daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Impurity Removal Efficiency of the Extraction Process with P204 from Lepidolite Leaching Solution AITranslate

School of Materials Science and Engineering, Jiangxi Institute of Technology;Jiangxi Jiangtungsten Rare Earth Technology Development Co., Ltd.;Ganzhou Nonferrous Metallurgical Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

P204-sulphonated kerosene system was used to extract A1,Fe and Mn impurities from lepidolite leaching solution to separate the main metal Li. Influences were investigated of phase ratio, extractant con- centration,initial water phase pH value and extraction time on A1,Fe and Mn extraction rates. The optimal extraction technical conditions were determined as follows:P204 concentration of 1.5 tool/L, phase ratio of 1/1 ,initial water phase pH value of 2.5 ,and extraction time of 18 min. Under the above conditions and by single-stage extraction, the extraction rates of AI,Fe and Mn are 99.1 %,99.3% and 99.0%, respectively, only with lithium loss of 6. 9%. The optimum separation are realized of aluminum, iron and manganese from lithium.

KeyWords AITranslate

lepidolite leaching solution P204 solvent extraction purification and impurity removal techni-cal condition

1汪剑岭,王继民,朱建春,周金云,顾玉行.硫酸盐法从锂云母制取碳酸锂的研究[J].新疆有色金属,1996,19(1):85-89. 被引量:17

2张选旭.宜春锂云母采用硫酸盐法制取碳酸锂工艺净化除杂试验[J].江西有色金属,1995,9(1):45-47. 被引量:5

3胡建锋,朱云.P204萃取硫酸体系中钒的性能研究[J].稀有金属,2007,31(3):367-370. 被引量:39

4汤兵,朱又春,白雪梅,蔡斌,陈丽卿,张俊浩.溶剂萃取法从镀锌酸洗废液中分离锌、铁的研究[J].矿冶工程,2003,23(5):47-49. 被引量:16

5徐美燕,马燕,孙贤波,赵庆祥.萃取法回收水厂污泥中铝的技术研究 Ⅰ.清液萃取法[J].华东理工大学学报:自然科学版,2007,33(3):369-374. 被引量:7

6王成彦,王含渊,江培海,尹飞,陈永强.P204萃取分离钴锰铁试验研究[J].有色金属:冶炼部分,2006(5):2-5. 被引量:20

7伍静静,李登新.P204-仲辛醇皂化萃取氰化尾渣酸浸液中铁的初步研究[J].矿冶工程,2011,31(1):57-62. 被引量:4

8胡威,黄兴远,李小理.低浓度钴溶液除铁、钙、镁和P204深度除杂工艺研究[J].稀有金属与硬质合金,2011,39(3):10-12. 被引量:17

1周志全,赵凤岐,舒祖骏,张永明,支梅峰,邓慧东,任燕.高浓度硫酸体系中铀与铁的HDEHP萃取分离[J].湿法冶金,2018,37(6):468-473. 被引量:1

2苏慧,朱兆武,王丽娜,齐涛.矿石资源中锂的提取与回收研究进展[J].化工学报,2019,70(1):10-23. 被引量:22

1刘爽,王水龙,邢新龙,汪龙飞,张也.江西省锂矿资源分布、矿床类型及找矿前景[J].资源环境与工程,2019,33(2):195-198. 被引量:7

2李想.基于数据挖掘的矿石金属元素分离与提取方法研究[J].世界有色金属,2019,0(13):239-240.

3尚玺,孟宇航,张乾,杨华明.富锂矿物的锂提取与战略性应用[J].矿产保护与利用,2019,39(6):152-158. 被引量:5

4吴进方,曾小毛,刘剑叶,南天,南东东.关于从锂瓷石矿原料中提取锂方法分析研究[J].世界有色金属,2020(12):125-126.

5傅昕,王玲.硅酸盐矿石资源中铷的提取工艺综述[J].矿产综合利用,2020(6):171-179. 被引量:8

6伍德佑,潘湛昌,刘志强.从废旧锂离子电池中回收制备磷酸锂的工艺研究[J].材料研究与应用,2020,14(4):312-316. 被引量:1

7程籽毅,魏卓,何智妍,肖淑云,王彦旭,周堃.三元体系Li^(+),NH_(4)^(+)∥SO_(4)^(2-)-H_(2)O 298 K相平衡研究[J].矿产保护与利用,2021,41(1):141-145.

