An Individualized Core–Shell Architecture Derived from Covalent Triazine Frameworks: Toward Enhancing the Flame Retardancy, Smoke Release Suppression, and Toughness of Bismaleimide Resin AITranslate

University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China; University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although the bismaleimide (BMI) resin is a star material in industries, its further applications have been plagued by the serious brittleness and fire hazard for a long time. Hence, a core–shell architecture (MPPM) derived from covalent triazine frameworks was designed to overcome the shortcomings. Excitedly, compared to those of neat BMI, the resultant BMI-2 with only 1 wt % MPPM was capable of achieving 23.4%, 48.6%, and 39.7% decrements on the peak of heat release rate, total heat release, and total smoke release, respectively, exhibiting unprecedented flame-retardant effects under a low addition of flame retardants. Besides, the impact strength of BMI-2 was enhanced by 62.7% with a close tensile strength and storage modulus to those of neat BMI, implying that the toughness of BMI was improved successfully without sacrificing its rigidity. This work provided a unique clue for designing efficient multifunctional modifiers and promoted the development of advanced BMI.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01173

Chinese Library Classification Number:

Citation Information:

Although the bismaleimide (BMI) resin is a star material in industries, its further applications have been plagued by the serious brittleness and fire hazard for a long time. Hence, a core–shell architecture (MPPM) derived from covalent triazine frameworks was designed to overcome the shortcomings. Excitedly, compared to those of neat BMI, the resultant BMI-2 with only 1 wt % MPPM was capable of achieving 23.4%, 48.6%, and 39.7% decrements on the peak of heat release rate, total heat release, and total smoke release, respectively, exhibiting unprecedented flame-retardant effects under a low addition of flame retardants. Besides, the impact strength of BMI-2 was enhanced by 62.7% with a close tensile strength and storage modulus to those of neat BMI, implying that the toughness of BMI was improved successfully without sacrificing its rigidity. This work provided a unique clue for designing efficient multifunctional modifiers and promoted the development of advanced BMI.

quote

GB/T 7714-2015 [1] Xin Jiang, Fukai Chu, Wei Liu, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01173.
MLA [1] Xin Jiang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01173.
APA [1] Xin Jiang, Fukai Chu, Wei Liu, Yuan Hu, Weizhao Hu, & Lei Song. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01173
IEEE [1] Xin Jiang, Fukai Chu, Wei Liu, Yuan Hu, Weizhao Hu, and Lei Song, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01173.