Experimental Research on Rhenium Separation from Molybdenum in the Leaching Solution of Molybdenum Concentrate AITranslate
Abstract AITranslate
With molybdenum concentrate leaching solution as the object of study, effective separation ofrhenium from molybdenum was achieved by ion exchange experiments. The results show that the adsorp- tion rate of rhenium is 99.97% and its saturated adsorption capacity is 43.66 g/kg,with 201# resin as the ion adsorbent and under the optimal conditions of leaching solution pH of 8. 5 and flow velocity of 20 mL/min. The desorption rate of rhenium is 99.99% with 9% NH4SCN as the strippant. 201~ resinhasgood regeneration performance, suitable for recycling.
KeyWords AITranslate
1常宝乾,徐彪,李营生,阳建国.钼精矿固化焙烧-树脂交换法回收铼的工艺研究[J].矿产综合利用,2011(4):22-25. 被引量:8
2王海哲,杨盛良.铼的特性、应用及其制造技术[J].中国稀土学报,2005,23(S2):189-193. 被引量:18
3于世昆,伍艳辉.铼的分离提取研究进展[J].中国钼业,2010,34(2):7-12. 被引量:30
4邱朝辉,钟宏,曹占芳,姚禛.铼的分离分析方法研究进展[J].稀有金属与硬质合金,2010,38(1):56-59. 被引量:13
5张俊,姚林,吕改芳,邓桂春.D-314树脂动态分离钼铼的研究[J].稀有金属,2010,34(1):85-89. 被引量:14
6廖秋玲,高竹青.离子交换法从烟道灰中提取铼的工艺研究[J].中国资源综合利用,2011,29(12):18-21. 被引量:6
7马红周,王耀宁,兰新哲.树脂富集钼精矿焙烧烟尘浸出液中铼的研究[J].西安建筑科技大学学报:自然科学版,2005,37(4):584-586. 被引量:7
1吉鸿安,鲁兴武.钼酸铵溶液中锌净化新工艺的研究[J].稀有金属与硬质合金,2016,0(3):5-8.
2陈昆昆,孟晗琪,吴永谦,吴贤.从废旧高温合金中提取Re的试验研究[J].稀有金属与硬质合金,2016,44(6):26-30. 被引量:8
3刘伟,丁留亮,郭明宜,李继文,魏世忠.钼冶金中铼的综合提取研究进展[J].稀有金属与硬质合金,2017,45(5):1-6. 被引量:4
1陈昆昆,许万祥,郭瑞,操齐高.从高温合金电溶液中回收铼酸铵的工业试验[J].有色金属:冶炼部分,2018(7):31-34. 被引量:4
2刘伟,丁留亮,朱鹏飞,李继文,魏世忠.Purolite A172树脂对铼和钼的静态分离[J].中国有色金属学报,2019,29(7):1519-1527. 被引量:1
3陈昆昆,操齐高,张卜升,孟晗琪,赵盘巢.高温合金酸浸液回收高纯铼酸铵试验研究[J].有色金属:冶炼部分,2019,0(9):45-48. 被引量:6
4郭瑞,许万祥,王靖坤,李波,李进,周严.含钌含铼高温合金电化学溶解工艺研究[J].有色金属:冶炼部分,2019,0(8):57-60. 被引量:2
5郭瑞,许万祥,王靖坤,周严,李进.含钌含铼阳极泥处理工艺研究[J].有色金属:冶炼部分,2019,0(10):55-57. 被引量:1
6鲁兴武,李守荣,张恩玉,程亮,李俞良,牛永胜.铜冶炼污酸中铼富集工艺技术研究[J].有色金属:冶炼部分,2020,0(4):47-50. 被引量:9
7张春伟,孙元,唐俊杰,房大维.工业废料中铼元素的回收与再利用研究进展[J].材料导报,2020,34(15):15145-15152. 被引量:2
8卢晓锋,朱纪念,卢苏君,李亦婧,赵淑琴,郭勇.高温合金中铼金属回收制备高纯铼酸铵研究[J].稀有金属,2021,45(8):972-979. 被引量:3
9黄宗朋,沈裕军,彭俊,周小舟,蔡云卓,沈凌畅.铜冶炼污酸中铼的提取分离技术研究进展[J].稀有金属与硬质合金,2022,50(1):23-26. 被引量:1
10陈昆昆,李林波,操齐高,孟晗琪.从沉钨钼后液中制备高纯铼酸铵[J].稀有金属材料与工程,2022,51(8):3049-3056.
1高岗强,李守诚.粘结剂对高铝粉煤灰球团强度的影响研究[J].内蒙古科技与经济,2012(3):92-93.
2隋丽丽,翟玉春,葛欣,任红.硫酸铵焙烧钛渣提钛的研究[J].矿冶,2016,25(2):40-43. 被引量:1
3宋招权.MgO对球团矿质量的影响[J].烧结球团,2001,26(6):22-24. 被引量:37
4曹耀华,李清,高照国,刘红召,王威.低品位金钼混合精矿提取金钼新工艺[J].有色金属:冶炼部分,2014(7):42-44. 被引量:1
5余清,王艳,任春生,应海松.高频燃烧红外吸收法测定铬矿石及精矿中的硫[J].金属矿山,2007(9):74-75. 被引量:10
6王振文,王成彦,卢惠民.含锡铁精矿还原焙烧脱锡试验研究[J].矿冶,2005,14(2):63-66. 被引量:12
7邵传兵,李守荣,马琳亭,张恩玉,李俞良.提高氧化锌烟尘中铟浸出率试验研究[J].矿冶,2016,25(1):41-44. 被引量:4
8钟爱国,王宏青,王劲松,李玉白.离子交换分离钨钼及微波诱导树脂再生的研究[J].离子交换与吸附,1999,15(3):228-234.
9吴人驹.离子交换法除钼及其树脂再生的化学原理初探[J].中国钨业,1997,0(6):18-20. 被引量:3
10何星存,谢祖芳,陈孟林.聚酰胺树脂吸附钯的性能研究[J].贵金属,2003,24(4):16-20. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
With molybdenum concentrate leaching solution as the object of study, effective separation ofrhenium from molybdenum was achieved by ion exchange experiments. The results show that the adsorp- tion rate of rhenium is 99.97% and its saturated adsorption capacity is 43.66 g/kg,with 201# resin as the ion adsorbent and under the optimal conditions of leaching solution pH of 8. 5 and flow velocity of 20 mL/min. The desorption rate of rhenium is 99.99% with 9% NH4SCN as the strippant. 201~ resinhasgood regeneration performance, suitable for recycling.
quote
| GB/T 7714-2015 | [1] QI Dong, WANG Yi. Experimental Research on Rhenium Separation from Molybdenum in the Leaching Solution of Molybdenum Concentrate[J]. Rare Metals and Cemented Carbides, 2013(1): 20-23. |
| MLA | [1] QI Dong, and WANG Yi. "Experimental Research on Rhenium Separation from Molybdenum in the Leaching Solution of Molybdenum Concentrate." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 20-23. |
| APA | [1] QI Dong, & WANG Yi. (2013). Experimental Research on Rhenium Separation from Molybdenum in the Leaching Solution of Molybdenum Concentrate. Rare Metals and Cemented Carbides(1), 20-23. |
| IEEE | [1] QI Dong and WANG Yi, "Experimental Research on Rhenium Separation from Molybdenum in the Leaching Solution of Molybdenum Concentrate," Rare Metals and Cemented Carbides, no. 1, pp. 20-23, 2013. keywords: {molybdenum concentrate leaching solution;rhenium;molybdenum;201# resin;ion exchange} |