A New Process for Molybdenum-Tungsten Extraction from High Pressure Leaching Solution of Crude Molybdenum-Tungsten Oxide Concentrate AITranslate
Abstract AITranslate
A new process of molybdenum-tungsten extraction from high pressure leaching solution of crude molybdenum-tungsten oxide concentrate was studied,including the steps of solution pre-treatment, molyb- denum-tungsten precipitation, solid-liquid separation, product drying and so on. When the high pressure leaching solution contains 27.26 g/L Mo and 5.70 g/L WOa ,Mo and WOa precipitation rates are 99.94% and 85.08 %, respectively, under the conditions of pH value of 7-8, precipitation time of 1-1.5 h, reaction temperature of 80 ℃, and CaC12 dosage of 2. 15 times the theoretical value, and the calcium molybdate- tungstate product contains 36.08% Mo and 7.11% WO3 ,with impurity of 0. 012% P and 0. 004 5% As. The new process has simple flowsheet,good operability and high molybdenum-tungsten recovery.
KeyWords AITranslate
1曹耀华,刘红召,高照国,杨绍文.低品位氧化钼精矿高压浸出新工艺[J].有色金属:冶炼部分,2011(1):5-8. 被引量:7
2皮关华,徐徽,陈白珍,石西昌,李俊丽.从难选镍钼矿中回收钼的研究[J].湖南有色金属,2007,23(1):9-12. 被引量:42
3李青刚,张启修,肖连生.离子交换树脂吸附镍钼矿氯浸液中钼的研究[J].稀有金属,2007,31(3):351-356. 被引量:14
4盘茂森,朱云.高压浸出钼酸钙中钼的实验研究[J].中国钼业,2005,29(6):19-21. 被引量:20
5李青刚,肖连生,张贵清,张启修.镍钼矿生产钼酸铵全湿法生产工艺及实践[J].稀有金属,2007,31(S1):85-89. 被引量:52
6符剑刚,王晖,钟宏,常庆伟,魏志锋,马盛韬.从彩钼铅矿中提取钼的研究现状[J].稀有金属与硬质合金,2007,35(1):41-43. 被引量:12
7张文朴.我国钼资源综合利用及再生研发的进展[J].资源再生,2007(1):67-70. 被引量:1
8汪胜东,蒋训雄,王海北,范艳青,张邦胜,王玉芳.贵州某彩钼铅矿碱浸工艺研究[J].有色金属,2007,59(3):65-67. 被引量:10
1张鸿彪,牟文宁,宋佩,卢媛嫄,孙雷雷.钼矿冶炼新工艺发展概论[J].材料导报:纳米与新材料专辑,2013,27(2):87-90. 被引量:5
2Fei Cao,Wei Wang,De-zhou Wei,Wen-gang Liu.Separation of tungsten and molybdenum with solvent extraction using functionalized ionic liquid tricaprylmethylammonium bis(2,4,4-trimethylpentyl)phosphinate[J].矿物冶金与材料学报:英文版,2021,28(11):1769-1776. 被引量:1
1陈德良,董会娜,张锐.二硫化钼基纳米复合材料的构筑与应用[J].郑州大学学报:工学版,2015,36(6):18-29.
2黄万抚,李英杰,李新冬,梁娟,陈洋,刘玉娇.纳滤技术在矿冶领域的应用研究进展[J].工业水处理,2016,36(11):1-4. 被引量:5
3李建涛,庄肃凯,南宁,李凯斌,朱明明.浸矿菌的选育及对低品位钼矿的浸出试验研究[J].金属矿山,2018,47(5):103-107. 被引量:1
4郜伟,张永禄,揭晓武,余群波.钼精矿氧化焙烧试验研究[J].中国资源综合利用,2020,38(10):12-14.
5夏新兵,张贵清,关文娟,曾理,巫圣喜,李青刚,曹佐英.采用TRPO从过氧化氢溶液中萃取钼和钨的数学模型和反应机理[J].中国有色金属学报:英文版,2022,32(9):3123-3135.
