Study on Surface Roughness of Superalloy GH4169 after High Speed Milling AITranslate
Abstract AITranslate
The orthogonal experiment was carried out of high speed milling of superalloy GH4169 with KYHS10 ceramic tool. The effects were studied by range analysis of milling speed,milling depth,and feed per tooth on the surface roughness of the machined materials. The influencing law was analyzed of each machining parameter on surface roughness. Aprediction model of surface roughness was established,and its reliability was verified. The results show that the primary and secondary influence factors on the surface roughness are milling depth, feed per tooth and milling speed. The surface roughness gradually decreases with the increase of the milling speed, but increases with the increase of the milling depth and feed per tooth.
KeyWords AITranslate
1傅玉灿.难加工材料高效加工技术[M].西安:西北工业大学出版社,2011.
2杨斌,耿国盛,徐九华,傅玉灿,何坚,贺敏岐.钴基高温合金高速铣削研究[J].航空制造技术,2011,0(14):58-61. 被引量:5
3肖茂华,何宁,李亮,刘海滨.陶瓷刀具高速切削镍基高温合金沟槽磨损试验研究[J].中国机械工程,2008,19(10):1188-1192. 被引量:24
4宋新玉,赵军,姜俊玲.加工Inconel 718时陶瓷刀具的磨损机理[J].中国机械工程,2009,20(7):763-767. 被引量:16
5RAHMAN M,SEAH W K H,TEO T T. The machin- ability of Inconel 718[J]. Journal of Materials Processing Technology, 1997,63(1/3) : 199-204.
6DUDZINSKI D,DEVILLEZ A,MOUFKI A,et al. A re- view of developments towards dry and high speed ma- chining of Inconel 718 alloy[J]. International Journal of Machine Tools and Manufacture, 2004,44 (4) : 439-456.
7EZUGWU E O,WANG Z M, MACHADO A R. The machinability of nickel-based alloys: A review[J]. Jour- nal of Materials Processing Technology, 1999,86 ( 1/3 ) : 1-16.
8CHOUDHURY I A,EI-BARADIE M A. Machinabili- ty of nickel-based super alloys= A general review[J]. Journal of Materials Processing Technology, 1998, 77 (1/3) :278-284.
9ALAUDDIN M,MAZID M A,BARADI M A E, et al. Cutting forces in the end milling of lnconel 718 [J]. Journal of Materials Processing Technology, 1998, 77 (1/3) : 153-159.
10PAWADE R S, JOSHI S S, BRAHMANKAR P K. Effect of machining parameters and cutting edge geom- etry on surface integrity of high speed turned Ineonel 718[J]. International Journal of Machine Tools and Manufacture, 2008,48 ( 1 ) : 15-28.
1梁军华,韩俊峰.不同冷却润滑条件下铣削镍基高温合金GH4169的表面粗糙度试验研究[J].制造技术与机床,2019,0(12):120-122. 被引量:5
2陈光军,韩松鑫,潘佳琦,侯帅,孙光兴.切削加工表面粗糙度影响因素及预测建模综述[J].机床与液压,2020,48(13):185-188. 被引量:4
3于凤云,郭绍炳,付云良,张力猛,高坡.高温合金GH4169铣削振动试验研究[J].机床与液压,2020,48(15):114-117. 被引量:1
1王玉春,田永久,江帆.浅谈钛合金在切削加工中的特性[J].中国金属通报,2020(8):201-202.
2邓志博,王哲.GH4169热辅助切削过程分析[J].工业加热,2021,50(2):24-26.
3陈英.环形刀高速铣削加工P1.2738钢表面粗糙度预测模型试验研究[J].吉林工程技术师范学院学报,2021,37(6):95-98.
4高奇,荆小飞,郭光岩.基于微量润滑的微铣削单晶高温合金表面粗糙度研究[J].机床与液压,2021,49(16):29-32. 被引量:1
5李阳,刘俨后,张昆,田业冰,田承金.基于改进遗传算法的磨削能耗预测及工艺参数优化[J].组合机床与自动化加工技术,2021(10):124-128. 被引量:2
6纪任可,郑光明,韩康宁,李勋.高温合金GH4169球头刀铣削表面完整性测试实验研究[J].机床与液压,2022,50(10):36-40. 被引量:1
7王明海,图晨华,吴志新,王奔,张静波.硬质合金铣刀钝圆半径对Inconel 718高温合金切削力与切削温度的影响[J].工具技术,2022,56(10):117-120.
