The Latest Development of the New Sintering Process of Heavy Tungsten Alloys AITranslate

School of Materials Engineering, Nanjing Institute of Technology;School of Materials Engineering, Nanjing Institute of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Various sintering methods are reviewed,including solid phase sintering, spark plasma sintering, microwave sintering, two-step sintering, low-temperature activated sintering, selective laser sintering, stacking sintering and so on. Besides, the problems of these methods are summarized.

KeyWords AITranslate

heavy tungsten alloy spark plasma sintering microwave sintering two-step sintering stacking sintering the latest development

1王松,谢明.高密度钨合金的研究现状与发展趋势[J].稀有金属材料与工程,2012,41(S2):145-148. 被引量:22

2丁飞,范景莲,曾毅,龚星,田家敏.稀土La对细晶93W-4.9Ni-2.1Fe合金致密化与显微组织的影响[J].粉末冶金材料科学与工程,2011,16(4):517-522. 被引量:5

3范景莲,刘涛,彭石高,祁美贵,田家敏.稀土Y在90W-7Ni-3Fe合金中的存在形态和分布特征[J].稀有金属材料与工程,2011,40(8):1438-1441. 被引量:4

4李鹏.高密度钨合金研究现状与发展趋势[J].稀有金属与硬质合金,2004,32(3):32-35. 被引量:9

5邹俭鹏,张兆森.真空烧结制备90W-Ni-Fe高密度钨合金的性能与显微结构[J].中国有色金属学报,2013,23(3):703-710. 被引量:12

6刘桂荣,王玲,王广达,杨海兵.钨合金轧制变形强化的组织与性能研究[J].兵器材料科学与工程,2010,33(5):39-41. 被引量:13

7Xiang D P, Ding L, Li Y Y, et al. Preparation of fine- grained tungsten heavy alloys by spark plasma sintered W-TNi-3Fe composite powders with different bail milling time [J]. Journal of Alloys and Compounds, 2013,562:19-24.

8马运柱,黄伯云,范景莲,熊翔,汪登龙.纳米级90W-7Ni-3Fe复合粉末的烧结特性[J].中国有色金属学报,2004,14(8):1382-1388. 被引量:6

9向道平,丁雷.高密度W-Ni-Fe合金的烧结新技术[J].稀有金属,2013,37(1):155-163. 被引量:10

10范景莲,曲选辉,李益民,黄伯云.高比重合金的固相烧结[J].中国有色金属学报,1999,9(2):327-329. 被引量:28

1邹树梁,颜亮,唐德文,谢宇鹏,张德.高密度W-Ni-Fe合金制备与应用研究进展[J].南华大学学报:自然科学版,2015,29(1):53-59. 被引量:3

2武杰,孙毅,王晖.烧结和热处理对WNiFe合金板材轧制性能的影响[J].热加工工艺,2016,45(20):239-241. 被引量:2

3田野,孙大智,李萍,梁辰,华睿.高压扭转对难熔金属粉末钨致密固结及强韧化的影响研究[J].稀有金属与硬质合金,2016,44(5):37-42. 被引量:1

1邓力群,邹树梁,唐德文.基于ProCAST研究冷却速率对新型铁基铸锭凝固过程的影响[J].中国铸造装备与技术,2016,51(4):43-48. 被引量:1

2李奎江,邹树梁,唐德文.核辐射屏蔽材料的研究进展及发展趋势[J].现代制造技术与装备,2017,53(8):178-178. 被引量:4

3吴春凌,刘霞,陈斌.纳米粉末、切屑的固态成型方法研究与发展[J].热加工工艺,2017,46(22):9-12.

4高建平,葛鹏.钨/环氧树脂辐射防护复合材料制备以及原位拉伸性能和微观组织演变[J].中国胶粘剂,2020,29(5):20-23. 被引量:1

5张浩,石科学,郑晓斐.高密度钨合金部件断裂失效分析[J].铸造技术,2020,41(6):557-559.

6张俊,杨晓青,李志翔.钨粉粒度和烧结温度对添加La_(2)O_(3)的钨合金性能和组织的影响[J].稀有金属与硬质合金,2021,49(2):24-28. 被引量:1

1向道平,丁雷.高密度W-Ni-Fe合金的烧结新技术[J].稀有金属,2013,37(1):155-163. 被引量:10

2刘建华,吕晓军,李劼,胡凌云,蒋良兴.两步烧结法制备镁铝尖晶石及其在Na_3AlF_6-AlF_3-CaF_2-Al_2O_3电解质中的腐蚀(英文)[J].中国有色金属学报:英文版,2016,26(10):2754-2761.

3章晓波,孙文,陈永明,沈崇.粉末轧制-叠层烧结法制备较厚93W-4.9Ni-2.1Fe高密度钨合金片材的研究[J].稀有金属与硬质合金,2013,41(5):28-31. 被引量:3

4蔡俊,丰平,贺跃辉.烧结工艺对梯度结构硬质合金梯度层组织和厚度的影响[J].硬质合金,2007,24(2):91-95. 被引量:12

5杨斌,宋丽叶.低温活化烧结超细晶粒钼坯的轧制工艺及其特性探讨[J].稀有金属材料与工程,1989(3):23-29.

6罗伟红,宋宁,谢刚,姚云,田林.高能球磨法制备NiFe_2O_4基惰性阳极[J].金属功能材料,2012,19(6):7-11. 被引量:1

7黄晓玲,张菊平.钼细晶材料制备工艺研究[J].中国钼业,2008,32(4):42-44. 被引量:2

8谭澄宇,郑学斌,赵旭山,刘宇,李劲风.Cu-ZrW_2O_8复合镀层的制备[J].中南大学学报:自然科学版,2008,39(2):234-238. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

Various sintering methods are reviewed,including solid phase sintering, spark plasma sintering, microwave sintering, two-step sintering, low-temperature activated sintering, selective laser sintering, stacking sintering and so on. Besides, the problems of these methods are summarized.

quote

GB/T 7714-2015 [1] SUN Wen, ZHANG Xiao-bo. The Latest Development of the New Sintering Process of Heavy Tungsten Alloys[J]. Rare Metals and Cemented Carbides, 2014(2): 36-40.
MLA [1] SUN Wen, and ZHANG Xiao-bo. "The Latest Development of the New Sintering Process of Heavy Tungsten Alloys." Rare Metals and Cemented Carbides, no. 2, 2014, pp. 36-40.
APA [1] SUN Wen, & ZHANG Xiao-bo. (2014). The Latest Development of the New Sintering Process of Heavy Tungsten Alloys. Rare Metals and Cemented Carbides(2), 36-40.
IEEE [1] SUN Wen and ZHANG Xiao-bo, "The Latest Development of the New Sintering Process of Heavy Tungsten Alloys," Rare Metals and Cemented Carbides, no. 2, pp. 36-40, 2014. keywords: {heavy tungsten alloy;spark plasma sintering;microwave sintering;two-step sintering;stacking sintering;the latest development}