Experimental Research on Silicon Extraction from the Filter Residue in the Process of Titanium Extraction of Roasted Titanium Slag with Concentrated Sulfuric Acid AITranslate

Shenyang Medical College Basic Medical College;Northeast University School of Materials Metallurgy
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The process conditions were investigated of silicon extraction and calcium silicate preparation from the filter residue in the process of titanium extraction of roasted titanium slag with concentrated sulfuric acid. The main process steps include alkali-solution and calcification. The effects were investigated of NaOH-residue mass ratio, reaction temperature, reaction time and liquid-solid mass ratio on SiO2 extraction rate from the filter residue during alkali-solution. The optimum operating conditions of alkali-solution are obtained as follows: reaction temperature of 190 ℃ ,NaOH-residue mass ratio of 3 : 1 ,liquid-solid mass ratio of 4.5 : 1 and reaction time of 60 min. And SiO2 extraction rate is 74.09 % under the above conditions. The effects were investigated of reaction temperature and reaction time on calcification rate of sodium silicate solution during calcification. The optimum operating conditions of calcification are obtained as follows: reaction temperature of 100 ℃ and reaction time of 45 min. And the calcification rate of sodium silicate solution is 94% under the above conditions. Calcium silicate powder product contains 44.36% CaO and its main phase is CaSiO3 ,having loose and porous morphology and micron-level particle size.

KeyWords AITranslate

titanium slag filter residue alkali-solution calcification silicon dioxide calcium silicate

1王甲春,阎培渝.ETIC外墙外保温系统对室内居住环境的影响[J].新型建筑材料,2003,30(2):5-7. 被引量:2

2林青,李延报,兰祥辉,陆春华,许仲梓.水硬性硅酸钙生物材料的研究[J].硅酸盐通报,2008,27(3):556-561. 被引量:2

3张寿国,谢红波,李国忠.硅酸钙保温材料研究进展[J].建筑节能,2006,34(1X):28-30. 被引量:18

4刘晓文,黄圣生,邱冠周.硅灰石粉末的制备和应用现状[J].矿产保护与利用,2001,21(1):20-24. 被引量:24

5李酽.硅灰石的研究与应用进展[J].化工矿物与加工,2004,33(4):1-4. 被引量:25

6王焕磊.我国硅灰石的生产应用及深加工现状[J].中国非金属矿工业导刊,2005(5):14-16. 被引量:10

7余丽秀,孙亚光,张然.硅灰石合成及应用[J].化工新型材料,2005,33(1):58-60. 被引量:18

8于乾.我国硅灰石的在陶瓷工业中的应用[J].建筑材料工业信息,2004(1):3-4.

9陈淑祥,倪文,江翰,董文辉.超轻硬硅钙石型硅酸钙绝热材料制备技术国内外研究现状[J].新型建筑材料,2004,31(1):53-55. 被引量:11

10李懋强,陈玉峰,夏淑琴,李建辉,梁宏勋.超轻微孔硅酸钙绝热材料的显微结构和工艺控制[J].硅酸盐学报,2000,28(5):401-406. 被引量:28

1张晗,隋丽丽,葛欣,翟玉春.钛渣硫酸铵焙烧法提钛渣提硅试验研究[J].矿产综合利用,2018(1):111-114. 被引量:2

2徐丽霜,隋丽丽,葛欣,翟玉春,邵爽.碱浸提钛渣提硅实验过程及其动力学研究[J].稀有金属与硬质合金,2019,47(4):20-23.

3隋丽丽,张俊,马明阳,翟玉春,董微,常红.浓硫酸焙烧钛渣后的滤渣碱浸动力学研究[J].稀有金属与硬质合金,2020,48(6):20-23. 被引量:1

1周娴,李文光,包崇军,刘捷.响应曲面法优化钛渣酸浸实验研究[J].云南冶金,2021,50(3):55-60. 被引量:2

2隋丽丽,马明阳,翟玉春,张俊,张大军.硫酸铵焙烧法提钛渣碱浸提硅反应动力学[J].矿产综合利用,2022(1):142-145. 被引量:1

3刘荣江,刘丽娜.含钛高炉渣的综合利用[J].山西冶金,2023,46(8):80-82.

