Research on Composition of the Reaction Products from Two-stage Carbon Reduction of MoO_3 AITranslate
Abstract AITranslate
MoO3 powders were reduced by two stages with graphite powders as the carbon source. The re- duction products at different stages were characterized by XRD,FESFM and EDS,and then a preliminary discussion was made on the possible reaction mechanism during carbon reduction. The results show that Mo4O11 may be the transitional phase during the carbon reduction of MoO3 to MoO2. MoO3 can be com- pletely reduced with carbon by reaction for 1 h both at 650 ℃ and 1 250 ℃ to obtain metallic molybdenum of high crystallinity and uniform particle size,containing a small amount of a-Mo2 C byproduct.
KeyWords AITranslate
1罗振中.钼的应用及其发展[J].中国钼业,2003,27(2):7-10. 被引量:66
2黄晓玲,薛夏英.一种亚微米级钼粉的制备方法[P].中国专利:201010107245.6,2010-06-30.
3Mohamed H Kahn, Joel Taube, Loyal M Johnson Jr. Molybdenum metal powder [ P ]. US Pat: 7625421, 2009-12-01.
4王廉舫,王彦新.从还原钨钼粉的粒度波动论氢气再生装置[J].硬质合金,2010,27(3):172-176. 被引量:3
5匡社颖.吸附法氢气回收净化工艺在钨钼还原系统中的应用[J].稀有金属与硬质合金,2010,38(3):50-53. 被引量:1
6梁静,李来平,张新.氨分解制氢在钼加工行业的应用进展[J].中国钼业,2011,35(1):46-48. 被引量:3
7Satyajeet Chaudhury, Mukerjee S K, Vaidya V N, et al. Kinetics and mechanism of carbothermic reduction of MoO3 to MoeC[J]. Journal of Alloys and Com- pounds, 1997, 261: 105-113.
8Aydinyana S V, Gumruyana Zh, Manukyan Kh V, et al. Self-sustaining reduction of MoOa by the Mg-C mixture [J]. Materials Science and Engineering B, 2010, 172: 267-271.
1于志涛,王快社,胡平,杨帆,谭江飞,何欢承,康轩齐,王华.低氧TZM合金研究进展[J].材料导报,2015,29(1):92-98. 被引量:11
2张瑞华,郝振华,车玉思,舒永春,孙院军,何季麟.钼粉的制备方法及研究进展[J].稀有金属,2022,46(4):510-522.
1王苗,杨双平,王利东,杨鑫,刘海金.MHC-HfC合金棒材的制备及其高温氧化行为[J].稀有金属,2022,46(10):1278-1286.
2宋瑞,王快社,胡平,杨帆,胡卜亮,于志涛,谭江飞,曹维成,安耿,郭磊.钼及钼合金表面高温抗氧化涂层研究现状[J].材料导报,2016,30(5):69-74. 被引量:15
3郭磊,宋瑞,淡新国,金波,赵娟,张清,胡平.稀土钼合金制备工艺及强韧化机理研究现状[J].中国钼业,2017,41(2):45-51. 被引量:6
4周宇航,胡平,常恬,邓洁,胡卜亮,王快社,冯鹏发.钼合金强韧化方式及机理研究进展[J].功能材料,2018,49(1):1026-1032. 被引量:14
5曹俊,刘伟,朱鹏飞,孙铁龙,李继文,潘昆明,魏世忠.料浆包渗法制备MoSi_2高温抗氧化涂层[J].表面技术,2019,48(1):69-76. 被引量:5
6赵虎.钼及钼合金烧结技术研究及发展[J].粉末冶金技术,2019,37(5):382-391. 被引量:11
7朱鹏飞,刘伟,曹俊,王飞鸿,李继文,潘昆明,魏世忠.钼电极表面Y2O3-玻璃基涂层抗氧化性能研究[J].表面技术,2020,49(4):263-270.
