Efficient Photothermal Energy Conversion Triggered by near-Infrared Light in a Dithiolene-Based Metal–Organic Framework AITranslate

The University of Sydney; Nanjing University; Nagasaki University; Nanjing University; Nanjing University; The University of Sydney; Nanjing University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A Ni-dithiolene ligand, {Ni(pedt)2}− (pedt = 1-(pyridine-4-yl)ethylene-1,2-dithiolate), was used to prepare a novel interpenetrated redox-active Metal–Organic Framework (MOF), which exhibited an efficient photothermal conversion under low-power-density near-infrared (NIR) laser illumination. Solid-state UV–vis-NIR spectroscopy on bulk crystals indicated strong absorbance in the NIR region, attributed to the radical monoanion of the pedt ligands, which was also evident in the solid-state Electron Paramagnetic Resonance (EPR) spectrum. DFT computations on a model system provided new insights into the structural factors underpinning the photothermal properties. First, the NIR absorption corresponds to a high-energy excited state (D4), while the lowest-lying excited state (D1) is close in energy to the energies of the vibrational motions, facilitating the conversion of electronic to thermal energy. Second, close contacts between interpenetrated nets of the MOF may further enhance the propagation of thermal motion. The new photothermal MOF was then doped into a self-healing polymer, PDU (polydimethylsiloxane-urea), leading to composites which could recover from dynamic damage using the heat generated from the embedded MOF by photostimulus. This process led by the photothermal effect offers a highly efficient and energy-saving approach for self-healing materials design.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c00700

Chinese Library Classification Number:

Citation Information:

A Ni-dithiolene ligand, {Ni(pedt)2}− (pedt = 1-(pyridine-4-yl)ethylene-1,2-dithiolate), was used to prepare a novel interpenetrated redox-active Metal–Organic Framework (MOF), which exhibited an efficient photothermal conversion under low-power-density near-infrared (NIR) laser illumination. Solid-state UV–vis-NIR spectroscopy on bulk crystals indicated strong absorbance in the NIR region, attributed to the radical monoanion of the pedt ligands, which was also evident in the solid-state Electron Paramagnetic Resonance (EPR) spectrum. DFT computations on a model system provided new insights into the structural factors underpinning the photothermal properties. First, the NIR absorption corresponds to a high-energy excited state (D4), while the lowest-lying excited state (D1) is close in energy to the energies of the vibrational motions, facilitating the conversion of electronic to thermal energy. Second, close contacts between interpenetrated nets of the MOF may further enhance the propagation of thermal motion. The new photothermal MOF was then doped into a self-healing polymer, PDU (polydimethylsiloxane-urea), leading to composites which could recover from dynamic damage using the heat generated from the embedded MOF by photostimulus. This process led by the photothermal effect offers a highly efficient and energy-saving approach for self-healing materials design.

quote

GB/T 7714-2015 [1] Qinyi Gu, ZiHan Zhao, Bun Chan, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00700.
MLA [1] Qinyi Gu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00700.
APA [1] Qinyi Gu, ZiHan Zhao, Bun Chan, Tong Yan, JingLin Zuo, Deanna M. D’Alessandro, & ChengHui Li. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00700
IEEE [1] Qinyi Gu, ZiHan Zhao, Bun Chan, Tong Yan, JingLin Zuo, Deanna M. D’Alessandro, and ChengHui Li, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00700.