8米茂龙,严润华.锂辉石提锂工艺综述[J].广州化工,2021,49(14):22-24. 被引量:4

9朱丽,杨永琼,顾汉念,温汉捷,杜胜江,罗重光.电感耦合等离子体质谱-X射线衍射法研究云南玉溪和美国内华达地区黏土型锂资源矿物学特征[J].岩矿测试,2021,40(4):532-541. 被引量:1

10韩佳欢,乜贞,方朝合,伍倩,曹倩,王云生,卜令忠,余疆江.中国锂资源供需现状分析[J].无机盐工业,2021,53(12):61-66. 被引量:32

1和晓才,谢刚,李怀仁,杨大锦,徐庆鑫.高铁、高硅溶液中萃取钼[J].有色金属:冶炼部分,2012(1):16-19. 被引量:4

2何宾宾,梁玉军,杨超,田熙科,皮振邦.电解金属锰合格液中锰镁的萃取分离研究[J].中国锰业,2010,28(1):41-44. 被引量:16

3曾冬铭,舒万艮,刘又年,雷存喜.低酸浸出-溶剂萃取法从含铟渣中回收铟[J].有色金属,2002,54(3):41-44. 被引量:29

4俞宏伟,陈虹,刘润,张勇.从含钼的P204—煤油体系中反萃取钼的研究[J].浙江化工,1998,29(1):40-41.

5王玮.氧化铜矿硫酸搅拌浸出工艺研究[J].中国资源综合利用,2016,34(12):23-25. 被引量:2

6张莹,张廷安.N1923萃取钒渣无焙烧浸出液中钒的实验探究[J].有色金属科学与工程,2015,6(6):14-19. 被引量:6

7汤兵,朱又春,白雪梅,蔡斌,陈丽卿,张俊浩.溶剂萃取法从镀锌酸洗废液中分离锌、铁的研究[J].矿冶工程,2003,23(5):47-49. 被引量:16

8严明英.溶剂萃取在硫化铜矿的湿法工艺中的应用研究[J].重庆钢研,1997(22):19-28.

9范元俊.铟萃取工艺条件的探讨[J].株冶科技,2001,29(1):18-20. 被引量:7

10段丽萍,许延辉,徐海平,胡卫红,郭文亮.蓖麻油脂肪酸对铝和钕共萃取行为的机理研究[J].湿法冶金,2008,27(1):19-21.

Basic Information:

DOI:

Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]

Citation Information:

P204-sulphonated kerosene system was used to extract A1,Fe and Mn impurities from lepidolite leaching solution to separate the main metal Li. Influences were investigated of phase ratio, extractant con- centration,initial water phase pH value and extraction time on A1,Fe and Mn extraction rates. The optimal extraction technical conditions were determined as follows:P204 concentration of 1.5 tool/L, phase ratio of 1/1 ,initial water phase pH value of 2.5 ,and extraction time of 18 min. Under the above conditions and by single-stage extraction, the extraction rates of AI,Fe and Mn are 99.1 %,99.3% and 99.0%, respectively, only with lithium loss of 6. 9%. The optimum separation are realized of aluminum, iron and manganese from lithium.

quote

GB/T 7714-2015 [1] WANG Lin-sheng, WANG Fa-bo, WEN Xiao-qiang. Study on Impurity Removal Efficiency of the Extraction Process with P204 from Lepidolite Leaching Solution[J]. Rare Metals and Cemented Carbides, 2013(1): 24-27.
MLA [1] WANG Lin-sheng, et al., "Study on Impurity Removal Efficiency of the Extraction Process with P204 from Lepidolite Leaching Solution." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 24-27.
APA [1] WANG Lin-sheng, WANG Fa-bo, & WEN Xiao-qiang. (2013). Study on Impurity Removal Efficiency of the Extraction Process with P204 from Lepidolite Leaching Solution. Rare Metals and Cemented Carbides(1), 24-27.
IEEE [1] WANG Lin-sheng, WANG Fa-bo, and WEN Xiao-qiang, "Study on Impurity Removal Efficiency of the Extraction Process with P204 from Lepidolite Leaching Solution," Rare Metals and Cemented Carbides, no. 1, pp. 24-27, 2013. keywords: {lepidolite leaching solution;P204;solvent extraction;purification and impurity removal;techni-cal condition}