Synthesis of TiO_2 Nanoparticles by Hydrothermal Hydrolysis with Titanium Sulfate and Their Optical Absorption Properties AITranslate

Suqian College 3 Department;Suqian College 3 Department
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Anatase TiO2 nanoparticles were synthesized by hydrothermal hydrolysis with Ti(SO4)2 as the titanium source and strong ammonia as the precipitant. The samples were analyzed through XRD, SEM, TEM and spectrophotometer. The results show that without strong ammonia, the increase of the reaction time results in little change of TiO2 particle size. By adding strong ammonia,with the increase of pH Value the particle size of TiO2 significantly decreases,but it doesn't change when pH value is more than 7. UVVIS analysis shows that the decrease of TiO2 particle size is beneficial to the blue shift of TiO2 absorption peak. Under the conditions of 240 ℃ ,48 h and pH9, square or elliptical TiO2 nanoparticles,with better dispersity and diameter of 20 nm,are synthesized.

KeyWords AITranslate

Ti(SO4 ) hydrothermal hydrolysis method pH value TiO2 nanoparticle optical absorption property

1Jiang X,Wang T,Wang Y W. Preparation ofTiO2 nano- particles on the surface of SiO2 in binary liquids [J]. Colloids Surf A: Physicochem Eng Aspects, 2004,234 : 9- 15.

2Kavan L, Kalbac M, Zukalova M,et al. Lithium storage in nanostructured TiO2 made by hydrothermal growth [J]. Chem Mater,2004,16(3) :477-485.

3Addamo M, Augugliaro V, Paola A D,et al. Preparation, characterization and photoaetivity of polystalline nano- structured TiO2 [J]. J Phys Chem B, 2004, 108 (10): 3 303-3 310.

4丘永樑,陈洪龄,汪效祖,徐南平.水热法制备纳米TiO_2及其等电点的研究[J].高校化学工程学报,2005,19(1):129-133. 被引量:24

5李海龙,罗武林,陈涛,田文宇,孙茂,黎春,朱地,刘冉冉,赵宇亮,刘春立.载Ag二氧化钛纳米管的制备及其光催化性能[J].物理化学学报,2008,24(8):1383-1386. 被引量:35

6李海龙,朱地,刘冉冉,陈涛,田文宇,孙茂,黎春,赵宇亮,刘春立.Ti(SO4)2水解-水热法制备锐钛型纳米TiO2及其光催化性能[J].光谱学与光谱分析,2010(3):767-769. 被引量:9

7Pierre A C,Paionk G M. Chemistry of aerogels and their applications[J]. Chem Rev, 2002,102 ( 11 ) : 4 243-4 265.

8Golubko N V, Yanovskaya M I,Romm 1 P. Preparation of barium titanate and related materials by the alkoxide- hydroxide route[J]. J Sol-gel Sci Technol, 2001,20 : 135- 143.

9王细凤,罗昔贤,肖志国.一种分散的纳米TiO_2的制备[J].中国陶瓷工业,2005,12(3):21-23. 被引量:1

10周利民,王一平,黄群武.pH值对溶胶-凝胶法制备纳米TiO_2的影响[J].过程工程学报,2007,7(3):556-560. 被引量:6

1水解法合成羟基乙酸[J].精细化工经济与技术信息,1994(2):22-23.

2杨艳平,张毅安.水解法合成羟基乙酸[J].陕西化工,1994,23(1):37-38. 被引量:9

3刘成兵.水解法合成苯甲酰氯的研究[J].山东化工,2015,44(1):36-37.

4韩家骏,刘润柱.三氯乙烯水解法制备一氯乙酸的研究[J].太化科技,1995(1):13-15.

5董研,朱云江.相转移催化水解法合成烯丙醇的新工艺[J].化学试剂,1998,20(5):303-304. 被引量:1

6水解法合成羟基乙酸[J].精细化工经济与技术信息,1994(6):5-6.

7赵锐峰.氯乙酸碱性水解法合成羟基乙酸单体的研究[J].山西化工,2007,27(5):17-18. 被引量:7

8潘卫军,傅小明,刘照文.CuO微米球的水热法合成及其光吸收特性[J].稀有金属与硬质合金,2013,41(2):33-36. 被引量:2

9郭春芳.水热法合成ZnO纳米微球及其光吸收特性[J].中国粉体技术,2014,20(2):64-67. 被引量:3

10傅小明.γ-AlOOH纳米棒的水热法合成及其光吸收特性(英文)[J].人工晶体学报,2013,42(8):1673-1676. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TQ134.11[化学工程—无机化工]

Citation Information:

Anatase TiO2 nanoparticles were synthesized by hydrothermal hydrolysis with Ti(SO4)2 as the titanium source and strong ammonia as the precipitant. The samples were analyzed through XRD, SEM, TEM and spectrophotometer. The results show that without strong ammonia, the increase of the reaction time results in little change of TiO2 particle size. By adding strong ammonia,with the increase of pH Value the particle size of TiO2 significantly decreases,but it doesn't change when pH value is more than 7. UVVIS analysis shows that the decrease of TiO2 particle size is beneficial to the blue shift of TiO2 absorption peak. Under the conditions of 240 ℃ ,48 h and pH9, square or elliptical TiO2 nanoparticles,with better dispersity and diameter of 20 nm,are synthesized.

quote

GB/T 7714-2015 [1] LIU Zhao-wen, FU Xiao-ming. Synthesis of TiO_2 Nanoparticles by Hydrothermal Hydrolysis with Titanium Sulfate and Their Optical Absorption Properties[J]. Rare Metals and Cemented Carbides, 2012(6): 19-22.
MLA [1] LIU Zhao-wen, and FU Xiao-ming. "Synthesis of TiO_2 Nanoparticles by Hydrothermal Hydrolysis with Titanium Sulfate and Their Optical Absorption Properties." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 19-22.
APA [1] LIU Zhao-wen, & FU Xiao-ming. (2012). Synthesis of TiO_2 Nanoparticles by Hydrothermal Hydrolysis with Titanium Sulfate and Their Optical Absorption Properties. Rare Metals and Cemented Carbides(6), 19-22.
IEEE [1] LIU Zhao-wen and FU Xiao-ming, "Synthesis of TiO_2 Nanoparticles by Hydrothermal Hydrolysis with Titanium Sulfate and Their Optical Absorption Properties," Rare Metals and Cemented Carbides, no. 6, pp. 19-22, 2012. keywords: {Ti(SO4 ),;hydrothermal hydrolysis method;pH value;TiO2 nanoparticle;optical absorption property}