New Process of Vanadium Extraction from Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A new process of vanadium extraction from alkali leach liquor of carbonaceous shale containing vanadium was studied.The process includes the four steps of silicon initial removal,vanadium alkali extraction,silicon washing removal and vanadium stripping.The results show that the silicon removal rate is up to 99.58% by controlling the final pH value at 9.5,keeping the ratio of organic phase(N263) to aqueous phase at 1/4,and employing Na2CO3 solution(pH=10) as the eluent.The process is simple,and both its vanadium recovery and separation efficiency of vanadium and silicon are high.

KeyWords AITranslate

carbonaceous shale containing vanadium alkali leach liquor silicon removal rate pH value N263 solvent extraction

1浙江省煤炭工业局.石煤的综合利用[M].北京:煤炭工业出版社,1980.

2张生.二氧化硅水溶物种与热力学性质[J].世界地质,1997,16(2):16-22. 被引量:10

3Li Zeng, Chu Yongcheng. A literature review of the recovery of molybdenum and vanadium from spent hydrodesulphurisation catalysts (Part Ⅱ) :Separation and purification[J]. Hydrometallurgy, 2009,98 (1-2) : 10-20.

4刘波,冯光熙,黄祥玉,张敏.用N-263从钒溶液中回收钒[J].化学研究与应用,2003,15(1):54-57. 被引量:26

1何东升,秦芳,徐雄依.石煤酸浸过程酸浓度与电位变化[J].现代矿业,2011(12):12-14. 被引量:2

2陈金清,熊家任,林凯.碱性体系下萃取钒的研究[J].有色金属科学与工程,2014,5(1):20-24. 被引量:6

3齐兆树,李青刚.从碱性含钒溶液中萃取钒的研究[J].有色金属:冶炼部分,2014(10):43-48. 被引量:3

4周小舟,曹佐英,肖连生,张魁芳,张贵清,李青刚.硫酸型季铵盐从石煤苏打浸出液中萃取钒的研究[J].矿冶工程,2015,35(1):68-71. 被引量:8

5阳亚玲,颜文斌,华骏,高峰,易静,张晓君,何新波.含钒浸出液除硅试验研究[J].非金属矿,2015,38(2):8-10. 被引量:2

6张莹,张廷安.溶剂萃取法从含钒浸出液中提钒的研究进展[J].有色金属科学与工程,2017,8(5):14-20. 被引量:11

7刘波.碱性含钒浸出液除硅研究及高纯五氧化二钒制备[J].钢铁钒钛,2019,40(5):8-15. 被引量:2

8李青芸,成宝海,徐乔楚,杨丽娜.D290离子交换树脂从石煤含钒浸出液中提取钒的研究[J].山西化工,2020,40(6):7-10. 被引量:3

9秦身钧,徐飞,崔莉,王金喜,李神勇,赵泽森,肖林,郭彦霞,赵存良.煤型战略关键微量元素的地球化学特征及资源化利用[J].煤炭科学技术,2022,50(3):1-38. 被引量:11

10朱思琴,叶国华,亢选雄,梁雪崟.含钒酸浸液净化与富集的研究进展[J].钢铁钒钛,2022,43(5):10-22. 被引量:1

1关洪亮,操艳兰,顾逸雅,李彩霞,王杏林,何东升,余训民.硫酸亚铁沉淀法处理含钒废水[J].武汉工程大学学报,2012,34(12):25-27. 被引量:8

2李嘉豪,曹佐英,李嘉,张贵清,李青刚,曾理,关文娟.高级脂肪胺类萃取剂在稀有金属溶剂萃取中的应用[J].稀有金属与硬质合金,2018,46(6):10-18. 被引量:1

