Concentration Improvement of Ammonia Water Resulting from Ammonia Tail Gas Condensation in the Process of APT Crystallization AITranslate
Abstract AITranslate
The influences of condensation and evaporation area ratio,crystallization temperature and stirring rate were investigated on the concentration of the ammonia water resulting from ammonia tail gas condensation in the process of APT crystallization.The results show that both lower crystallization temperature and faster stirring rate can increase ammonia concentration of the recovered solution from crystallization ammonia tail gas.When the condensation and vaporization area ratio is 3.9 and the crystallization temperature is 110 ℃,the total ammonia concentration of the recovered solution is 9.9 mol/L.
KeyWords AITranslate
1万林生,胡之钧,于浓芳,魏光敬.NH_4Cl-NH_3·H_2O-H_2O系仲钨酸铵结晶动力学Ⅰ仲钨酸铵蒸发结[J].中国有色金属学报,1994,4(4):41-45. 被引量:12
2聂民.仲钨酸铵生产过程中回收氨的探讨[J].江西冶金,1999,19(5):26-27. 被引量:1
3何长仪,刘志明,张浩军.钨湿法冶炼氨的回用[J].湖南有色金属,1999,15(5):20-22. 被引量:5
1万林生,邓登飞,赵立夫,李红超,徐国钻,梁勇.钨绿色冶炼工艺研究方向和技术进展[J].有色金属科学与工程,2013,4(5):15-18. 被引量:18
1万林生,舒柳飞,赵立夫,谌勇明,李红超.黑钨矿与碳酸钙人工合成白钨的反应过程和机理[J].稀有金属与硬质合金,2014,42(2):1-4. 被引量:3
2万林生,黄小晶,杨亮,邓登飞,李红超,谌勇明.钨酸钠溶液氢氧化钙苛化-沉淀白钨的研究[J].有色金属科学与工程,2014,5(4):23-27. 被引量:3
3黄泽辉,韩宝军,邓登飞,龚丹丹,邓声华,李红超.煤渣过滤调酸钨冶炼废水的研究[J].赣南师范学院学报,2014,35(6):46-48. 被引量:1
4万林生,潘明然,谌勇明,赵立夫,李红超.黑钨矿与碳酸钙人工合成白钨工艺研究[J].稀有金属与硬质合金,2014,42(6):1-3.
5刘飞飞,罗贤平,辛鹏武,龚亚忠.基于机器视觉的钨浓度在线检测系统[J].中国钨业,2015,30(6):73-76. 被引量:1
6刘飞飞,罗贤平,古帅奇,辛鹏武.碱煮过程浸出率预测与优化研究[J].有色金属:冶炼部分,2016(5):29-32. 被引量:1
7万林生,张龙辉,赖星任,杨亮,梁勇,刘鹏.(NH_4)_2HPO_4-H_2O系仲钨酸铵溶解性能及磷钨杂多酸形成的影响[J].稀有金属与硬质合金,2016,44(3):1-4. 被引量:1
8万林生,金先文,赖星任,杨亮,刘鹏,梁勇.(NH_4)_2HPO_4-NH_3·H_2O-H_2O系APT溶解度研究[J].稀有金属与硬质合金,2016,44(5):6-10. 被引量:1
9杨金洪,李江涛,刘文婷,赵中伟.硝酸-磷酸混合溶液中钨的萃取[J].中国有色金属学报,2018,28(5):1024-1032. 被引量:2
10曹才放,章行,李小文,邱晓辰,李昱芃,钟镇宇,王艺瞾,王建松.氯型季铵树脂对钨酸根吸附的热力学研究[J].有色金属科学与工程,2018,9(3):1-4. 被引量:2
1李凯,王服群,刘成,雷涛.利用渗滤液中氨尾气进行烟气脱硝的可行性研究[J].工业安全与环保,2015,41(1):36-39. 被引量:1
2阿不都克里木.我厂合成氨尾气的综合利用[J].中氮肥,2012(3):37-38.
3罗章青,廖小英,王文华,陈树茂.从APT结晶尾气中回收氨的工业实践[J].稀有金属,2007,31(S1):90-92. 被引量:5
4杜雯.钨冶金过程氨尾气的治理与循环利用工艺研究[J].中国钨业,2008,23(6):43-46. 被引量:4
5吕振水,杨翠彦.氨焚烧及硫磺生产的尾气利用[J].河北冶金,2005(2):67-68. 被引量:1
6无动力氨回收技术成功应用[J].化学工业与工程技术,2005,26(4):50-50.
7徐晓华,徐光来.基于GIS的中国酸雨控制区酸雨空间分布特征研究[J].石家庄学院学报,2014,16(3):77-83. 被引量:4
8王飞,贾军.宁安化工合成氨尾气提取LNG装置的设计探讨[J].中氮肥,2014(2):22-24.
9世界最大炼油厂启动新型脱硫系统[J].现代化工,2010(1):96-96.
10李清海,杨瑞昌,于凤玲,王彦武,周立加.修正PR方程在深冷分离回收氢气设备设计计算中的应用[J].低温与特气,1999,17(4):24-26. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:X758[环境科学与工程—环境工程]
Citation Information:
The influences of condensation and evaporation area ratio,crystallization temperature and stirring rate were investigated on the concentration of the ammonia water resulting from ammonia tail gas condensation in the process of APT crystallization.The results show that both lower crystallization temperature and faster stirring rate can increase ammonia concentration of the recovered solution from crystallization ammonia tail gas.When the condensation and vaporization area ratio is 3.9 and the crystallization temperature is 110 ℃,the total ammonia concentration of the recovered solution is 9.9 mol/L.
quote
| GB/T 7714-2015 | [1] WAN Lin-sheng, WANG Zhong-bing, FU Zhan-hui, et al. Concentration Improvement of Ammonia Water Resulting from Ammonia Tail Gas Condensation in the Process of APT Crystallization[J]. Rare Metals and Cemented Carbides, 2011(1): 13-16. |
| MLA | [1] WAN Lin-sheng, et al., "Concentration Improvement of Ammonia Water Resulting from Ammonia Tail Gas Condensation in the Process of APT Crystallization." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 13-16. |
| APA | [1] WAN Lin-sheng, WANG Zhong-bing, FU Zhan-hui, & XI Xue-kang. (2011). Concentration Improvement of Ammonia Water Resulting from Ammonia Tail Gas Condensation in the Process of APT Crystallization. Rare Metals and Cemented Carbides(1), 13-16. |
| IEEE | [1] WAN Lin-sheng, WANG Zhong-bing, FU Zhan-hui, and XI Xue-kang, "Concentration Improvement of Ammonia Water Resulting from Ammonia Tail Gas Condensation in the Process of APT Crystallization," Rare Metals and Cemented Carbides, no. 1, pp. 13-16, 2011. keywords: {APT;crystallization tail gas;condensation recovery;ammonia water concentration} |