Study on Physicochemical Properties of WO_3 and W Powders Prepared with Cr-doped APT AITranslate
Abstract AITranslate
WO3 and W powders were prepared with Cr-doped APT as raw material,and their physicochemical properties were studied. The results show that Cr-doped WO3 and W powders have consistent crystal structure with ordinary WO3 and W powders,and Cr exists in the form of Cr2O3 in the two powders. Compared with ordinary W powder,Cr-doped W powder has smaller particle size, good uniformity and complete crystal structure. Cr can effectively inhibit vapor deposition and growth of W power during reduction, but the oxygen index is slightly higher. Cr distribution in both WO3 and W powders is of good macroscopic and microscopic uniformity.
KeyWords AITranslate
1林晨光.中国超细晶粒WC-Co硬质合金研究进展[J].稀有金属,2004,28(4):762-766. 被引量:20
2程涛,汪重露.纳米硬质合金的研究进展[J].稀有金属与硬质合金,2006,34(3):46-50. 被引量:13
3李宁,邱友绪,张伟,文玉华,张勇,周永贵.超细晶硬质合金中VC/Cr_3C_2对晶粒长大的抑制作用及机理研究[J].稀有金属材料与工程,2007,36(10):1763-1766. 被引量:20
4孙东平.添加VC与Cr_3C_2对超细晶硬质合金烧结过程的影响[J].硬质合金,2009,26(3):141-147. 被引量:4
5全峰,周建,刘伟波,刘桂珍.VC/Cr_3C_2对微波烧结超细WC-10Co性能的影响[J].武汉理工大学学报,2007,29(12):49-51. 被引量:5
6刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21
7吴冲浒,聂洪波,肖满斗.中国超细晶硬质合金及原料制备技术进展[J].中国材料进展,2012,31(4):39-46. 被引量:34
8羊建高,谭敦强,陈颢.硬质合金[M].长沙:中南大学出版社,2012.
9万林生,黄海,赵立夫,章秋霖.仲钨酸铵结晶过程掺铬工艺研究[J].中国钨业,2015,30(1):56-60. 被引量:1
10万林生,赖星任,黄海,赵立夫,章秋霖.仲钨酸铵结晶过程掺Cr制备APT的物化性能研究[J].稀有金属与硬质合金,2015,43(5):1-3 15. 被引量:3
1吴晓东,柴永新,傅小明,傅明喜,戴起勋.蓝钨制取超细钨粉的研究[J].稀有金属,2005,29(4):570-573. 被引量:12
2杨超尘,姚犁.低压金刚石涂层技术的发展动向[J].硬质合金,1991,8(2):7-11. 被引量:1
3傅练英,王逸云.紫钨的质量与检测探讨[J].硬质合金,2004,21(1):42-44. 被引量:2
4王季林.钨粉粒度和烧结工艺对高比重钨合金组织结构和力学性能的影响[J].粉末冶金工业,2009,19(2):16-21. 被引量:12
5高丽娜.连铸钢坯纵裂分析[J].一重技术,2004(4):28-29.
6王东,阎圣刚,张爱丽,周科衍.二烯丙基硒的研制[J].低温与特气,1994,12(4):56-57.
7傅练英.降低细颗粒碳化钨中聚集体量的研究[J].硬质合金,2001,18(2):93-98. 被引量:4
8万林生,曾学品,赖星任,杨亮,刘鹏.仲钨酸铵结晶掺Cr制备的WC粉和超细硬质合金的性能研究[J].稀有金属与硬质合金,2016,44(6):54-59. 被引量:6
9徐晓娟,张丽英,郭志猛,吴成义.纳米级WO_3粉的还原动力学特征[J].粉末冶金技术,2002,20(3):147-150. 被引量:11
10赖高惠.抗弯强度高的W-Ni-Fe合金[J].中国钨业,1991,0(12):33-33.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
WO3 and W powders were prepared with Cr-doped APT as raw material,and their physicochemical properties were studied. The results show that Cr-doped WO3 and W powders have consistent crystal structure with ordinary WO3 and W powders,and Cr exists in the form of Cr2O3 in the two powders. Compared with ordinary W powder,Cr-doped W powder has smaller particle size, good uniformity and complete crystal structure. Cr can effectively inhibit vapor deposition and growth of W power during reduction, but the oxygen index is slightly higher. Cr distribution in both WO3 and W powders is of good macroscopic and microscopic uniformity.
quote
| GB/T 7714-2015 | [1] WAN Lin-sheng, XU Li-qiang, HUANG Hai, et al. Study on Physicochemical Properties of WO_3 and W Powders Prepared with Cr-doped APT[J]. Rare Metals and Cemented Carbides, 2016(4): 32-37. |
| MLA | [1] WAN Lin-sheng, et al., "Study on Physicochemical Properties of WO_3 and W Powders Prepared with Cr-doped APT." Rare Metals and Cemented Carbides, no. 4, 2016, pp. 32-37. |
| APA | [1] WAN Lin-sheng, XU Li-qiang, HUANG Hai, ZHAO Li-fu, LIANG Yong, YANG Yun-guang, & ZHANG Qiu-lin. (2016). Study on Physicochemical Properties of WO_3 and W Powders Prepared with Cr-doped APT. Rare Metals and Cemented Carbides(4), 32-37. |
| IEEE | [1] WAN Lin-sheng, XU Li-qiang, HUANG Hai, ZHAO Li-fu, LIANG Yong, YANG Yun-guang, and ZHANG Qiu-lin, "Study on Physicochemical Properties of WO_3 and W Powders Prepared with Cr-doped APT," Rare Metals and Cemented Carbides, no. 4, pp. 32-37, 2016. keywords: {Cr-doped APT;WO3 powder;W powder;physieochemical property;Cr2 O3} |