6赵欢,张广积,杨巧文,李媛媛,吴涛,杨超.低品位钼尾矿生物浸出实验研究[J].稀有金属与硬质合金,2015,43(6):7-11. 被引量:2
1和晓才.生产钨酸钙过程中的除钼工艺[J].云南冶金,2008,37(1):33-35. 被引量:1
2冯慧君,王洪杰,刘小明.低品位氧化钼钨精矿高温高压碱浸工艺工业生产实践[J].矿冶工程,2013,33(4):98-100. 被引量:3
3范树森.钨酸钙的粒度控制及白钨母液中钨的回收[J].稀有金属与硬质合金,1993,21(2):13-16. 被引量:2
4范树森.钨酸钙沉淀的粒度控制[J].中国钨业,1993,0(8):15-17.
5瑞林.美国难熔金属协会抑制中国钨进口[J].中国钨业,1993,0(8):32-32.
6А.С.Медведев,秦川.酸分解白钨精矿的方法[J].中国钨业,1993,0(4):27-29.
7李裕芳,赖道玉.不同颗粒人造白钨的制取[J].中国钨业,1990(11):11-14. 被引量:2
8刘吉刚,李正邦,刘彦华,杨海森,梁林宝.钨酸钙球团碳化硅还原试验研究[J].有色金属:冶炼部分,2013(3):20-23.
9殷家旺,舒国兵.电炉初炼钢As含量来源分析[J].柳钢科技,2007(F09):121-123.
10殷家旺,舒国兵.电炉初炼钢As含量来源分析[J].鄂钢科技,2007,0(3):1-2.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
A new process of molybdenum-tungsten extraction from high pressure leaching solution of crude molybdenum-tungsten oxide concentrate was studied,including the steps of solution pre-treatment, molyb- denum-tungsten precipitation, solid-liquid separation, product drying and so on. When the high pressure leaching solution contains 27.26 g/L Mo and 5.70 g/L WOa ,Mo and WOa precipitation rates are 99.94% and 85.08 %, respectively, under the conditions of pH value of 7-8, precipitation time of 1-1.5 h, reaction temperature of 80 ℃, and CaC12 dosage of 2. 15 times the theoretical value, and the calcium molybdate- tungstate product contains 36.08% Mo and 7.11% WO3 ,with impurity of 0. 012% P and 0. 004 5% As. The new process has simple flowsheet,good operability and high molybdenum-tungsten recovery.
quote
| GB/T 7714-2015 | [1] CAO Yao-hua, WANG Hong-jie, LIU Hong-zhao, et al. A New Process for Molybdenum-Tungsten Extraction from High Pressure Leaching Solution of Crude Molybdenum-Tungsten Oxide Concentrate[J]. Rare Metals and Cemented Carbides, 2013(1): 17-19. |
| MLA | [1] CAO Yao-hua, et al., "A New Process for Molybdenum-Tungsten Extraction from High Pressure Leaching Solution of Crude Molybdenum-Tungsten Oxide Concentrate." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 17-19. |
| APA | [1] CAO Yao-hua, WANG Hong-jie, LIU Hong-zhao, & GAO Zhao-guo. (2013). A New Process for Molybdenum-Tungsten Extraction from High Pressure Leaching Solution of Crude Molybdenum-Tungsten Oxide Concentrate. Rare Metals and Cemented Carbides(1), 17-19. |
| IEEE | [1] CAO Yao-hua, WANG Hong-jie, LIU Hong-zhao, and GAO Zhao-guo, "A New Process for Molybdenum-Tungsten Extraction from High Pressure Leaching Solution of Crude Molybdenum-Tungsten Oxide Concentrate," Rare Metals and Cemented Carbides, no. 1, pp. 17-19, 2013. keywords: {crude molybdenum-tungsten oxide concentrate;high pressure leaching solution;molybdenum-tungsten precipitation;calcium molybdate-tungstate} |