A new S/TiO2 composite cathode material was synthesized with elemental sulfur and titanium dioxide. The crystal structure and surface morphology of the composite were characterized by XRD and SEM, and its electrochemical performance was studied by charge-discharge test and electrochemical impedance test. The results show that S/TiO2 composite cathode material with a S/TiO2 mass ratio of 5 : 1 has good electrochemical performance,with initial discharge specific capacity up to 370 mA · h/g at 0.1C and kept at 290 mA · h/g after 30 cycles.
KeyWords AITranslate
1曹占芳,钟宏,姜涛,王帅,刘广义,夏柳荫.栾川钼矿高效选矿试验研究[J].稀有金属与硬质合金,2012,40(1):1-4. 被引量:9
2叶雪均,余夏静,刘军.某钨矿矿石回收钼和白钨的试验研究[J].中国钨业,2008,23(3):16-19. 被引量:14
3叶雪均,王李鹏,邬东,金婷婷.新型钼捕收剂浮选某钨矿伴生钼的试验研究[J].矿产综合利用,2011(1):21-25. 被引量:3
4魏德州.固体物料分选学[M].北京:冶金工业出版社,2009:95-103.
1姜雨婷,宁超凡,潘俊安,杜子博,谢淑红.TiO2/S复合材料在锂硫电池中的应用[J].湘潭大学自然科学学报,2016,38(2):50-55.
1鞠定德.化学镀二氧化钛硅太阳电池减反射膜的研制[J].云南师范大学学报:自然科学版,1991,11(2):37-39.
2蔡振平.LiCoO_2改性LiMn_2O_4的制备及性能的研究[J].电池,2007,37(5):351-353.
3冯勇,周廉.Y_(1-x)Ho_xBa_2Cu_3O_y超导体的制备及性能[J].低温与超导,1992,20(4):31-36. 被引量:1
4陈学定,大森明,荒田吉明.低气压等离子喷涂TiO_2时涂层的电学性能研究[J].硅酸盐学报,1990,18(5):443-449. 被引量:3
5饶睦敏,耿秀玉,孙娉,李小平,李伟善.锂电池单质硫/碳复合正极材料的研究进展[J].材料导报,2013,27(21):132-138. 被引量:1
6余兴增,蔡加勒,周绍民.铅晶电极的制备及性能[J].电源技术,1994,18(2):9-12. 被引量:7
7陈灵谦.正极材料Li_3V_2(PO_4)_3的制备及性能[J].电池,2007,37(2):107-108. 被引量:3
8叶超超,梁兴华,史琳,刘于斯,曾帅波.不同电解液对硫复合正极材料导电性能的影响[J].化工新型材料,2015,43(9):175-176.
9鲍自力,朱彦荣,郝国栋,周安娜.锂离子电池Li_4Ti_(4.95)Zr_(0.05)O_(12)负极材料的结构与电化学性能[J].有色金属工程,2015,5(6):7-10. 被引量:3
10张万红,方亮,岳敏,于作龙.碳纳米管用于锂离子电池负极材料[J].电池,2006,36(1):50-51. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]
Citation Information:
A new S/TiO2 composite cathode material was synthesized with elemental sulfur and titanium dioxide. The crystal structure and surface morphology of the composite were characterized by XRD and SEM, and its electrochemical performance was studied by charge-discharge test and electrochemical impedance test. The results show that S/TiO2 composite cathode material with a S/TiO2 mass ratio of 5 : 1 has good electrochemical performance,with initial discharge specific capacity up to 370 mA · h/g at 0.1C and kept at 290 mA · h/g after 30 cycles.
quote
| GB/T 7714-2015 | [1] LU Hong-guang, PAN Feng. Preparation and Performance of S/TiO_2 Composite Cathode Material in Rechargeable Lithium/Sulfur Battery[J]. Rare Metals and Cemented Carbides, 2014(2): 45-48. |
| MLA | [1] LU Hong-guang, and PAN Feng. "Preparation and Performance of S/TiO_2 Composite Cathode Material in Rechargeable Lithium/Sulfur Battery." Rare Metals and Cemented Carbides, no. 2, 2014, pp. 45-48. |
| APA | [1] LU Hong-guang, & PAN Feng. (2014). Preparation and Performance of S/TiO_2 Composite Cathode Material in Rechargeable Lithium/Sulfur Battery. Rare Metals and Cemented Carbides(2), 45-48. |
| IEEE | [1] LU Hong-guang and PAN Feng, "Preparation and Performance of S/TiO_2 Composite Cathode Material in Rechargeable Lithium/Sulfur Battery," Rare Metals and Cemented Carbides, no. 2, pp. 45-48, 2014. keywords: {rechargeable lithium/sulfur battery;S/TiO2 cathode material;composite material;electrochemical performance} |