daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Treatment Methods for Complicated Materials Containing Selenium, Tellurium and Precious Metals AITranslate

School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Advantages and disadvantages are summarized of the conventional treatment methods for complicated materials containing selenium,tellurium and precious metals. The improved process in a Russian precious metal refinery and its efficiency is emphatically introduced, including leaching of initial materials in NaOH solution to enrich precious metal in alkali leaching residue, step-by-step adjustment of alkali leaching solution pH to precipitate and separate base metals such as selenium and tellurium,precious metal replacement and removal from mother liquor, and mixing smelting of alkali leaching residue and replacement product. Using the improved process, both precious and base metals are effectively recovered, and displacer consumption is also reduced during subsequent mother liquor replacement.

KeyWords AITranslate

precious metals platinum group metal selenium tellurium volatile dust- fume neutralizationprecipitation refining

1Быховский Ю А, Грейвер Н С. Основы металлургии (Том5) [М]. Москва: Издательство Металлургиэцат , 1968.316.

2Ефимов В Н, Темеров С А, Москалев А Б, и др. Способ переработки продуктов, содержащих халькогениды неблагородных металлов, свинец, металлы платиновой группы,золото и серебро[Р]. RU Pat:2291212,2007-01- 10.

3Ефимов В Н, Темеров С А. Способ переработки продуктов, содержащих халькогениды неблагородных металлов, свинец, металлы платиновой группы, золото и сеоебооГРl. RU Pat: 2335792,2009-05-20.

1彭国敏,张玉明,张福元,李晓恒.高铅含硒物料湿法处理回收硒的工艺研究[J].稀有金属,2015,39(10):928-933. 被引量:6

2张福元,熊领领,郑雅杰,马亚赟.添加NaCl氧化焙烧法回收酸泥中硒的新工艺研究[J].稀有金属,2016,40(8):831-837. 被引量:5

3宋宏儒,张燕,周鹤立,曹杰义,王皓.硫酸氢钾在硒精炼工艺中的应用与研究[J].金川科技,2020(2):19-25.

4刘鹏,张兴勇,蔡加武.稀散金属硒、碲的火法回收工艺研究进展[J].有色冶金设计与研究,2020,41(4):19-21. 被引量:3

1冯海亮,车小奎,郑其,马立成,王雷.某难选贫辉碲铋矿的选矿工艺研究[J].稀有金属,2016,40(7):687-694. 被引量:6

2张福元,熊领领,郑雅杰,马亚赟.添加NaCl氧化焙烧法回收酸泥中硒的新工艺研究[J].稀有金属,2016,40(8):831-837. 被引量:5

3熊庆丰,范兴祥,余宇楠,刘琼,刘振楠,姚春玲.用氢氧化钠从银渣中浸出硒碲试验研究[J].湿法冶金,2017,36(4):281-284. 被引量:2

4张焕然,衷水平,张永锋,刘建强,吴健辉,林泓富,林家永.铜阳极泥卡尔多炉处理工艺硒回收系统改进实践[J].有色金属:冶炼部分,2017(11):57-59. 被引量:4

5邓伟,舒超,王昌良,饶系英.四川某难选低品位碲铋矿的选矿试验研究[J].矿产综合利用,2018,0(3):34-37. 被引量:5

6肖鹏,王红军,叶逢春,易宇,纪宏巍,邱士伟.稀散金属硒、碲回收工艺现状与展望[J].金属矿山,2020,0(4):52-60. 被引量:9

7张福元,徐亮,赵卓,郑雅杰,张玉明.贵金属熔炼烟尘综合处理富集稀贵金属研究[J].稀有金属,2020,44(9):988-995. 被引量:1

8邱叶红,谢小林,殷亮,朱刘.从碲化镉废料中回收碲的研究[J].化工技术与开发,2021,50(4):49-51.

9王永梅,李雪山,曲超.含硒酸泥除汞提硒的工艺研究[J].世界有色金属,2021(12):4-6.

10谢容生,罗柏青,王春香.微波强化辅助浸出铜冶炼酸泥中硒的试验研究[J].云南冶金,2022,51(3):92-95. 被引量:2

1陈佩环.从铋冰铜中回收白银等有价金属的研究[J].矿产综合利用,1989(6):12-16.

2崔秋华.金银泥混合熔炼电解新工艺[J].有色金属:冶炼部分,1990(1):12-13.

3雷霆.含钴钙镁渣制取氧化钴工艺研究及生产实践[J].云南冶金,1995,24(1):39-43. 被引量:3

4刘兰玲,黄晓芳.锑铋复杂物料铋的回收[J].铜业工程,2011(3):31-33.

5高春娟,张雨山,蔡荣华.贵金属富集提取技术研究进展[J].盐业与化工,2010,39(2):39-43. 被引量:2

6刘大春,杨斌,戴永年,杜国山,唐万启,韩龙.从富铟渣提取金属铟的研究[J].稀有金属,2005,29(4):574-577. 被引量:25

7简洪生,曹璇,张宝.高锑铋复杂含银物料中有价金属的综合回收[J].铜业工程,2007(1):34-36. 被引量:2

8姬宏图.关于铅冶炼底吹炉烟灰镉金属回收试验研究[J].世界有色金属,2017,42(2):40-42. 被引量:2

9刘思林,陈趣山,滕荣厚,徐教仁,王忠义,冯志杰,刘时杰,张光录.镍羰化过程中贵金属富集的研究[J].有色金属,1998,50(3):80-84. 被引量:3

10马琼,刘进县.500kA预焙阳极电解槽针振和摆动现象的处理[J].有色金属:冶炼部分,2014(12):11-15. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF83[冶金工程—有色金属冶金]

Citation Information:

Advantages and disadvantages are summarized of the conventional treatment methods for complicated materials containing selenium,tellurium and precious metals. The improved process in a Russian precious metal refinery and its efficiency is emphatically introduced, including leaching of initial materials in NaOH solution to enrich precious metal in alkali leaching residue, step-by-step adjustment of alkali leaching solution pH to precipitate and separate base metals such as selenium and tellurium,precious metal replacement and removal from mother liquor, and mixing smelting of alkali leaching residue and replacement product. Using the improved process, both precious and base metals are effectively recovered, and displacer consumption is also reduced during subsequent mother liquor replacement.

quote

GB/T 7714-2015 [1] ZHAO Qin-sheng. Treatment Methods for Complicated Materials Containing Selenium, Tellurium and Precious Metals[J]. Rare Metals and Cemented Carbides, 2012(6): 15-18.
MLA [1] ZHAO Qin-sheng. "Treatment Methods for Complicated Materials Containing Selenium, Tellurium and Precious Metals." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 15-18.
APA [1] ZHAO Qin-sheng. (2012). Treatment Methods for Complicated Materials Containing Selenium, Tellurium and Precious Metals. Rare Metals and Cemented Carbides(6), 15-18.
IEEE [1] ZHAO Qin-sheng, "Treatment Methods for Complicated Materials Containing Selenium, Tellurium and Precious Metals," Rare Metals and Cemented Carbides, no. 6, pp. 15-18, 2012. keywords: {precious metals;platinum group metal;selenium;tellurium;volatile dust- fume;neutralizationprecipitation;refining}