Experimental Research on the Static Separation of Rhenium from Molybdenum with D314 Resin AITranslate
Abstract AITranslate
Experiments on the separation of rhenium from molybdenum were carried out with a macroporous alkalescence acrylic anion exchange regenerative resin(D314).The absorption and desorption conditions of rhenium and molybdenum were studied.The results show that rhenium and molybdenum can be adsorbed together in the solution of pH4.0~7.0.Rhenium can be separated from molybdenum by first using the eluent of 8% NH3·H2O+10% NH4NO3 to desorb molybdenum and then using 4% NH3·H2O to desorb rhenium.The above process is applied in rhenium separation from molybdenum of molybdenum ash,the obtained molybdenum can be used for preparing ammonium dodecamolybdate with a purity of 98.78%,and the trace rhenium is enriched by nearly 1 000 times,which provides favorable conditions for the downstream concentration extraction process.
KeyWords AITranslate
1王靖芳,罗锦超,冯彦琳,魏志华.N7301萃取铼的研究[J].有色金属:冶炼部分,2001(2):29-30. 被引量:14
2邹振球,周勤俭.钼精矿石灰焙烧-N_(235)萃取工艺提取钼铼[J].矿冶工程,2002,22(1):79-81. 被引量:33
3邓解德.从含钼废液中萃取回收铼[J].中国钼业,1999,23(2):32-36. 被引量:16
4刘峙嵘,刘欣萍,彭雪娇,刘健强,穆士忠.阴离子交换树脂F3吸附铼的研究[J].稀有金属,2002,26(3):221-224. 被引量:18
5刘峙嵘,刘欣萍,刘健强,许光东.SMF-425树脂吸附和解吸铼的研究[J].湿法冶金,2002,21(2):70-75. 被引量:18
6宋金如,龚治湘,刘淑娟,邓义琴.P_(350)萃淋树脂吸附铼的性能研究及应用[J].华东地质学院学报,2003,26(3):274-278. 被引量:16
7郭锦勇,李庸华,杨志平,柯家骏.D-990离子交换树脂吸附铂和铼性能的研究[J].稀有金属,2000,24(6):401-405. 被引量:12
8李玉萍,李莉芬,王献科.液膜法提取高纯铼[J].中国钼业,2001,25(6):23-26. 被引量:26
9蒋克旭,邓桂春,赵丽艳,孟伟,王晓娜,李莹,翟玉春.催化动力学光度法测定钼样品中痕量铼[J].分析化学,2009,37(2):312-312. 被引量:9
1王晓龙,俎建华,韦悦周.AR-01树脂对铼的吸附和解吸行为[J].核化学与放射化学,2014,36(4):205-209. 被引量:1
2刘燕,李来平,张新,蒋丽娟,林小辉,杨健,李延超.钼铼分离富集技术的研究进展[J].中国钼业,2015,39(4):6-9. 被引量:2
3孟晗琪,陈昆昆,吴贤,马光.高温合金及其再生回收现状[J].广州化工,2015,43(18):14-16. 被引量:2
4常云龙,刘洋,邓丽,宋增意,刘丹.NH_4SCN解吸剂对负载Re的D296树脂的解吸影响[J].沈阳工业大学学报,2016,38(3):263-267. 被引量:1
5刘红召,王力军,张博,王威.一种弱碱性树脂对淋洗液中铼的静态吸附性能[J].稀有金属,2017,41(9):1028-1034. 被引量:12
6刘伟,丁留亮,郭明宜,李继文,魏世忠.钼冶金中铼的综合提取研究进展[J].稀有金属与硬质合金,2017,45(5):1-6. 被引量:4
7赵恒勤,宁阳坤,王威,张博,刘红召,任保增.D314树脂吸附钼的试验研究[J].矿冶工程,2018,38(1):81-83. 被引量:5
8Hong-Zhao Liu,Bo Zhang,Xiao-Jing Jing,Wei Wang,Li-Jun Wang.Adsorption and desorption properties for rhenium using a kind of weak-base anion resin[J].稀有金属:英文版,2018,37(8):707-715. 被引量:9
9刘红召,井小静,张博,王威,王力军.提高钼冶炼废酸中钼离子交换吸附性能的研究[J].稀有金属,2019,43(3):312-318. 被引量:8
10胥国龙,闻振乾,原渊,姚益轩,张翀,刘双民,腾飞.用N235从高浓度盐酸溶液中萃取铼[J].湿法冶金,2021,40(3):224-228. 被引量:3
1于凯,艾峥嵘,宁志强,胡伟,谢宏伟.离子交换法净化硝酸银溶液吸附过程研究[J].稀有金属,2021,45(11):1352-1358. 被引量:3
2汪振文,王会才,杨继斌,刘霞平,岳瑞瑞.吸附法去除水中重金属复合污染物的研究状况[J].稀有金属,2020,0(1):87-99. 被引量:19
3张妮,卢苏君,张素超.铼的提纯分离研究现状[J].金川科技,2017,0(1):46-49. 被引量:1
4刘伟,丁留亮,郭明宜,李继文,魏世忠.钼冶金中铼的综合提取研究进展[J].稀有金属与硬质合金,2017,45(5):1-6. 被引量:4
5Hong-Zhao Liu,Bo Zhang,Xiao-Jing Jing,Wei Wang,Li-Jun Wang.Adsorption and desorption properties for rhenium using a kind of weak-base anion resin[J].稀有金属:英文版,2018,37(8):707-715. 被引量:9
