Process Design of Rare Earth Metal Smelting Production Line AITranslate
Abstract AITranslate
The existing processes of rare earth metal smelting are analyzed.Molten salt electrolysis with fluoride system,calcium thermal reduction and lanthanum thermal reduction can be used to produce different rare earth products in accordance with their properties.A feasible scheme for automatic feeding and discharging in the electrolysis process is proposed.A complete set of equipment consisting of a bale breaker,automatic feeding equipment and control system is adopted in the feeding process,realizing mechanized charging,automatic feeding,and information-based statistical analysis.The vacuum siphon or manipulator could be used for the discharging process.The treatment scheme of “three wastes”,especially the waste gas,is proposed with nearly all dust being recovered,fluorine being solidified into calcium fluoride for comprehensive utilizayion,and waste gas being emitted in compliance with standards.
KeyWords AITranslate
1庞思明,颜世宏,李宗安,陈德宏,徐立海,赵斌.我国熔盐电解法制备稀土金属及其合金工艺技术进展[J].稀有金属,2011,35(3):440-450. 被引量:79
2颜世宏,李宗安,赵斌,杨广禄,庞思明,王志强.我国稀土金属产业现状及其发展前景[J].稀土,2005,26(2):81-86. 被引量:23
3张小联,胡珊玲,王科军,邓左民,彭光怀,向燕.稀土金属电解虹吸出炉技术研究[J].稀土,2007,28(5):49-51. 被引量:6
4刘玉宝,陈国华,于兵,张文灿,梁行方,陈宇昕.稀土熔盐电解过程出金属技术研究进展[J].稀土,2018,39(2):134-140. 被引量:8
1陶理科,秦赟,李辰辉,胡清钟.智能化稀土金属冶炼大数据平台的研发及应用研究[J].稀土信息,2023(4):21-25.
2刘思琦,吴刚,熊朋帆,王雁翎.基于IA平台三废控制系统CP控制器升级改造方案[J].仪器仪表用户,2023,30(10):30-34.
3许晨薇,龙胤宏,王伊珂.世界青瓷大会文旅融合经验及启示[J].合作经济与科技,2023(21):33-35.
4钱蕴文,季中远,尹志伟.涉农整合类项目绩效重点评价的难点及解决思路——以“苏州市农村一二三产业融合发展资金”为例[J].财政监督,2023(17):10-14.
5韦文贤,吴傲庭,刘正元,李洪广,李争,陈广泰.港口调车机车火灾防控系统设计与实现[J].铁道机车与动车,2023(8):21-24.
6肖珺,张琪云.走出偏见:刮痧的新媒体跨文化传播启示——兼谈中医药文化对外传播的发展路径[J].未来传播,2023,30(4):109-121.
7郭博健,魏霖静.基于数字孪生的马铃薯收获期损伤监测系统[J].软件导刊,2023,22(9):103-107.
8高师敏,吕松.一种新型连续钛及钛合金制造工艺探讨[J].中国有色冶金,2023,52(4):7-16.
9陈图南,李康,邱宗甲,韩冬,张国强.绝缘材料光声池的理论分析与实验验证[J].光谱学与光谱分析,2023,43(9):2922-2927.
10张钧,宋国智,常成.颞下经小脑幕入路显微手术治疗桥脑外侧海绵状血管瘤海绵状血管瘤的体会[J].中国临床神经外科杂志,2023,28(8):526-527.
Basic Information:
DOI:
Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]
Citation Information:
The existing processes of rare earth metal smelting are analyzed.Molten salt electrolysis with fluoride system,calcium thermal reduction and lanthanum thermal reduction can be used to produce different rare earth products in accordance with their properties.A feasible scheme for automatic feeding and discharging in the electrolysis process is proposed.A complete set of equipment consisting of a bale breaker,automatic feeding equipment and control system is adopted in the feeding process,realizing mechanized charging,automatic feeding,and information-based statistical analysis.The vacuum siphon or manipulator could be used for the discharging process.The treatment scheme of “three wastes”,especially the waste gas,is proposed with nearly all dust being recovered,fluorine being solidified into calcium fluoride for comprehensive utilizayion,and waste gas being emitted in compliance with standards.
quote
| GB/T 7714-2015 | [1] WANG Ming. Process Design of Rare Earth Metal Smelting Production Line[J]. Rare Metals and Cemented Carbides, 2023(4): 13-17. |
| MLA | [1] WANG Ming. "Process Design of Rare Earth Metal Smelting Production Line." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 13-17. |
| APA | [1] WANG Ming. (2023). Process Design of Rare Earth Metal Smelting Production Line. Rare Metals and Cemented Carbides(4), 13-17. |
| IEEE | [1] WANG Ming, "Process Design of Rare Earth Metal Smelting Production Line," Rare Metals and Cemented Carbides, no. 4, pp. 13-17, 2023. keywords: {rare earth metal;molten salt electrolysis;metallothermic reduction;automation;"three wastes"treatment;process design} |