Research on Low Temperature Denitration Performance of In/Al_2O_3 Catalyst AITranslate
Abstract AITranslate
In/Al2O3 catalyst was prepared with impregnation method and coprecipitation method, respectively,and research on selective reduction of NOx with the catalyst was carried out. The results show that the catalyst prepared by coprecipitation has higher low-temperature activity and NO selectivity. The bimetal component catalyst of In-Ti/Al2O3 was obtained by the carrier modification with transition metal Ti. And In-Ti/Al2O3 has high activity due to amorphous In oxides and high specific surface area. The added TiO2 can weaken the interaction between In and Al2O3 to form amorphous InTiO2 crystal, resulting in low- er reduction temperature of In.
KeyWords AITranslate
1HELD W, KOING A, RICHTER T, et al. Catalytic NO, reduction in net oxidizing exhaust gas[J]. SAE Trans, 1990,99(4) ..209-216.
2IWAMOTO M, HAMADA H. Removal of nitrogen monoxide from exhaust gases through novel catalytic process[J]. Catalysis Today, 1991,10(1):57-71.
3SEKER E,CAVATAIO J, GULARI E, et al. Nitric ox ide reduction by propene over silver/alumina and silver- gold/alumina catalysts: Effect of preparation methods [J]. Applied Catalysis A.. General, 1999, 183 (1) .. 121-134.
4CHEN L Y, HORIUCHI T, OSAKI T, et al. Catalytic selective reduction of NO with propylene over Cu-A12 03 catalysts.. Influence of catalyst preparation method[J]. Applied Catalysis B.. Environmental, 1999,23 (4): 259- 269.
5HANEDA M,KINTAICHI Y, SHIMADA H. Selective reduction of NO with propene over Ga2 O3-A12 03 : Effect of sol-gel method on the catalytic performance[J].Jour- nal of Catalysis,2000,192(1) : 137-148.
6LIU Z M,HAO J M,FU L X,et al. Promoting effect of sol-gel method and pre-treatment on the activity of SnO2/A1203 catalyst for NO reduction by propene[J]. Reaction Kinetics and Catalysis Letters, 2003,80 (1) : 45- 52.
7HANEDA M, KINTAICHI Y, HAMADA H. Effect of SO2 on the catalytic activity of Ga2 O3-A12 O3 for the se- lective reduction of NO with propene in the presence of oxygen[J]. Applied Catalysis B Environmental, 2001,31 (4) .. 251-261.
8LI J H,HAO J M,FU L X,et al. The activity and char- acterization of sol-gel Ag/AI2 03 catalyst for selective catalytic reduction of NOx in the presence of oxygen[J]. Catalysis Today, 2004,90(3/4) .. 215-221.
9李明利,余琼,马兰,周春江,逯庆国,徐英,郭洪光,黄凤莉,曹慧,吕绯.汽车尾气净化催化剂研究发展现状[J].兵器材料科学与工程,2012,35(6):96-98. 被引量:10
10LLIOPOULOU E F, EVDOU A P, LEMONIDOU A A,et al. Ag/alumina catalysts for the selective catalytic reduction of NO~ using various reductants[J]. Applied Catalysis A..General,2004,274(1/2) ..179-189.
1杨洁,李侠,杜红伟,柳召刚.低温La/Ce掺杂锰基脱硝催化剂的制备及表征[J].稀有金属与硬质合金,2021,49(3):41-45. 被引量:2
1黄力,王虎,纵宇浩,常峥峰,高义博,李金珂,于洋.P对V-Mo/Ti脱硝催化剂的性能影响研究[J].钢铁钒钛,2022,43(1):67-73.
2王莹,赵然,张凯,武文斐.独居石负载钼氧化物催化材料制备及其NH3-SCR脱硝性能研究[J].稀有金属与硬质合金,2023,51(1):40-46.
1刘建东,黄张根,李哲,郭倩倩,李巧艳.Ce对Mn/TiO2/堇青石整体低温脱硝选择性催化还原催化剂的改性[J].高等学校化学学报,2014,35(3):589-595. 被引量:30
2方璐希,刘灿明,喻鹏,阳杰,郑为民.新型Al、Ti改性MCM-41材料对污水中Cu^(2+)的吸附研究[J].广州化学,2011,36(3):37-43.
3赖瑞云,唐晓龙,易红宏,李凯,王盼,孙鑫.Mn-Mg-Ox催化剂低温NH3选择性催化还原NO的性能的研究[J].现代化工,2014,34(9):76-79. 被引量:4
4邢帅,姜宏,熊春荣,马艳平.椰壳活性炭氧化后负载硅基复合氧化物低温脱硝催化剂的研究[J].分子催化,2016,30(2):140-150. 被引量:13
5张相俊,刘晓刚,李清雍,李岩,魏波,王虹,李翠清,宋永吉.载体对铜基催化剂NH_3-SCR低温脱硝性能的影响[J].燃料化学学报,2017,45(2):220-226. 被引量:11
6杨瀚,仲兆平,朱林,王春华.铁铈复合催化剂的低温SCR脱硝性能[J].环境工程学报,2017,11(4):2413-2418. 被引量:6
7肖峰,顾韵婕,陈智栋,唐喆,邵景玲,韩粉女,许琦,朱红丽.低温SCR脱硝催化剂的制备及其催化性能[J].合成化学,2015,23(6):485-489. 被引量:2
8宋淑美,王睿.具有低温活性的高效脱硝催化体系研究进展[J].现代化工,2007,27(z1):108-112. 被引量:5
9沈岳松,余勇,丘泰,祝社民.稀土掺杂双组分整体式低温脱硝催化剂的制备与性能(英文)[J].稀有金属材料与工程,2011,40(6):967-972. 被引量:7
10刘振,程瑞华,何雪莲,田洲,刘柏平.铬系催化乙烯配位聚合/齐聚分子模拟研究进展[J].化学反应工程与工艺,2014,30(3):218-228. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:O643.36[理学—物理化学]
Citation Information:
In/Al2O3 catalyst was prepared with impregnation method and coprecipitation method, respectively,and research on selective reduction of NOx with the catalyst was carried out. The results show that the catalyst prepared by coprecipitation has higher low-temperature activity and NO selectivity. The bimetal component catalyst of In-Ti/Al2O3 was obtained by the carrier modification with transition metal Ti. And In-Ti/Al2O3 has high activity due to amorphous In oxides and high specific surface area. The added TiO2 can weaken the interaction between In and Al2O3 to form amorphous InTiO2 crystal, resulting in low- er reduction temperature of In.
quote
| GB/T 7714-2015 | [1] XU Zhen-chong, WU Shuang. Research on Low Temperature Denitration Performance of In/Al_2O_3 Catalyst[J]. Rare Metals and Cemented Carbides, 2016(4): 48-52. |
| MLA | [1] XU Zhen-chong, and WU Shuang. "Research on Low Temperature Denitration Performance of In/Al_2O_3 Catalyst." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 48-52. |
| APA | [1] XU Zhen-chong, & WU Shuang. (2016). Research on Low Temperature Denitration Performance of In/Al_2O_3 Catalyst. Rare Metals and Cemented Carbides(4), 48-52. |
| IEEE | [1] XU Zhen-chong and WU Shuang, "Research on Low Temperature Denitration Performance of In/Al_2O_3 Catalyst," Rare Metals and Cemented Carbides, no. 4, pp. 48-52, 2016. keywords: {In/Al2O3 catalyst;impregnation method;coprecipitation method;Ti modification;selective reduc-tion;NO} |