6刘雪梅,马闯,陶嘉熙,田秉汝.生物吸附材料对Cr(Ⅵ)的吸附研究进展[J].应用化工,2018,47(7):1509-1512. 被引量:7
7井小静,赵恒勤,刘红召,张博,任保增.钼精矿焙烧烟尘中回收铼的研究进展[J].有色金属:冶炼部分,2018(11):42-46. 被引量:11
8刘红召,井小静,张博,王威,王力军.提高钼冶炼废酸中钼离子交换吸附性能的研究[J].稀有金属,2019,43(3):312-318. 被引量:8
9杨海,黄新,林子增,何秋玫,丁炜.离子交换法处理重金属废水的研究进展[J].应用化工,2019,48(7):1675-1680. 被引量:34
10郭树军,董雪平.铪在高温合金中的应用及回收[J].广州化工,2019,47(13):38-40. 被引量:1
1刘红召,曹耀华,王威,高照国.离子交换法从钨钼氧化矿浸出渣洗水中回收钼、钨试验研究[J].湿法冶金,2015,34(1):35-38. 被引量:6
2何焕杰.大孔弱碱性树脂吸附铼的动力学研究[J].湿法冶金,1993(4):14-17.
3何焕杰,詹适新,王永红.D380大孔弱碱性树脂吸附钼的机理研究[J].湿法冶金,1994,13(2):40-44. 被引量:3
4魏宗武,陈建华,艾光华,刘智林.生物浸出——萃取法分离彩钼铅矿的研究[J].有色矿冶,2007,23(1):22-24. 被引量:4
5郭双华.用D314离子交换树脂从沉钼后液中回收钼[J].湿法冶金,2015,34(6):471-473. 被引量:2
6孙应.石煤提钒后液中钼的回收[J].有色金属:冶炼部分,2009(3):11-12. 被引量:2
7吴占贤.粉煤灰是生产保护渣的资源[J].中国物资再生,1997(8):11-12.
8李青刚,张启修,肖连生.离子交换树脂吸附镍钼矿氯浸液中钼的研究[J].稀有金属,2007,31(3):351-356. 被引量:14
9任宝江.钼泥废料中提取钼的工艺研究[J].中国钼业,2011,35(1):12-14. 被引量:2
10胡长柏.矿石预先造粒堆浸金的扩大试验研究[J].铀矿冶,1993,12(2):127-127.
Basic Information:
DOI:
Chinese Library Classification Number:TF803.23[冶金工程—有色金属冶金]
Citation Information:
Experiments on the separation of rhenium from molybdenum were carried out with a macroporous alkalescence acrylic anion exchange regenerative resin(D314).The absorption and desorption conditions of rhenium and molybdenum were studied.The results show that rhenium and molybdenum can be adsorbed together in the solution of pH4.0~7.0.Rhenium can be separated from molybdenum by first using the eluent of 8% NH3·H2O+10% NH4NO3 to desorb molybdenum and then using 4% NH3·H2O to desorb rhenium.The above process is applied in rhenium separation from molybdenum of molybdenum ash,the obtained molybdenum can be used for preparing ammonium dodecamolybdate with a purity of 98.78%,and the trace rhenium is enriched by nearly 1 000 times,which provides favorable conditions for the downstream concentration extraction process.
quote
| GB/T 7714-2015 | [1] JIANG Ke-xu, DENG Gui-chun, ZHANG Qian, et al. Experimental Research on the Static Separation of Rhenium from Molybdenum with D314 Resin[J]. Rare Metals and Cemented Carbides, 2011(1): 8-12. |
| MLA | [1] JIANG Ke-xu, et al., "Experimental Research on the Static Separation of Rhenium from Molybdenum with D314 Resin." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 8-12. |
| APA | [1] JIANG Ke-xu, DENG Gui-chun, ZHANG Qian, ZHANG Jun, & DI Yu-chun. (2011). Experimental Research on the Static Separation of Rhenium from Molybdenum with D314 Resin. Rare Metals and Cemented Carbides(1), 8-12. |
| IEEE | [1] JIANG Ke-xu, DENG Gui-chun, ZHANG Qian, ZHANG Jun, and DI Yu-chun, "Experimental Research on the Static Separation of Rhenium from Molybdenum with D314 Resin," Rare Metals and Cemented Carbides, no. 1, pp. 8-12, 2011. keywords: {rhenium;molybdenum;separation;D314 resin;molybdenum ash} |