1何宾宾,张晖,尹伟,傅英,赵智波,陆伟才,周琼波.磷石膏制备硫酸钙晶须的研究[J].磷肥与复肥,2016,31(6):18-20. 被引量:1

2程志民,安霞.钢铁行业环保标准的升级与应对措施研究[J].山西建筑,2013,39(32):186-187. 被引量:2

3王湖坤,熊玲,龚文琪.复合混凝剂的制备及处理垃圾渗滤液的研究[J].武汉理工大学学报,2008,30(4):69-72. 被引量:4

4李富华,孔青青,康亚璞,林晓璇,王枫亮,陈平,刘国光,吕文英,姚琨.BiVO_4联合H_2O_2或K_2S_2O_8光催化降解布洛芬[J].环境工程学报,2016,10(10):5380-5386. 被引量:2

5王宝辉,张学佳,纪巍,阮琴,匡丽.聚丙烯酰胺在黑土上的吸附解吸特性研究[J].化学工程,2009,37(7):9-12. 被引量:3

6张兵兵,于丹丹,王芳,李俊峰.废脱硝催化剂中五氧化二钒回收工艺研究[J].河南科学,2016,34(6):866-870. 被引量:12

7张宇浩,熊易.浅谈《动态微生物好氧发酵技术》在污水处理厂污泥处理应用中的主要工序[J].林业科技情报,2014,46(2):60-61.

8雷存喜,文岳中.对某复杂含铟锑渣浸取方法的研究[J].益阳师专学报,1998,15(5):36-42. 被引量:1

9李耀忠.合成氨主要工序重大事故危险与防范[J].安全与健康,2002(01S):41-42.

10郭文霞,吴永军.TiO_2/CaSiO_3复合型光催化剂的制备及其性能研究[J].广州化工,2015,43(23):102-104.

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

The process conditions were investigated of silicon extraction and calcium silicate preparation from the filter residue in the process of titanium extraction of roasted titanium slag with concentrated sulfuric acid. The main process steps include alkali-solution and calcification. The effects were investigated of NaOH-residue mass ratio, reaction temperature, reaction time and liquid-solid mass ratio on SiO2 extraction rate from the filter residue during alkali-solution. The optimum operating conditions of alkali-solution are obtained as follows: reaction temperature of 190 ℃ ,NaOH-residue mass ratio of 3 : 1 ,liquid-solid mass ratio of 4.5 : 1 and reaction time of 60 min. And SiO2 extraction rate is 74.09 % under the above conditions. The effects were investigated of reaction temperature and reaction time on calcification rate of sodium silicate solution during calcification. The optimum operating conditions of calcification are obtained as follows: reaction temperature of 100 ℃ and reaction time of 45 min. And the calcification rate of sodium silicate solution is 94% under the above conditions. Calcium silicate powder product contains 44.36% CaO and its main phase is CaSiO3 ,having loose and porous morphology and micron-level particle size.

quote

GB/T 7714-2015 [1] SUI Li-li, DI Yu-chun. Experimental Research on Silicon Extraction from the Filter Residue in the Process of Titanium Extraction of Roasted Titanium Slag with Concentrated Sulfuric Acid[J]. Rare Metals and Cemented Carbides, 2016(4): 28-31.
MLA [1] SUI Li-li, and DI Yu-chun. "Experimental Research on Silicon Extraction from the Filter Residue in the Process of Titanium Extraction of Roasted Titanium Slag with Concentrated Sulfuric Acid." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 28-31.
APA [1] SUI Li-li, & DI Yu-chun. (2016). Experimental Research on Silicon Extraction from the Filter Residue in the Process of Titanium Extraction of Roasted Titanium Slag with Concentrated Sulfuric Acid. Rare Metals and Cemented Carbides(4), 28-31.
IEEE [1] SUI Li-li and DI Yu-chun, "Experimental Research on Silicon Extraction from the Filter Residue in the Process of Titanium Extraction of Roasted Titanium Slag with Concentrated Sulfuric Acid," Rare Metals and Cemented Carbides, no. 4, pp. 28-31, 2016. keywords: {titanium slag;filter residue;alkali-solution;calcification;silicon dioxide;calcium silicate}