Study on Fine-grained Tantalum Carbide Preparation by In-situ Diffusion Reaction AITranslate

Xuchang Xuji Wind Power Technology Co., Ltd.;Xuchang Xuji Wind Power Technology Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using waste tantalum as the raw material and high-carbon iron as the carbon carrier, the fine grained TaC was produced by solid-liquid diffusion reaction during smelting combined with acid leaching. The products were characterized by XRD and SEM. The results show that carbon atoms react with tanta lure by diffusion during smelting and heat preservation, to form TaC grains in a-Fe matrix. After acid leac hing,shattering and ball milling of the TaC/Fe complex,the fine-grained TaC can be obtained with a parti cle size of about μm.

KeyWords AITranslate

fine-grained TaC waste tantalum high-carbon iron smelting heat preservation acid leaching

1周菊秋,黄列如,谭日善,张同桂,李光辉,曾芳屏.中国钽、铌碳化物的生产和应用[J].稀有金属材料与工程,1998,27(1):26-31. 被引量:14

2汤仁中.两次碳化法制取细颗粒碳化钽的工艺研究[J].稀有金属与硬质合金,2000,28(1):5-9. 被引量:5

3谭卫宁.自蔓延高温合成TaC粉末[J].湖南化工,1998,28(2):27-29. 被引量:2

4杜银霄.Facile Route to Prepare TaC,NbC and WC Nanoparticles[J].武汉理工大学学报:材料科学英文版,2008,23(6):779-782. 被引量:1

1李建钢.一种陶瓷烧结的新工艺及其配套设备[J].景德镇陶瓷,1998,8(1):12-13.

2石天宝.开发和应用钌基氨合成催化剂[J].化工进展,1993,12(6):46-51. 被引量:5

3王祝堂.冷空气烧嘴与再生烧嘴的能耗比较[J].轻合金加工技术,2010(1):44-44.

4冷空气烧嘴与再生烧嘴的能耗比较[J].轻合金加工技术,2009(11):26-26.

5程振民,刘国群,袁渭康.固定床反应器中扩散反应问题的实验测定[J].化学反应工程与工艺,1995,11(2):173-180. 被引量:2

6E.Molga,S.Wronski,钟妙坤.获取高纯物质的动态过滤——洗涤过程模拟[J].化工装备技术,1990,11(4):38-43.

7王岚,高学绪.金刚石单晶与其表面钛镀膜之间扩散反应的定量相分析[J].粉末冶金技术,1997,15(2):146-148.

8周飞,李志章,罗启富.通过Cu/Ti液相扩散反应进行Si_3N_4/Cu的连接[J].浙江大学学报:工学版,2001,35(1):109-112.

9李庆刚,张新恩,刘硕.直接甲醇燃料电池碳载铂基电催化剂的研究进展[J].材料导报:纳米与新材料专辑,2015,29(1):148-150.

10袁浩,汪洋.对苯二甲酸加氢精制催化剂的研究进展[J].合成纤维工业,2009,32(4):52-55. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ135.13[化学工程—无机化工]

Citation Information:

Using waste tantalum as the raw material and high-carbon iron as the carbon carrier, the fine grained TaC was produced by solid-liquid diffusion reaction during smelting combined with acid leaching. The products were characterized by XRD and SEM. The results show that carbon atoms react with tanta lure by diffusion during smelting and heat preservation, to form TaC grains in a-Fe matrix. After acid leac hing,shattering and ball milling of the TaC/Fe complex,the fine-grained TaC can be obtained with a parti cle size of about μm.

quote

GB/T 7714-2015 [1] LI Cheng-chen, SONG Ke. Study on Fine-grained Tantalum Carbide Preparation by In-situ Diffusion Reaction[J]. Rare Metals and Cemented Carbides, 2013(1): 32-34.
MLA [1] LI Cheng-chen, and SONG Ke. "Study on Fine-grained Tantalum Carbide Preparation by In-situ Diffusion Reaction." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 32-34.
APA [1] LI Cheng-chen, & SONG Ke. (2013). Study on Fine-grained Tantalum Carbide Preparation by In-situ Diffusion Reaction. Rare Metals and Cemented Carbides(1), 32-34.
IEEE [1] LI Cheng-chen and SONG Ke, "Study on Fine-grained Tantalum Carbide Preparation by In-situ Diffusion Reaction," Rare Metals and Cemented Carbides, no. 1, pp. 32-34, 2013. keywords: {fine-grained TaC;waste tantalum;high-carbon iron;smelting;heat preservation;acid leaching}