Study on Interfacial Microstructure and Mechanical Properties of SnAg0.5CuZn0.1Ni/Cu Brazed Joints AITranslate

Sinopec Pipeline Storage and Transportation Co., Ltd.;School of Mechanical Engineering, Taiyuan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects were studied of brazing parameters on interfacial microstructure, intermetallic com- pound layer thickness and mechanical properties of SnAg0.5CuZn0.1Ni/Cu lead-free brazed joints by OM, XRD, TEM,SEM and tensile testing. The results show that 0.1% Ni addition can obviously refine the pri- mary/9-Sn phase and eutectic microstructure of SnAg0.5CuZn solder alloy. The brazed joint has the maxi- mum shear strength of 45.6 MPa when brazing temperature is 270 ℃ and brazing time is 240 s. All the interfacial roughness,intermetallic compound layer thickness and the shear strength of the brazed joints vary with the change of brazing parameters.

KeyWords AITranslate

lead-free solder alloy SnAg0. 5CuZn0. 1Ni brazing interface intermetallic compound shear strength

1MA H T,SUHLING J C. A review of mechanical prop- erties of lead-free solders for electronic packaging[J]. Journal of Materials Science. 2009,44(5) .. 1 141-1 158.

2李军,胡宗保.电子产品及电子器件绿色环保化[J].电子器件,2004,27(3):537-542. 被引量:13

3王春青,王学林,田艳红.SnAgCu无铅微焊点剪切力学性能的体积效应[J].焊接学报,2011,32(4):1-4. 被引量:20

4邹贵生,闫剑锋,母凤文,吴爱萍,Zhou Y.Norman.微连接和纳连接的研究新进展[J].焊接学报,2011,32(4):107-112. 被引量:48

5ZHANG Liang,XUE Song-bai, GAO Li-li, et al. Effects of rare earths on properties and microstructures of lead- free solder alloys[J]. Journal of Materials Science : Mate- rials in Electronics, 2009,20 (8) : 685-694.

6DONG Wenxing, SHI Yaowu, LEI Yongping, et al. Effects of small amounts of Ni/P/Ce element additions on the microstructure and properties of Sn3.0Ag0.5Cu solder alloy[J]. Journal of Materials Science: Materials in Electronics,2009,20(10) ..1 008-1 017.

7CHUANG Chiangming, SHIH Po-Cheng, LIN Kwang- Lung. Mechanical strength of Sn-3. 5Ag-based solders and related bondings[J]. Journal of Electronic Materials, 2004,33(1) :1-6.

8CHENG Fangjie, NISHIKAWA Hiroshi, TAKEMOTO Tadashi. Microstructural and mechanical properties of Sn-Ag-Cu lead-free solders with minor addition of Ni and/or Co [J]. Journal of Materials Science, 2008, 43 (10) :3 643-3 648.

9王文海,王珺,唐兴勇,肖斐,俞宏坤.添加微量高熔点金属对无铅焊料性能的影响[J].电子元件与材料,2005,24(9):48-51. 被引量:10

10ZHANG Keke, WANG Yaoli, FAN Yan-Li, et al. Sn- 2.5Ag-0.7Cu-0.1Re-.:Ni lead-free solder alloy and its creep properties of solder joints[J]. Materials Science Forum, 2010,650..91-96.

1蔡航伟,杜昆.焊片对钎焊空洞率的影响研究[J].焊接技术,2019,0(10):73-76. 被引量:1

1奉林晚,陈禹伽,李小梅.射频隔离器高功率密度负载焊接可靠性[J].磁性材料及器件,2023,54(1):65-69.

1林瑾.SnAg0.5CuZn0.1Ni/Cu钎焊接头的组织与力学性能[J].特种铸造及有色合金,2016,36(9):985-988. 被引量:1

2李臣阳,张柯柯,王要利,赵恺,杜宜乐.Ni元素对Sn2.5Ag0.7Cu0.1RE/Cu无铅微焊点界面IMC和力学性能的影响[J].焊接学报,2012,33(11):39-42. 被引量:7

3苌文龙,于治水,房加强,王波.尺寸效应下的无铅微焊点研究进展[J].上海工程技术大学学报,2012,26(2):111-115. 被引量:1

4周敏波,马骁,张新平.BGA结构Sn-3.0Ag-0.5Cu/Cu焊点低温回流时界面反应和IMC生长行为[J].金属学报,2013,49(3):341-350. 被引量:5

5黎滨,杨艳,尹立孟,张新平.无铅微焊点界面断裂行为的尺寸效应[J].机械工程学报,2010,46(18):77-84. 被引量:3

6孙凤莲,王家兵,刘洋,王国军.SnAgCu-Bi-Ni无铅微焊点的电迁移行为[J].哈尔滨理工大学学报,2012,17(3):1-4. 被引量:2

7王春青,王学林,田艳红.SnAgCu无铅微焊点剪切力学性能的体积效应[J].焊接学报,2011,32(4):1-4. 被引量:20

8刘洋,孙凤莲.SnAgCu/Cu微焊点界面IMC演变及脆断分析[J].机械制造文摘:焊接分册,2013(1):28-29.

9秦红波,李望云,李勋平,张新平.BGA结构无铅微焊点的低周疲劳行为研究[J].机械工程学报,2014,50(20):54-62. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TG425.1[金属学及工艺—焊接]

Citation Information:

The effects were studied of brazing parameters on interfacial microstructure, intermetallic com- pound layer thickness and mechanical properties of SnAg0.5CuZn0.1Ni/Cu lead-free brazed joints by OM, XRD, TEM,SEM and tensile testing. The results show that 0.1% Ni addition can obviously refine the pri- mary/9-Sn phase and eutectic microstructure of SnAg0.5CuZn solder alloy. The brazed joint has the maxi- mum shear strength of 45.6 MPa when brazing temperature is 270 ℃ and brazing time is 240 s. All the interfacial roughness,intermetallic compound layer thickness and the shear strength of the brazed joints vary with the change of brazing parameters.

quote

GB/T 7714-2015 [1] CUI Jun, LIU Qiu-zu. Study on Interfacial Microstructure and Mechanical Properties of SnAg0.5CuZn0.1Ni/Cu Brazed Joints[J]. Rare Metals and Cemented Carbides, 2016(4): 53-56.
MLA [1] CUI Jun, and LIU Qiu-zu. "Study on Interfacial Microstructure and Mechanical Properties of SnAg0.5CuZn0.1Ni/Cu Brazed Joints." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 53-56.
APA [1] CUI Jun, & LIU Qiu-zu. (2016). Study on Interfacial Microstructure and Mechanical Properties of SnAg0.5CuZn0.1Ni/Cu Brazed Joints. Rare Metals and Cemented Carbides(4), 53-56.
IEEE [1] CUI Jun and LIU Qiu-zu, "Study on Interfacial Microstructure and Mechanical Properties of SnAg0.5CuZn0.1Ni/Cu Brazed Joints," Rare Metals and Cemented Carbides, no. 4, pp. 53-56, 2016. keywords: {lead-free solder alloy;SnAg0. 5CuZn0. 1Ni;brazing;interface;intermetallic compound;shear strength}