Study on the Preparation of Ti-enriched Slag by Chemical Beneficiation of Red Mud AITranslate

School of Materials Science and Engineering, Henan University of Technology;School of Materials Science and Engineering, Henan University of Technology;School of Materials Science and Engineering, Henan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation method of Ti-enriched slag was studied by hydrochloric acid leaching of impurities from red mud. The effects of hydrochloric acid concentration, leaching temperature, liquid-solid ratio and leaching time on titanium dioxide grade of Ti-enriched slag were investigated. Phase transformation and action mechanism of the acid leaching process were analyzed by ICP-AES and XRD. The results show that under the conditions of hydrochloric acid concentration of 30%,leaching temperature of 80 ℃,liquidsolid ratio of 7 : 1 and leaching time of 60 min, the titanium dioxide grade of Ti-enriched slag can reach 24 %. With the increase of concentration of hydrochloric acid, calcite in the red mud disappears, the hema- tite,cancrinite and perovskite gradually dissolve, but the brookite and quartz haraly dissolved.

KeyWords AITranslate

red mud Ti-enriched slag TiO2 chemical beneficiation hydrochloric acid leaching phase transformation action mechanism

1LIU W C,SUN S Y,ZHANG L,et al. Experimental and simulative study on phase transformation in Bayer red mud soda-lime roasting system and recovery of A1, Na and Fe[J]. Minerals Engineering, 2012, 39 (12) .. 213 - 218.

2南相莉,张廷安,刘燕,豆志河.我国赤泥综合利用分析[J].过程工程学报,2010,10(S1):264-270. 被引量:127

3姜平国,廖春发.盐酸浸出赤泥分离有价金属的工艺研究[J].中国矿业,2011,20(12):85-87. 被引量:15

4OCHSENKUHN- PETROPULU M, LYBEROPULU T, OCHSENKIIHN K M, et al. Recovery of lanthanides and yttrium from red mud by selective leaching[J]. An- alytica Chimica Acta,1996,319(1/2) :249-254.

5孙道兴.赤泥脱碱处理和有价金属钛钪提取的研究[J].无机盐工业,2008,40(10):49-52. 被引量:39

6GHOSH I,GUHA S,BALASUBRAMANIAM R, et al. Leaching of metals from fresh and sintered red mud[J].Journal of Hazardous Materials, 2011, 185 (2/3) : 662- 668.

7王克勤,宋嘉伟,高燕,姜武.氧化铝赤泥盐酸浸出稀土元素研究[J].稀有金属,2012,36(4):676-680. 被引量:16

8李小斌,肖伟,刘伟,刘桂华,彭志宏,周秋生,齐天贵.Recovery of alumina and ferric oxide from Bayer red mud rich in iron by reduction sintering[J].中国有色金属学会会刊:英文版,2009,19(5):1342-1347. 被引量:31

9AGATZINI-LEONARDOU S, OUSTADAKIS P,TSA- KIRIDIS P E,et al. Titanium leaching from red mud by diluted sulfuric acid at atmospheric pressure[J]. Journal of Hazardous Materials, 2008,157 (2/3) .. 579-586.

10DEEP A,MALIK P,GUPTA B. Extraction and sepa- ration of Ti(Ig) using thiophosphinic acids and its re- covery from ilmenite and red mud[J].Separation Sci- ence and Technology, 2001,36 (4) :671-685.

1王璐,郝彦忠,郝增发.赤泥中有价金属提取与综合利用进展[J].中国有色金属学报,2018,28(8):1697-1710. 被引量:32

2赵恒,李望,牛泽鹏,朱晓波.赤泥制备聚合氯化铝铁及其吸附性能研究[J].稀有金属与硬质合金,2019,47(5):64-68. 被引量:4

3王玲,周晨晨,范燕青,马保中,王成彦,傅昕.赤泥转型-碱溶提铝过程钛的矿相转化[J].中国有色金属学报,2022,32(9):2714-2725.

4吴小华,李雯霏.广西高铁赤泥高值化综合利用途径[J].中国有色冶金,2023,52(2):104-115. 被引量:2

5杨慧,房辉,程志远,郭丰佳,汲庆涛,麻芳,彭倩倩.赤泥资源化综合利用研究进展[J].中国资源综合利用,2023,41(6):109-115.

