Effects of Ti Doping Amount on Microstructure and Properties of TZM Alloy AITranslate
Abstract AITranslate
TZM alloys doped with different amount of Ti were prepared by powder metallurgy,their micro- structure is observed by SEM, and their microhardness was also measured. Gleeble 1500 thermal/mechanical testing machine was employed to simulate the heating and deformation process of the alloys at high temperature,and then stress-strain curves were drawn. The results show that higher Ti doping amount results in more and more obvious enrichment of Ti and Zr oxide or simple substance at the alloy grain boundaries to strengthen the alloy. The alloy microhardness increases first and then decreases with Ti doping amount increasing,and reaches a maximum with 0.6% TiH2 content. High temperature deformation resistance of the alloys is improved with higher Ti doping amount.
KeyWords AITranslate
1潘叶金.钼、钨及其合金[J].中国钼业,2001,25(2):44-47. 被引量:12
2张全孝,刘全利,熊晓松,贾万明,杨玉君.钼合金在结构件应用方面的发展[J].兵器材料科学与工程,2001,24(4):58-60. 被引量:12
3王东辉,袁晓波,李中奎,郑欣,张军良,张清,白润.钼及钼合金研究与应用进展[J].稀有金属快报,2006,25(12):1-7. 被引量:89
4都业志 张相一 孙院军.TZM合金中第二相组织行为分析与控制.稀有金属材料与工程,2002,31(2):115-118.
5吴新光,杜晓斌.TZM合金及其特性[J].中国钼业,2005,29(5):30-31. 被引量:40
6黄强,李青,宋尽霞,王定刚,韩雅芳.TZM合金的研究进展[J].材料导报,2009,23(21):38-42. 被引量:20
7蔡宗玉.TZM钼合金强化机理分析[J].钼业经济技术,1991(3):70-73. 被引量:5
8成会朝,范景莲,刘涛,陈玉柏,田家敏.TZM钼合金制备技术及研究进展[J].中国钼业,2008,32(6):40-45. 被引量:33
9范景莲,成会朝,卢明园,黄伯云,田家敏.微量合金元素Ti、Zr对Mo金性能和显微组织的影响[J].稀有金属材料与工程,2008,37(8):1471-1474. 被引量:42
1舒先进,张淑琴,宋志刚.00Cr22Ni5Mo3N双相不锈钢热加工性能的试验研究[J].钢管,2004,33(6):15-19. 被引量:27
2方淑芳.利用热模拟技术探讨微Ti对低碳钢热变形特性的影响[J].攀钢技术,1996,19(3):58-61.
3李萍,薛克敏,吕炎.热变形参数对Ti-15-3合金流动应力的影响[J].哈尔滨工业大学学报,2000,32(4):29-32. 被引量:1
4葛懋琦,程晓茹,李虎兴,罗德信,郑琳.变形条件对X65钢高温变形抗力的影响[J].钢铁,1997,32(5):44-50. 被引量:5
5朱向炜,张国赏,魏世忠,徐流杰,崔超鹏.Ti、Zr加入形式对TZM合金组织和性能的影响[J].稀有金属与硬质合金,2013,41(4):30-33.
6靳芳芳,张军力,孙胜英.无取向电工钢HW600高温变形抗力的研究[J].河北冶金,2013(4):1-3.
7程广平,张明如.60Si2Mn钢高温变形抗力的热模拟实验测定[J].湖南冶金,2000,28(3):22-24. 被引量:4
8改进铸铝合金结构部件的方法[J].铝加工,2015,0(4):61-61.
9刘建生,郭会光,孙捷先,杨明鼎.关于大型转子钢高温变形抗力的实验与分析[J].太原重型机械学院学报,1992,13(2):50-55. 被引量:1
10王向成.微量合金成分对钢的高温变形抗力的影响[J].武钢技术,1996,34(6):36-41.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]
Citation Information:
TZM alloys doped with different amount of Ti were prepared by powder metallurgy,their micro- structure is observed by SEM, and their microhardness was also measured. Gleeble 1500 thermal/mechanical testing machine was employed to simulate the heating and deformation process of the alloys at high temperature,and then stress-strain curves were drawn. The results show that higher Ti doping amount results in more and more obvious enrichment of Ti and Zr oxide or simple substance at the alloy grain boundaries to strengthen the alloy. The alloy microhardness increases first and then decreases with Ti doping amount increasing,and reaches a maximum with 0.6% TiH2 content. High temperature deformation resistance of the alloys is improved with higher Ti doping amount.
quote
| GB/T 7714-2015 | [1] CUI Chao-peng, ZHANG Guo-shang, WEI Shi-zhong, et al. Effects of Ti Doping Amount on Microstructure and Properties of TZM Alloy[J]. Rare Metals and Cemented Carbides, 2012(6): 27-30. |
| MLA | [1] CUI Chao-peng, et al., "Effects of Ti Doping Amount on Microstructure and Properties of TZM Alloy." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 27-30. |
| APA | [1] CUI Chao-peng, ZHANG Guo-shang, WEI Shi-zhong, & XU Liu-jie. (2012). Effects of Ti Doping Amount on Microstructure and Properties of TZM Alloy. Rare Metals and Cemented Carbides(6), 27-30. |
| IEEE | [1] CUI Chao-peng, ZHANG Guo-shang, WEI Shi-zhong, and XU Liu-jie, "Effects of Ti Doping Amount on Microstructure and Properties of TZM Alloy," Rare Metals and Cemented Carbides, no. 6, pp. 27-30, 2012. keywords: {TZM alloy;Ti doping;microstructure;hardness;high temperature deformation resistance} |