-66. 被引量:1
1张俊晓,李志敏,史亚鸣,蒋泰旭,张玉勤.热处理对Ti-5Al-2V-3Fe-0.2O热轧板材组织和力学性能的影响[J].热加工工艺,2018,47(24):188-192.
2史亚鸣,李志敏,蒋泰旭,曹占元,张玉勤.固溶处理对Ti-4.5Al-2.5V-1.5Fe-0.25O热轧板材组织及力学性能的影响[J].热加工工艺,2017,46(8):202-206.
3杨钢,严继康.2016年云南金属材料与加工年评[J].云南冶金,2017,46(2):86-104.
4刘德波,张劲松,孔令云,鹿海艳.超声冲击处理对TC4钛合金焊接试样微观组织及力学性能的影响[J].铸造技术,2017,38(11):2744-2746. 被引量:2
5王琛,刘文博,李涛.热处理对航空用TC4合金组织与性能的影响[J].金属热处理,2018,43(8):107-110. 被引量:5
6冯哲,解秀萍.钛合金机械盘件锻压工艺的模糊PID控制[J].热加工工艺,2019,48(5):179-181. 被引量:1
7窦红强,翟大军,杜东方,侯勇.固溶时效对AZ31镁合金母材及搅拌摩擦点焊接头组织和性能的影响[J].装备制造与教育,2019,33(2):25-29.
8李敏娜,卢凯凯,周立鹏,肖松涛.加热温度及变形量对TC4钛合金棒材低倍清晰晶现象的影响[J].金属热处理,2019,44(12):120-124. 被引量:1
9卜嘉利,高志坤,佟文伟,孙佳斯.航空发动机油管固定支架断裂失效分析[J].航空发动机,2020,46(3):40-45. 被引量:3
10胡志立,李小兵,李建亮,付强,吴丹,张垂贵,李健,胡新太.钛合金特殊螺纹接头HSTI性能分析[J].钢管,2020,49(3):69-72. 被引量:2
1蹇海根,姜锋,黄宏锋,韦莉莉,蒋龙.固溶-时效处理对7B04合金组织和性能的影响[J].兵器材料科学与工程,2009,32(4):53-58. 被引量:7
2窦进,李保成,王瑞栋,韩孟岩.热处理对2024铝合金组织与性能的影响[J].热加工工艺,2011,40(22):176-178. 被引量:7
3郝红元,王瑞栋.弹体热成形模具材料成分及性能研究[J].热加工工艺,2012,41(14):115-116. 被引量:1
4崔丽,丁红园,陈俐,何恩光,顾长石.焊后热处理对铝锂合金激光焊接头微观组织的影响[J].材料热处理学报,2014,35(10):58-63. 被引量:4
5陈素娟,张瑞英,李艳辉.时效处理对TiB_(2P)/A356复合材料组织与性能的影响[J].热加工工艺,2014,43(2):114-116.
6尹志民,蒋蓉蓉,危明,聂波,石钰,何振波.固溶-时效处理对B93合金锻件组织与性能的影响[J].材料热处理学报,2009,30(5):79-82. 被引量:2
7杨金文,周旺松,陆建生,俞峰,许达,曹文全.α-Cr相对新型奥氏体合金热处理组织及性能的影响[J].钢铁,2015,50(7):84-91. 被引量:2
8董晓超,屈华,陶瑜,姜海洋,孙维勋,王健,张涛.微量Ag对Al-5.3Cu-0.8Mg合金组织与时效行为的影响[J].金属材料研究,2013,39(2):1-5.
9姜全,王福兴,范锡章.生产工艺对砂型铸造铬青铜组织及性能的影响[J].铸造,2009,58(6):598-601. 被引量:2
10王江涛,张永康,周金宇,卢雅琳,陈菊芳,葛茂忠,孙凌燕,叶霞,张朝阳.两种焊后处理工艺对铝合金焊接头力学性能的影响[J].中国有色金属学报,2017,27(1):40-50. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG156.9[金属学及工艺—热处理]
Citation Information:
The investigation was made of the effect of solid solution-aging process on the microstructure, mechanical properties and tensile fracture morphology at room temperature of TC4 titanium alloy. The results show that through solid solution-aging process, acicular martensite α' phase and metastable β phase are broken down into dispersive stable α+β phase, increasing the hardness and strength of TC4 titanium alloy. When the solid solution temperature is constant,the hardness and strength of the TC4 titanium alloy gradually decrease, while its plasticity gradually increases with the aging temperature increasing. Under the conditions of solid solution temperature 940 ~C and aging temperature 500 ℃, the TC4 titanium alloy can be obtained with higher strength and better plasticity. After solid solution-aging treatment, TC4 titanium alloy has better plasticity at room temperature,and its tensile fracture is characterized by ductile fracture.
quote
| GB/T 7714-2015 | [1] XU Jian, WANG Wen-yan, XIE Jing-pei, et al. Effect of Solid Solution-Aging on Microstructure and Performance of TC4 Titanium Alloy[J]. Rare Metals and Cemented Carbides, 2014(2): 41-44. |
| MLA | [1] XU Jian, et al., "Effect of Solid Solution-Aging on Microstructure and Performance of TC4 Titanium Alloy." Rare Metals and Cemented Carbides, no. 2, 2014, pp. 41-44. |
| APA | [1] XU Jian, WANG Wen-yan, XIE Jing-pei, & LI Luo-li. (2014). Effect of Solid Solution-Aging on Microstructure and Performance of TC4 Titanium Alloy. Rare Metals and Cemented Carbides(2), 41-44. |
| IEEE | [1] XU Jian, WANG Wen-yan, XIE Jing-pei, and LI Luo-li, "Effect of Solid Solution-Aging on Microstructure and Performance of TC4 Titanium Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 41-44, 2014. keywords: {TC4 titanium alloy;solid solution-aging;microstructure;mechanical property;tensile fracture} |