Study on the Process of Extracting Vanadium Pentoxide from Stone Coal Boiling Roasting Material AITranslate
Abstract AITranslate
In response to the problems of large differences in raw materials,long process flow,low vanadium recovery rate(mostly below 60%),and high cost in extracting vanadium from stone coal boiling roasting materials,a process route of mixing acid,curing and leaching-oxidation neutralization-ion exchange-vana-dium precipitation with ammonium salt-calcination was adopted to extract vanadium.The experimental results show that under the conditions of sulfuric acid dosage of 20% of the raw material weight,curing temperature of 100 ℃,and curing time of 6 h,the vanadium leaching rate of stone coal boiling roasting material reaches 90.2%.The final product V2O5 powder quality is stable and reliable,which reaches the level of industry standards.This process has a short process flow,low engineering construction investment,high vanadium recovery rate,and low vanadium smelting cost,achieving good economic and technical indicators.
KeyWords AITranslate
1李昌林,周向阳,王辉,张太康,李劼,欧星,江小舵.强化氧化对石煤钙化焙烧提钒的影响[J].中南大学学报:自然科学版,2011,42(1):7-10. 被引量:20
2别舒,王兆军,李清海,张衍国.石煤提钒钠化焙烧与钙化焙烧工艺研究[J].稀有金属,2010,34(2):291-297. 被引量:40
3赵杰,张一敏,黄晶,刘涛,王非,刘娟.石煤空白焙烧-加助浸剂酸浸提钒工艺研究[J].稀有金属,2013,37(3):446-452. 被引量:26
4李存兄,魏昶,李旻廷,樊刚,邓志敢.石煤氧压酸浸提钒工艺优化[J].中国有色金属学报,2008,18(E01):84-87. 被引量:10
5王学文,刘万里,张贵清,王明玉,胡健.石煤氯化钠焙烧水浸液纳滤提钒过程[J].过程工程学报,2009,9(2):289-292. 被引量:6
6居中军,王成彦,尹飞,杨永强,李敦钫.石煤钒矿硫酸活化常压浸出提钒工艺[J].中国有色金属学报,2012,22(7):2061-2068. 被引量:17
7湖南古丈发现最大规模钒矿床 可达150万吨[J].中国有色金属,2010(16):19-19. 被引量:1
8鲍超.石煤发电烟尘沸腾钠化焙烧提钒过程的分析[J].矿冶工程,1990,10(3):40-44. 被引量:4
9白国华,李建臣,张国范,李光辉.D201树脂吸附钒(Ⅴ)的行为研究[J].矿冶工程,2010,30(5):62-65. 被引量:14
10冯其明,何东升,张国范,欧乐明,卢毅屏.石煤提钒过程中钒氧化和转化对钒浸出的影响[J].中国有色金属学报,2007,17(8):1348-1352. 被引量:85
1蔡俊,高峰,颜文斌,华骏.浓硫酸熟化浸出提取湘西石煤中的钒[J].稀有金属与硬质合金,2023,51(4):24-27.
2潘仕斌,余宗魁.谭建军:奏响“火与水之歌”[J].中国有色金属,2023(8):48-49.
3杨孟华,杨洪玉,朱晓玉,张世文,田丰.硫精矿焙烧、浸出提金试验研究[J].矿冶工程,2023,43(3):124-127.
4朱昌毕,李永连,周先超,李玉章,李雨耕.沸腾焙烧余热锅炉安全因素分析及应用[J].云南冶金,2023,52(2):184-188.
5王军.大理石粉末掺量对水泥混凝土性能的影响研究[J].四川水泥,2023(4):11-13.
6卢俊刚,吕纪烈,王维兵,陈军峰,成丽鹏,郭庆军,张浩.用双氧水治理硫酸尾气效果研究[J].山西化工,2023,43(2):187-189.
7兰红丽.以合格评定技术推动检验检测行业标准高质量发展的路径初探[J].中国质量与标准导报,2023(2):46-49.
8马浩.铁矿冶炼工艺的优化研究[J].山西冶金,2023,46(6):70-72.
9潘琪琦.肿瘤标志物SCC-Ag、Cyf21-1、CEA、NSE联合检测在肺癌诊断中的应用[J].中文科技期刊数据库(全文版)医药卫生,2023(9):0068-0071.
10高嘉雯,朱旭江,姚世霞,牛钰婷.正交实验优化甘草多糖胶囊中总多糖含量测定[J].中国民族民间医药,2023,32(16):33-35.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
In response to the problems of large differences in raw materials,long process flow,low vanadium recovery rate(mostly below 60%),and high cost in extracting vanadium from stone coal boiling roasting materials,a process route of mixing acid,curing and leaching-oxidation neutralization-ion exchange-vana-dium precipitation with ammonium salt-calcination was adopted to extract vanadium.The experimental results show that under the conditions of sulfuric acid dosage of 20% of the raw material weight,curing temperature of 100 ℃,and curing time of 6 h,the vanadium leaching rate of stone coal boiling roasting material reaches 90.2%.The final product V2O5 powder quality is stable and reliable,which reaches the level of industry standards.This process has a short process flow,low engineering construction investment,high vanadium recovery rate,and low vanadium smelting cost,achieving good economic and technical indicators.
quote
| GB/T 7714-2015 | [1] WAN Hong-qiang, ZHANG Li-fen, WANG Feng-gang, et al. Study on the Process of Extracting Vanadium Pentoxide from Stone Coal Boiling Roasting Material[J]. Rare Metals and Cemented Carbides, 2023(4): 18-23. |
| MLA | [1] WAN Hong-qiang, et al., "Study on the Process of Extracting Vanadium Pentoxide from Stone Coal Boiling Roasting Material." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 18-23. |
| APA | [1] WAN Hong-qiang, ZHANG Li-fen, WANG Feng-gang, & MA Yun-cong. (2023). Study on the Process of Extracting Vanadium Pentoxide from Stone Coal Boiling Roasting Material. Rare Metals and Cemented Carbides(4), 18-23. |
| IEEE | [1] WAN Hong-qiang, ZHANG Li-fen, WANG Feng-gang, and MA Yun-cong, "Study on the Process of Extracting Vanadium Pentoxide from Stone Coal Boiling Roasting Material," Rare Metals and Cemented Carbides, no. 4, pp. 18-23, 2023. keywords: {stone coal;boiling roasting;vanadium pentoxide;mixing acid and curing;ion exchange;vanadium precipitation with ammonium salt} |