Effects of Thermal Hydrogenation on Microstructure and Phase Transition of TB8 Alloy AITranslate

College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogen element was implanted into TB8 titanium alloy by thermal hydrogenation. Microstructure and phase composition of hydrogenation TB8 titanium alloy were studied by OM, SEM and XRD. Effects of hydrogen on the phase transition point and elemental distribution of TB8 titanium alloy were analyzed by DTA and EDS. The results show that with hydrogen content increasing,β phase in the alloy decreases at first and then increases. Hydrogenation on the one hand reduces the critical cooling rate of co phase generation in the alloy,on the other hand reduces (α+β)/β phase transition temperature of TB8 titanium alloy. In addition, Hydrogenation promotes alloy element redistribution and phase transition from a

KeyWords AITranslate

TB8 titanium alloy thermal hydrogenation hydrogen content microstructure phase transition

1张青,李萍,薛克敏.Ti-15-3合金高温变形机制分析[J].合肥工业大学学报:自然科学版,2006,29(10):1189-1191. 被引量:4

2周晓虎,马文革,俞汉清,朱知寿.TB8超高强度钛合金热工艺参数研究[J].材料工程,2003,31(8):37-39. 被引量:19

3沈桂琴,徐斌,彭益群,脱祥明.Ti-15Mo-2.7Nb-3Al-0.2Si高强钛合金的相变[J].材料工程,1999(3):19-23. 被引量:11

4侯红亮,李志强,王亚军,关桥.钛合金热氢处理技术及其应用前景[J].中国有色金属学报,2003,13(3):533-549. 被引量:125

5黄东,南海,吴鹤,赵嘉琪.氢处理技术在钛合金中的应用[J].金属热处理,2004,29(6):44-48. 被引量:14

1梁培新,朱卫东,杨刚,翟月雯,周乐育.渗氢工艺对TA15钛合金氢含量和显微组织的影响[J].锻压技术,2020,45(8):190-194. 被引量:4

1郝国建,杨刚,梁培新,朱卫东,孙剑飞,陈哲铭.热氢处理对TA15钛合金组织及性能的影响[J].金属热处理,2021,46(1):38-42.

2韩秀峰,王伦,朱明亮,廖仲祥,张露.TA19钛合金电子束焊接头微观组织与性能研究[J].稀有金属,2021,45(7):778-785. 被引量:8

3罗登超,王云,李维.不同工艺制备TA15钛合金管材[J].锻压技术,2022,47(8):118-122.

4齐铭,安震,张凯,孟广慧,丁旭.热处理对锻压TA15钛合金棒组织和性能的调控[J].锻压技术,2022,47(8):193-199.

1李萍,江政,袁宝国,薛克敏.置氢对TB8钛合金室温压缩性能的影响[J].塑性工程学报,2012,19(6):15-18. 被引量:2

2张鹏省,曾卫东,赵永庆.钛及钛合金热氢处理技术[J].热加工工艺,2009,38(12):133-136. 被引量:1

3曹兴民,赵永庆,奚正平.热氢处理在铸造钛合金中的应用[J].铸造,2005,54(4):391-393. 被引量:10

4危卫华,徐九华,傅玉灿.置氢处理对钛合金切削时刀具磨损形态的影响[J].热加工工艺,2015,44(20):128-130. 被引量:1

5危卫华,徐九华,傅玉灿,杨树宝,侯红亮,王耀奇,李志强.置氢钛合金TC4的切削加工性研究[J].南京航空航天大学学报,2009,41(5):633-638. 被引量:10

6张青,李萍,薛克敏.TB8合金再结晶组织的分形特征[J].材料研究与应用,2011,5(1):31-34. 被引量:6

7周游,王忠堂,宋鸿武,张士宏.氢含量及工艺参数对Ti600合金激活能的影响[J].热加工工艺,2009(4):20-23. 被引量:1

8戚运莲,洪权,卢亚锋,曾立英,杜宇,刘伟,郭萍.氢对钛合金组织及加工性能的影响[J].钛工业进展,2010,27(6):10-15. 被引量:12

9王震,洪权,赵永庆.钛合金热变形行为研究[J].钛工业进展,2010,27(3):13-18. 被引量:15

10李萍,段园培,薛克敏,王晓溪,甘国强.TB8钛合金的热变形组织与织构[J].中国有色金属学报,2010,20(5):872-877. 被引量:14

Basic Information:

DOI:

Chinese Library Classification Number:TG166.5[金属学及工艺—热处理]

Citation Information:

Hydrogen element was implanted into TB8 titanium alloy by thermal hydrogenation. Microstructure and phase composition of hydrogenation TB8 titanium alloy were studied by OM, SEM and XRD. Effects of hydrogen on the phase transition point and elemental distribution of TB8 titanium alloy were analyzed by DTA and EDS. The results show that with hydrogen content increasing,β phase in the alloy decreases at first and then increases. Hydrogenation on the one hand reduces the critical cooling rate of co phase generation in the alloy,on the other hand reduces (α+β)/β phase transition temperature of TB8 titanium alloy. In addition, Hydrogenation promotes alloy element redistribution and phase transition from a

quote

GB/T 7714-2015 [1] JIANG Zheng, LI Ping, YUAN Bao-guo, et al. Effects of Thermal Hydrogenation on Microstructure and Phase Transition of TB8 Alloy[J]. Rare Metals and Cemented Carbides, 2012(6): 23-26.
MLA [1] JIANG Zheng, et al., "Effects of Thermal Hydrogenation on Microstructure and Phase Transition of TB8 Alloy." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 23-26.
APA [1] JIANG Zheng, LI Ping, YUAN Bao-guo, & XUE Ke-min. (2012). Effects of Thermal Hydrogenation on Microstructure and Phase Transition of TB8 Alloy. Rare Metals and Cemented Carbides(6), 23-26.
IEEE [1] JIANG Zheng, LI Ping, YUAN Bao-guo, and XUE Ke-min, "Effects of Thermal Hydrogenation on Microstructure and Phase Transition of TB8 Alloy," Rare Metals and Cemented Carbides, no. 6, pp. 23-26, 2012. keywords: {TB8 titanium alloy;thermal hydrogenation;hydrogen content;microstructure;phase transition}