8董帝,康聚磊,熊宁,王承阳.HfC含量对钼钛锆合金显微组织和力学性能的影响[J].粉末冶金技术,2021,39(3):239-244. 被引量:1
9马玉康,侯清宇,马啸宇,光剑锋,唐木生,黄贞益.Cu含量对SPS烧结TZM合金涂层组织及性能的影响[J].稀有金属,2022,46(4):461-470.
10张强,蔡永丰,李晓静,刘赫雄,张楠,周文元,赖陈,董丽然,王金淑.钼合金粉末冶金研究进展[J].粉末冶金技术,2023,41(1):44-54.
1秦凤久.本钢二铁厂冶炼低铁适宜炉渣成分研究[J].辽宁冶金,1989(5):17-22.
2周旺枝,张洪雷,刘黎.活性石灰回转窑用复合砖内衬的研究[J].武钢技术,2014,52(4):28-29. 被引量:1
3周玉昌.配碳比对TiO2真空碳热还原的影响[J].钢铁钒钛,2012,33(6):6-10. 被引量:5
4吴悦梅,易磊隽,王新玲,熊计.WC含量对Ti(C,N)基金属陶瓷显微组织的影响[J].钢铁钒钛,2016,37(6):56-60. 被引量:4
5孙成才,吕有成,刘美晨,王琳,李福华.进口红土镍矿主要成分研究[J].山东国土资源,2015,31(1):23-26.
6孙康,马跃宇,白魁昌,刘凤军.预氧化钛铁矿的还原反应历程[J].中国有色金属学报,1998,8(S2):390-393. 被引量:8
7李长青,武万良,王树成,徐成彦.沉淀法制备氧化铝的相变过程[J].黑龙江科技学院学报,2009,19(6):427-430. 被引量:1
8高蔷,史培阳,刘承军,姜茂发.水热法制备钒酸铁的实验研究[J].功能材料,2014,45(22):22056-22059.
9王碧侠,兰新哲,赵西成,张静.电化学还原法制备金属钛的反应历程研究[J].稀有金属,2010,34(4):618-623. 被引量:6
10温燕明,陈昌华,孔凡朔.高炉喷吹用煤的摩擦电选实验研究[J].钢铁,2006,41(2):11-15. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF803.12[冶金工程—有色金属冶金]
Citation Information:
MoO3 powders were reduced by two stages with graphite powders as the carbon source. The re- duction products at different stages were characterized by XRD,FESFM and EDS,and then a preliminary discussion was made on the possible reaction mechanism during carbon reduction. The results show that Mo4O11 may be the transitional phase during the carbon reduction of MoO3 to MoO2. MoO3 can be com- pletely reduced with carbon by reaction for 1 h both at 650 ℃ and 1 250 ℃ to obtain metallic molybdenum of high crystallinity and uniform particle size,containing a small amount of a-Mo2 C byproduct.
quote
| GB/T 7714-2015 | [1] LIN Yu-lin, CHEN Tong-yun, HUANG Xian-fa, et al. Research on Composition of the Reaction Products from Two-stage Carbon Reduction of MoO_3[J]. Rare Metals and Cemented Carbides, 2013(1): 28-31. |
| MLA | [1] LIN Yu-lin, et al., "Research on Composition of the Reaction Products from Two-stage Carbon Reduction of MoO_3." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 28-31. |
| APA | [1] LIN Yu-lin, CHEN Tong-yun, HUANG Xian-fa, GUI Lin, & ZHAO Jing-xia. (2013). Research on Composition of the Reaction Products from Two-stage Carbon Reduction of MoO_3. Rare Metals and Cemented Carbides(1), 28-31. |
| IEEE | [1] LIN Yu-lin, CHEN Tong-yun, HUANG Xian-fa, GUI Lin, and ZHAO Jing-xia, "Research on Composition of the Reaction Products from Two-stage Carbon Reduction of MoO_3," Rare Metals and Cemented Carbides, no. 1, pp. 28-31, 2013. keywords: {MoO3;two-stage carbon reduction;reaction product;composition} |