Study on Hardness and Microstructure of Ni-Co Electroplated Coatings AITranslate
Abstract AITranslate
The effects of current density, bath temperature and pH value on hardness of Ni-Co alloy coatings were investigated with single variable method in sulfate system. The optimal technological conditions were determined as follows: the bath temperature is 45 ℃ ,pH value is 3, and the current density is 6 A/dm2. Under these conditions, the Ni-Co alloy coatings with high hardness and good bonding properties on the CuCrZr matrix were prepared. The influences of annealing temperature on hardness and texture of Ni-Co alloy coatings were analyzed. The results show that with the increase of the annealing temperature, the hardness of the coatings increases firstly and then decreases,and the highest HV0.05value reached 506.2 at 300 ℃. After annealing,the coatings exhibits a strong (111) texture.
KeyWords AITranslate
1杨明铎,张铁军.连铸机结晶器铜板电镀镍-钴(Ni-Co)合金工艺[J].鞍钢技术,2003(1):18-20. 被引量:26
2WANG L, GAO Y, XUE Q, et al. Microstructure and tribological properties of electrodeposited Ni-Co alloy deposits[J]. Applied Surface Science, 2005,242 (3) .. 326 -332.
3王丹,高吉成,张骥群,成艳芳,靳惠明.沉积参数对Ni-Co镀层成分及微观结构影响研究[J].四川大学学报:自然科学版,2013,50(1):118-124. 被引量:9
4陈志凯,王群,郭红霞,王澈,王东辰.Ni-Fe合金电沉积工艺参数对镀层铁含量的影响[J].材料保护,2010,43(8):60-62. 被引量:3
5张雷,李春福,尤郭群.热处理温度对Ni-Fe-P化学镀层性能的影响[J].金属热处理,2014,39(1):106-109. 被引量:5
6GB/T5270-2005.金属基体上的金属覆盖层(电沉积层和化学沉积层)附着强度试验方法评述[S].
7黄胜涛.固体x射线学[M].北京:高等教育出版社,1985.313-314.
8CHUNG C K,CHANG W T. Effect of pulse frequency and current density on anomalous composition and nano- mechanical property of eleetrodeposited Ni-Co films[J]. Thin Solid Films, 2009, 517(17): 4 800-4 804.
9乔学亮,许卫华,陈建国,孙培祯.Ni-P薄膜化学镀液的成分变化及镀膜控制[J].华中理工大学学报,1995,23(1):117-120. 被引量:6
10曹卓坤,刘宜汉,姚广春.硫酸盐酸性镀液中碳纤维电镀铜[J].过程工程学报,2006,6(4):651-655. 被引量:14
1张晓翠.基于模具钢基体的Ni-Co合金镀层的性能研究[J].电镀与环保,2018,38(5):1-4. 被引量:1
2吴忠.汽车用ZL101A铝合金表面Ni-Co合金镀层的硬度[J].电镀与精饰,2018,40(11):5-9. 被引量:3
1肖革,蓝玉良,向可友,高荣龙,罗泽庭,刘慧丛,李卫平,朱立群.汽车轻量化钢材及零部件表面处理技术的发展趋势[J].电镀与精饰,2019,41(7):25-30. 被引量:5
2王建伟,陆贞,刘兴科.曲轴模具的表面处理与耐蚀性能研究[J].真空科学与技术学报,2021,41(6):528-533.
3向可友,肖革,蓝玉良,张晓凤,刘慧丛,朱立群.表面处理技术在汽车轻量化方面的应用[J].腐蚀与防护,2021,42(7):48-52. 被引量:5
4骆骢,马硕.无铬封闭处理对ZL101A铝合金阳极氧化膜耐蚀性能的影响[J].电镀与精饰,2022,44(2):46-50. 被引量:2
1彭成章,杨添,曹获,向浪.热处理对Ni-Co合金镀层组织与耐蚀性能的影响[J].热加工工艺,2015,44(2):197-199. 被引量:1
2郑炜铭,戴品强,唐电.低温退火对电刷镀纳米晶Ni-Co合金镀层性能的影响[J].中国表面工程,2010,23(5):68-72. 被引量:2
3吕希建,唐德文,邹树梁.基于ABAQUS的Ti6Al4V切削仿真研究[J].机械工程与自动化,2017(1):66-68. 被引量:3
4何力佳,赵锐,刘鹏飞,李楠.渗硼处理对Cr12冷轧辊表面组织及性能的影响[J].热加工工艺,2014,43(14):118-122. 被引量:3
5钟远辉,戴品强,戴春福.脉冲电沉积纳米晶Ni-Co合金镀层热稳定性的研究[J].材料工程,2009,37(4):52-56. 被引量:6
6黄冀.表面合金镀层和合金化提高铸铁机械零件接触疲劳强度研究[J].机械传动,2009,33(2):9-13.
7马焕明,曲明贵.单脉冲电沉积Ni-Co合金镀层在NaCI盐膜下的腐蚀行为[J].热处理,2006,21(2):25-27. 被引量:2
8蔡炯.表面改性304不锈钢的微观组织和耐空蚀性能研究[J].铸造技术,2014,35(12):2920-2922. 被引量:1
9钟远辉,戴品强,许伟长,陈闪闪.脉冲电沉积纳米晶Ni-Co合金镀层腐蚀特性研究[J].稀有金属材料与工程,2009,38(6):1053-1057. 被引量:11
10张琳琳,王修春,牛玉超,伊希斌,潘喜庆,王金伟.铝合金的硅烷化工艺研究[J].山东科学,2014,27(4):42-45. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG-141[金属学及工艺]
Citation Information:
The effects of current density, bath temperature and pH value on hardness of Ni-Co alloy coatings were investigated with single variable method in sulfate system. The optimal technological conditions were determined as follows: the bath temperature is 45 ℃ ,pH value is 3, and the current density is 6 A/dm2. Under these conditions, the Ni-Co alloy coatings with high hardness and good bonding properties on the CuCrZr matrix were prepared. The influences of annealing temperature on hardness and texture of Ni-Co alloy coatings were analyzed. The results show that with the increase of the annealing temperature, the hardness of the coatings increases firstly and then decreases,and the highest HV0.05value reached 506.2 at 300 ℃. After annealing,the coatings exhibits a strong (111) texture.
quote
| GB/T 7714-2015 | [1] LIU Lin-jing, ZOU De-ning, HU Shu-mao, et al. Study on Hardness and Microstructure of Ni-Co Electroplated Coatings[J]. Rare Metals and Cemented Carbides, 2016(4): 57-61. |
| MLA | [1] LIU Lin-jing, et al., "Study on Hardness and Microstructure of Ni-Co Electroplated Coatings." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 57-61. |
| APA | [1] LIU Lin-jing, ZOU De-ning, HU Shu-mao, WANG Dong, LI Ke-xin, & ZHANG Ying-bo. (2016). Study on Hardness and Microstructure of Ni-Co Electroplated Coatings. Rare Metals and Cemented Carbides(4), 57-61. |
| IEEE | [1] LIU Lin-jing, ZOU De-ning, HU Shu-mao, WANG Dong, LI Ke-xin, and ZHANG Ying-bo, "Study on Hardness and Microstructure of Ni-Co Electroplated Coatings," Rare Metals and Cemented Carbides, no. 4, pp. 57-61, 2016. keywords: {electroplating;Ni-Co alloy coating;single variable method;hardness;bonding property;annealing} |