daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest Development of Inorganic Powder Materials Preparation by Molten Salt Synthesis AITranslate

Northeast University School of Metallurgical;Northeast University School of Metallurgical
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Basic properties of several common molten salts are introduced as well as the advantages and disadvantages of molten salt synthesis method. The action mechanisms of molten salts for preparing inorganic powder materials and their selection principles are summarized. The latest development is reviewed on preparing inorganic powder materials such as oxides and their composite powders, nitrides and carbides by molten salt synthesis. And the future application of molten salt synthesis method for preparing inorganic powder materials is also pointed out.

KeyWords AITranslate

molten salt synthesis method inorganic powder material oxide nitride carbide

1ARENDT R H. Liquid-phase sintering of magnetically isotropic and anise by the reaction of BaFe2 04 with Fe2O3 [J]. Journal of Solid State Chemistry,1973,8(4). 339-347.

2李月明,黄丹,廖润华,王进松.熔盐法合成晶体的研究现状与进展[J].陶瓷学报,2008,29(2):164-169. 被引量:20

3陈伟利.无机材料粉体制备中使用熔盐法的探究[J].山东化工,2015,44(11):61-63. 被引量:2

4李雪冬,朱伯铨.熔盐法合成氧化物陶瓷粉体的研究进展[J].中国陶瓷,2006,42(3):11-15. 被引量:7

5周健,焦宝祥.熔盐法合成无机粉体材料[J].常熟理工学院学报,2008,22(2):71-76. 被引量:6

6侯俊峰,武在军,王耀挺,毕明峰.熔盐法制备各向异性形貌晶粒的研究进展[J].中国陶瓷,2012,48(2):1-3. 被引量:6

7李雪冬,朱伯铨,汪厚植.熔盐法在无机材料粉体制备中的应用[J].材料导报,2006,20(3):44-47. 被引量:33

8邓三毛,叶红齐,苏周,周永华,杨鹰.片状氧化物粉体的合成与性能[J].化工新型材料,2004,32(7):13-15. 被引量:8

9杨鹰,苏周,刘辉,周涛,叶红齐.片状氧化铝粉体的熔盐法合成[J].过程工程学报,2004(z1):279-283. 被引量:10

10谭宏斌.粉煤灰制备片状氧化铝粉体[J].陶瓷,2010(2):20-22. 被引量:9

1吴峥强.添加剂Nb和烧结温度对ZrN粉末材料性能的影响[J].粉末冶金技术,2019,0(4):255-258.

1蔡宗英,邢献然,刘桂荣,于然波.熔盐法合成PbTiO_3粉体及其表征[J].金属学报,2006,42(1):109-112. 被引量:8

2谢超,徐龙君,刘成伦.锶铁氧体的结构特征及制备方法研究现状[J].世界科技研究与发展,2012,34(3):445-449.

3谈玲华,李勤华,郭长平,冯春霞,潘仁明,李凤生.纳米La_2O_3及其复合氧化物的制备方法研究进展[J].微纳电子技术,2010,47(5):257-266. 被引量:5

4周健,焦宝祥.熔盐法合成无机粉体材料[J].常熟理工学院学报,2008,22(2):71-76. 被引量:6

5张欣,肖秋国,刘清泉,伍泽广.熔盐合成法制备片状氧化铝的初步研究[J].硅酸盐通报,2009,28(4):859-861. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TB321[一般工业技术—材料科学与工程]

Citation Information:

Basic properties of several common molten salts are introduced as well as the advantages and disadvantages of molten salt synthesis method. The action mechanisms of molten salts for preparing inorganic powder materials and their selection principles are summarized. The latest development is reviewed on preparing inorganic powder materials such as oxides and their composite powders, nitrides and carbides by molten salt synthesis. And the future application of molten salt synthesis method for preparing inorganic powder materials is also pointed out.

quote

GB/T 7714-2015 [1] YIN Yue, MA Bei-yue. The Latest Development of Inorganic Powder Materials Preparation by Molten Salt Synthesis[J]. Rare Metals and Cemented Carbides, 2016(4): 66-72.
MLA [1] YIN Yue, and MA Bei-yue. "The Latest Development of Inorganic Powder Materials Preparation by Molten Salt Synthesis." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 66-72.
APA [1] YIN Yue, & MA Bei-yue. (2016). The Latest Development of Inorganic Powder Materials Preparation by Molten Salt Synthesis. Rare Metals and Cemented Carbides(4), 66-72.
IEEE [1] YIN Yue and MA Bei-yue, "The Latest Development of Inorganic Powder Materials Preparation by Molten Salt Synthesis," Rare Metals and Cemented Carbides, no. 4, pp. 66-72, 2016. keywords: {molten salt synthesis method;inorganic powder material;oxide;nitride;carbide}