3陈金清,林凯,熊家任,段敏,黄亚祥.改性季铵盐从高碱度溶液中萃取钒的研究[J].有色金属科学与工程,2015,6(2):21-26. 被引量:4

4康立武,胡江平,李强.用P204从废钒催化剂中萃取钒[J].有色金属:冶炼部分,2016(1):46-48. 被引量:3

5华骏,颜文斌,高峰,易静,刘倩倩.湘西石煤湿法提钒中复合添加剂的研究[J].矿冶工程,2016,36(1):72-75. 被引量:6

6曾辉,彭万通.用中和水解法从粗钴盐溶液中除硅[J].湿法冶金,2016,35(3):235-238. 被引量:2

7张一敏,包申旭.含钒浸出液净化富集技术现状及前景[J].金属矿山,2016,45(7):64-70. 被引量:9

8邓海碧,曹佐英,李嘉豪.新型季铵盐的合成及其与N263的碱性萃钒效果比较[J].稀有金属与硬质合金,2016,44(4):1-4. 被引量:2

9丁扬力,肖连生,曹佐英,张贵清,曾理.N263从钼酸钠溶液中萃取分离钼钒[J].有色金属科学与工程,2017,8(1):15-20. 被引量:6

10黄俊,张一敏,黄晶,刘涛,薛楠楠.石煤焙烧样循环加压酸浸提钒降杂研究[J].稀有金属,2017,41(6):701-708. 被引量:6

1曹耀华,刘红召,高照国,杨绍文.从彩钼铅粗精矿碱性浸出液中提取钼的新工艺[J].湿法冶金,2012,31(2):118-121. 被引量:6

2张立征,靳冉公,戚兴传,李云,王云.含锑金精矿的硫化钠碱性浸出液中锑电积试验[J].有色金属:冶炼部分,2015(10):22-24. 被引量:7

3陈惠,张岩岩,李建文,司士辉.石煤微波辅助提钒及浸出液除杂研究[J].稀有金属与硬质合金,2011,39(2):1-5. 被引量:3

4张曦,邹晓勇.含钒液体除硅过程的研究[J].金属材料与冶金工程,2007,35(6):19-22.

5李静,王素素,徐辉,高峰,颜文斌.硫酸镁去除工业偏钒酸铵中磷和硅的研究[J].广州化工,2012,40(22):64-66. 被引量:6

6李运姣,孙昭明,李洪桂,孙培梅,苏鹏抟,刘茂盛.Na_2WO_4溶液结晶过程中除砷、硅等杂质[J].中南工业大学学报,2001,32(3):251-254. 被引量:2

7曾美云,张萍,汤志勇.含钒碱浸液沉淀法除硅研究[J].稀有金属,2010,34(S1):80-83. 被引量:3

8阳亚玲,颜文斌,华骏,高峰,易静,张晓君,何新波.含钒浸出液除硅试验研究[J].非金属矿,2015,38(2):8-10. 被引量:2

9肖超,肖连生,李青刚.石煤提钒碱浸液的除硅实验研究[J].稀有金属与硬质合金,2010,38(1):8-10. 被引量:6

10曾美云,张萍,汤志勇.含钒碱浸液除硅试验研究[J].湿法冶金,2011,30(2):159-162. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

A new process of vanadium extraction from alkali leach liquor of carbonaceous shale containing vanadium was studied.The process includes the four steps of silicon initial removal,vanadium alkali extraction,silicon washing removal and vanadium stripping.The results show that the silicon removal rate is up to 99.58% by controlling the final pH value at 9.5,keeping the ratio of organic phase(N263) to aqueous phase at 1/4,and employing Na2CO3 solution(pH=10) as the eluent.The process is simple,and both its vanadium recovery and separation efficiency of vanadium and silicon are high.

quote

GB/T 7714-2015 [1] XIAO Chao, XIAO Lian-sheng, CHENG Bao-hai, et al. New Process of Vanadium Extraction from Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium[J]. Rare Metals and Cemented Carbides, 2011(1): 4-7.
MLA [1] XIAO Chao, et al., "New Process of Vanadium Extraction from Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 4-7.
APA [1] XIAO Chao, XIAO Lian-sheng, CHENG Bao-hai, & CAO Zuo-ying. (2011). New Process of Vanadium Extraction from Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium. Rare Metals and Cemented Carbides(1), 4-7.
IEEE [1] XIAO Chao, XIAO Lian-sheng, CHENG Bao-hai, and CAO Zuo-ying, "New Process of Vanadium Extraction from Alkali Leach Liquor of Carbonaceous Shale Containing Vanadium," Rare Metals and Cemented Carbides, no. 1, pp. 4-7, 2011. keywords: {carbonaceous shale containing vanadium;alkali leach liquor;silicon removal rate;pH value;N263;solvent extraction}