daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Extraction of Vanadium from Stone Coal in Xiangxi by Concentrated Sulfuric Acid Curing Leaching AITranslate

Xiangxi Autonomous Prefecture Institute of Science and Technology Information;Xiangxi Autonomous Prefecture Institute of Science and Technology Information;Xiangxi Autonomous Prefecture Institute of Science and Technology Information;Xiangxi Autonomous Prefecture Institute of Science and Technology Information
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The concentrated sulfuric acid curing leaching was used in extracting vanadium from Xiangxi stone coal,the effects of sulfuric acid dosage,decarbonization temperature,curing time,curing temperature,and leaching time on leaching rate of vanadium were researched by single factor experiments and orthogonal experiments.The experiment results show that the leaching rate of vanadium is 83.2% under the conditions of decarbo-nization temperature of 600 ℃,sulfuric acid dosage of 24%,curing temperature of 180 ℃,curing time of 8 h and leaching time of 8 h.The vanadium extraction process does not produce harmful gases and reduces environmental pollution.

KeyWords AITranslate

stone coal sulfuric acid curing leaching vanadium decarbonization

1邢学永,李斯加,宁顺明.从石煤钒矿酸浸液中制取白炭黑的工艺研究[J].矿产综合利用,2014(1):65-68. 被引量:3

2王克营,李岩,蔡宁波.湘西北湖田溶地区下寒武统牛蹄塘组含钒石煤地质特征及成矿环境[J].煤炭技术,2019,38(1):72-74. 被引量:4

3亢选雄,叶国华,朱思琴,梁雪崟.从含钒页岩中提取五氧化二钒的研究进展[J].钢铁钒钛,2022,43(2):25-34. 被引量:4

4曾广军,李培佑,贾秀敏,李广,唐宝彬,向秋林.某炭质页岩型石煤钒矿焙烧浸出试验研究[J].铀矿冶,2022,41(3):232-237. 被引量:1

5郝文彬,戴子林,郭秋松,危青,李云霄.石煤直接酸浸提钒富液铵盐沉钒工艺研究[J].金属矿山,2014,43(6):75-78. 被引量:6

6戴子林,张恩普.从石煤钒矿中浸钒技术的研究现状[J].矿冶工程,2015,35(6):85-88. 被引量:17

7蒋京航,叶国华,张世民,张爽.石煤直接酸浸提钒工艺研究进展[J].矿冶,2016,25(6):35-39. 被引量:12

8赵笑益,程倩,王望泊,宁新霞,程文康,曹欢,康敏,王勇.离子交换法从低品位石煤钒矿浸出液提钒工艺研究[J].矿产保护与利用,2022,42(3):69-74. 被引量:2

9华骏,颜文斌,高峰,蔡俊.过硫酸钠氧化浸出石煤中的钒及其动力学研究[J].稀有金属与硬质合金,2019,47(1):1-5. 被引量:5

10陈放,张一敏,黄晶,刘涛,薛楠楠.二氧化锰对石煤提钒直接酸浸的影响[J].化工进展,2017,36(3):1126-1133. 被引量:12

1万洪强,张丽芬,王奉刚,马云聪.石煤沸腾焙烧料提取五氧化二钒工艺研究[J].稀有金属与硬质合金,2023,51(4):18-23.

2闫荣伟,李会泉,邢鹏,叶春林,王晨晔,朱干宇,钟立钦.熔盐电解渣磁选—焙烧—浸出提取稀土元素[J].有色金属:冶炼部分,2023(5):43-51.

3马巧焕,韩少奇,徐承焱,王培龙.基于工艺矿物学分析的黏土型锂矿提锂实验设计[J].实验室研究与探索,2023,42(6):33-37.

4高嘉雯,朱旭江,姚世霞,牛钰婷.正交实验优化甘草多糖胶囊中总多糖含量测定[J].中国民族民间医药,2023,32(16):33-35.

5梁雪崟,叶国华,朱思琴,亢选雄.钒钛磁铁矿提钒工艺的研究进展[J].稀有金属,2023,47(6):893-907.

6谢志伟,吴张永,朱启晨,蒋佳骏,梁天祥,刘振阳.植物油基Ni_(0.5)Zn_(0.5)Fe_(2)O_(4)磁流体的黏度特性及磁黏特性[J].化工进展,2023,42(7):3623-3633.

7李彦龙,徐明远,房振全,盖安俊,杨天华,李润东.污泥/菱镁尾矿/煤矸石陶粒制备工艺优化研究[J].环境工程,2023,41(S01):404-409.

8魏晓霞,赵成,李乾坤,张小伟,马东平,王妍.饮用水中高锰酸盐指数的测定方法研究[J].陇东学院学报,2023,34(5):47-51.

9闫振君,贾明印,王佳明,薛平.工艺参数对反应湿法模压成型玻璃纤维增强TPU力学性能的影响[J].塑料工业,2023,51(8):117-121.

10章聪华,颜文斌,肖佳俊,赵珂,彭商权,韦玉红.响应面法优化酒石酸还原浸出电解锰阳极渣工艺[J].无机盐工业,2023,55(9):106-113.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

The concentrated sulfuric acid curing leaching was used in extracting vanadium from Xiangxi stone coal,the effects of sulfuric acid dosage,decarbonization temperature,curing time,curing temperature,and leaching time on leaching rate of vanadium were researched by single factor experiments and orthogonal experiments.The experiment results show that the leaching rate of vanadium is 83.2% under the conditions of decarbo-nization temperature of 600 ℃,sulfuric acid dosage of 24%,curing temperature of 180 ℃,curing time of 8 h and leaching time of 8 h.The vanadium extraction process does not produce harmful gases and reduces environmental pollution.

quote

GB/T 7714-2015 [1] CAI Jun, GAO feng, YAN Wen-bin, et al. Extraction of Vanadium from Stone Coal in Xiangxi by Concentrated Sulfuric Acid Curing Leaching[J]. Rare Metals and Cemented Carbides, 2023(4): 24-27.
MLA [1] CAI Jun, et al., "Extraction of Vanadium from Stone Coal in Xiangxi by Concentrated Sulfuric Acid Curing Leaching." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 24-27.
APA [1] CAI Jun, GAO feng, YAN Wen-bin, & HUA Jun. (2023). Extraction of Vanadium from Stone Coal in Xiangxi by Concentrated Sulfuric Acid Curing Leaching. Rare Metals and Cemented Carbides(4), 24-27.
IEEE [1] CAI Jun, GAO feng, YAN Wen-bin, and HUA Jun, "Extraction of Vanadium from Stone Coal in Xiangxi by Concentrated Sulfuric Acid Curing Leaching," Rare Metals and Cemented Carbides, no. 4, pp. 24-27, 2023. keywords: {stone coal;sulfuric acid;curing leaching;vanadium;decarbonization}