8唐林虎,马富荣,胡彦军,张季惠,孙永吉,李宝栋.宽温域油附三态水雾车削镍基高温合金钢已加工表面质量的研究[J].现代制造工程,2023(1):1-9.
9李远博,邵明辉,李顺才,王强.钛合金铣削表面粗糙度检测及多元预测模型研究[J].现代制造工程,2023(3):96-104.
10李远博,李顺才,邵明辉,刘志.N6镍铣削表面粗糙度与铣削力-铣削振动的耦合特性研究[J].机床与液压,2023,51(6):12-18.
1乔秉诚.提高热轧硅钢凸度精度的工艺措施[J].山西冶金,2012,35(5):22-24. 被引量:1
2高奇,蔡明.高速微尺度铣削单晶铝表面粗糙度试验研究[J].组合机床与自动化加工技术,2016(9):13-16. 被引量:2
3方玉峰,卢百平,陈诚.合金成分对Cu-Ni-Nb-Mo合金组织及热物性的影响[J].特种铸造及有色合金,2015,35(3):318-321. 被引量:1
4陈健,崔庭.CuNiCoBe合金表面等离子弧喷涂Cr_3C_2-NiCr涂层[J].焊接技术,2012,41(5):17-20. 被引量:1
5孙振国,陈扬,杨建新,傅汇彤,王维志.影响GCr15钢M/B复相组织强韧性的主次因素初探[J].材料科学与工艺,1994,2(1):44-48.
6苟刚,刘勇,张利堂.基于正交试验的电火花成形加工工艺研究[J].河南科技,2014,33(6):165-166.
7马利影,徐新成,张亚龙,晏彬彬.37CrMnMo钢热处理工艺研究与优化[J].热加工工艺,2016,45(10):222-224. 被引量:2
8韩芳,从善海,赵婷婷,谢青,胡莎.热处理对粉末冶金Cu-15Ni-8Sn合金组织与性能的影响[J].金属热处理,2012,37(4):84-87. 被引量:4
9孙士雷,赵杰,袁玮骏,奚望,赵灿.GH4169镍基高温合金表面加工硬化研究[J].工具技术,2016,50(10):24-27. 被引量:11
10陆小会,高原,韦文竹,张光耀,王成磊.基于正交试验研究0Cr18Ni9Ti不锈钢等离子渗铪的最优工艺[J].热加工工艺,2015,44(6):101-104. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG54[金属学及工艺—金属切削加工及机床]
Citation Information:
The orthogonal experiment was carried out of high speed milling of superalloy GH4169 with KYHS10 ceramic tool. The effects were studied by range analysis of milling speed,milling depth,and feed per tooth on the surface roughness of the machined materials. The influencing law was analyzed of each machining parameter on surface roughness. Aprediction model of surface roughness was established,and its reliability was verified. The results show that the primary and secondary influence factors on the surface roughness are milling depth, feed per tooth and milling speed. The surface roughness gradually decreases with the increase of the milling speed, but increases with the increase of the milling depth and feed per tooth.
quote
| GB/T 7714-2015 | [1] SUN Shi-lei, ZHAO Jie, ZHAO Can. Study on Surface Roughness of Superalloy GH4169 after High Speed Milling[J]. Rare Metals and Cemented Carbides, 2016(4): 62-65. |
| MLA | [1] SUN Shi-lei, et al., "Study on Surface Roughness of Superalloy GH4169 after High Speed Milling." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 62-65. |
| APA | [1] SUN Shi-lei, ZHAO Jie, & ZHAO Can. (2016). Study on Surface Roughness of Superalloy GH4169 after High Speed Milling. Rare Metals and Cemented Carbides(4), 62-65. |
| IEEE | [1] SUN Shi-lei, ZHAO Jie, and ZHAO Can, "Study on Surface Roughness of Superalloy GH4169 after High Speed Milling," Rare Metals and Cemented Carbides, no. 4, pp. 62-65, 2016. keywords: {superalloy;GH416 9;ceramic tool;orthogonal experiment;surface roughness;range analysis} |