1雷清源,周康根,何德文,张雪凯.赤泥中钪和钛的回收研究进展[J].矿产保护与利用,2019,39(3):15-20. 被引量:9

2刘世鸿,赵小莲,何奥平,曾建民,吴妮,蒙卓玮,黄寿标,关瑜婷.拜耳法赤泥还原制取抗磨白口铸铁的试验研究[J].铸造,2020,69(1):29-34. 被引量:4

3程相恩,杨惠玲,班俊生,姚永生,王风.电感耦合等离子体质谱法测定三水铝土矿中的15种有效稀土元素[J].化学分析计量,2020,29(3):16-20. 被引量:5

4吴立波,王贻明,陈威,刘家明,陈志强.基于正交实验的赤泥粉煤灰膏体充填材料配比优化[J].矿业研究与开发,2020,40(5):45-49. 被引量:12

5王晗.利用赤泥和粉煤灰吸附去除烟气中SO2的研究[J].中国环保产业,2020(6):35-39. 被引量:2

6郭长路,高益凡,李召峰.利用冶金废渣制备高铁铝酸盐相胶凝材料[J].材料与冶金学报,2020,19(2):105-112. 被引量:1

7李博琦,谢贤,纪翠翠,朱辉,黎洁,康博文.赤泥提钛技术研究现状与展望[J].矿冶,2020,29(6):87-93. 被引量:4

8万军营,陈铁军,周仙霖,罗艳红,陆启财,胡钺.高锰铁矿强化赤泥直接还原试验研究[J].烧结球团,2020,45(6):10-15. 被引量:4

9邢磊,杜培培,龙跃.SiO2/Al_(2)O_(3)对无机纤维微观结构及热稳定性的影响[J].钢铁研究学报,2021,33(1):9-14. 被引量:2

10挑战世界性难题,赤泥综合利用有望成为氧化铝下一个利润风口[J].中国粉体工业,2021(2):54-57.

1朱晓波,管学茂,李望.赤泥酸浸提钛实验研究[J].稀有金属与硬质合金,2015,43(2):11-13. 被引量:22

2李望,朱晓波.赤泥盐酸浸出钇试验研究[J].轻金属,2015(12):20-23.

3李穗中.废干电池热解过程的物相变化研究——《废干电池无害化与资源化技术研究》第一报[J].广州环境科学,2004,19(4):22-25.

4朱申红,荀志远,葛学韬.化学选矿用于处理黄铁矿烧渣[J].化工矿山技术,1997,26(6):37-39. 被引量:8

5朱申红.黄铁矿烧渣综合利用的研究[J].矿产综合利用,1998(2):16-19. 被引量:9

6刘成龙,夏举佩.高铁钛型煤矸石中脱铁富钛试验研究[J].硅酸盐通报,2015,34(3):664-669. 被引量:5

7陈玉洁,韩凤兰,罗钊.镁渣固化/稳定污酸渣中重金属Pb[J].环境工程学报,2016,10(6):3229-3234. 被引量:3

8廖昌华,孙水裕,张志.焚烧温度对电镀污泥后续处理影响研究[J].再生资源研究,2002(5):34-36. 被引量:27

9徐梦,辛志峰,李婷,白林山,董永平,储向峰.水热活化法对粉煤灰中镓浸出效果的影响研究[J].轻金属,2015(11):23-26. 被引量:1

10朱启红.化学药剂对粉煤灰改性作用的研究[J].洁净煤技术,2011,17(1):76-79. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

The preparation method of Ti-enriched slag was studied by hydrochloric acid leaching of impurities from red mud. The effects of hydrochloric acid concentration, leaching temperature, liquid-solid ratio and leaching time on titanium dioxide grade of Ti-enriched slag were investigated. Phase transformation and action mechanism of the acid leaching process were analyzed by ICP-AES and XRD. The results show that under the conditions of hydrochloric acid concentration of 30%,leaching temperature of 80 ℃,liquidsolid ratio of 7 : 1 and leaching time of 60 min, the titanium dioxide grade of Ti-enriched slag can reach 24 %. With the increase of concentration of hydrochloric acid, calcite in the red mud disappears, the hema- tite,cancrinite and perovskite gradually dissolve, but the brookite and quartz haraly dissolved.

quote

GB/T 7714-2015 [1] LI Wang, ZHU Xiao-bo, GUAN Xue-mao. Study on the Preparation of Ti-enriched Slag by Chemical Beneficiation of Red Mud[J]. Rare Metals and Cemented Carbides, 2016(4): 25-27.
MLA [1] LI Wang, et al., "Study on the Preparation of Ti-enriched Slag by Chemical Beneficiation of Red Mud." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 25-27.
APA [1] LI Wang, ZHU Xiao-bo, & GUAN Xue-mao. (2016). Study on the Preparation of Ti-enriched Slag by Chemical Beneficiation of Red Mud. Rare Metals and Cemented Carbides(4), 25-27.
IEEE [1] LI Wang, ZHU Xiao-bo, and GUAN Xue-mao, "Study on the Preparation of Ti-enriched Slag by Chemical Beneficiation of Red Mud," Rare Metals and Cemented Carbides, no. 4, pp. 25-27, 2016. keywords: {red mud;Ti-enriched slag;TiO2;chemical beneficiation;hydrochloric acid leaching;phase transformation;action mechanism}