Highly Luminescent Transparent Cs2AgxNa1–xBiyIn1–yCl6 Perovskite Films Produced by Single-Source Vacuum Deposition AITranslate

Forschungszentrum Jülich GmbH, Helmholtz-Institut Erlangen Nürnberg für Erneuerbare Energien (HI ERN);Forschungszentrum Jülich GmbH, Helmholtz-Institut Erlangen Nürnberg für Erneuerbare Energien (HI ERN); Universidad de Valencia; Universidad de Valencia;Friedrich-Alexander-Universität Erlangen-Nürnberg, Materials for Electronics and Energy Technology (i-MEET);Friedrich-Alexander-Universität Erlangen-Nürnberg, Materials for Electronics and Energy Technology (i-MEET);Forschungszentrum Jülich GmbH, Helmholtz-Institut Erlangen Nürnberg für Erneuerbare Energien (HI ERN); Universidad de Valencia;Forschungszentrum Jülich GmbH, Helmholtz-Institut Erlangen Nürnberg für Erneuerbare Energien (HI ERN)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermal deposition of halide perovskites as a universal and scalable route to transparent thin films becomes highly challenging in the case of lead-free double perovskites, requiring the evaporation dynamics of multiple metal halide sources to be balanced or a single-phase precursor preliminary synthesized to achieve a reliable control over the composition and the phase of the final films. In the present Letter, the feasibility of the single-source vacuum deposition of microcrystalline Cs2AgxNa1–xBiyIn1–yCl6 double perovskites into corresponding transparent nanocrystalline films while preserving the bulk spectral and structural properties is shown. The perovskite films produced from the most emissive powders with x = 0.40 and y = 0.01 revealed a photoluminescence quantum yield of 85%, highlighting thermal evaporation as a promising approach to functional perovskite-based optical materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00034

Chinese Library Classification Number:

Citation Information:

Thermal deposition of halide perovskites as a universal and scalable route to transparent thin films becomes highly challenging in the case of lead-free double perovskites, requiring the evaporation dynamics of multiple metal halide sources to be balanced or a single-phase precursor preliminary synthesized to achieve a reliable control over the composition and the phase of the final films. In the present Letter, the feasibility of the single-source vacuum deposition of microcrystalline Cs2AgxNa1–xBiyIn1–yCl6 double perovskites into corresponding transparent nanocrystalline films while preserving the bulk spectral and structural properties is shown. The perovskite films produced from the most emissive powders with x = 0.40 and y = 0.01 revealed a photoluminescence quantum yield of 85%, highlighting thermal evaporation as a promising approach to functional perovskite-based optical materials.

quote

GB/T 7714-2015 [1] Oleksandr Stroyuk, Oleksandra Raievska, Paz SebastiaLuna, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00034.
MLA [1] Oleksandr Stroyuk, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00034.
APA [1] Oleksandr Stroyuk, Oleksandra Raievska, Paz SebastiaLuna, Bas A. H. Huisman, Christian Kupfer, Anastasia Barabash, Jens Hauch, Henk J. Bolink, & Christoph J. Brabec. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00034
IEEE [1] Oleksandr Stroyuk, Oleksandra Raievska, Paz SebastiaLuna, Bas A. H. Huisman, Christian Kupfer, Anastasia Barabash, Jens Hauch, Henk J. Bolink, and Christoph J. Brabec, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00034.