Research on the Recycling Process of Praseodymium-Neodymium Metal Polished Waste AITranslate
Abstract AITranslate
At room temperature(5~35 ℃),rare earths,fluorine and iron in Pr-Nd metal polished waste were recovered and recycled by screening,wet magnetic separation,acidification,oxalic acid precipitation and roasting.The obtained Pr-Nd oxide and Pr-Nd fluoride exhibit high purity,and the recovery rates of rare earths,fluorine,and iron are also high.The recovery rate of rare earths exceeds 96%,fluorine 90%,and iron 93%.The waste acid produced in the process of recovering the acid insolubles and the dust and washing water produced in the process of washing sieve oversize can be recycled in the treatment of the next batch.The whole process not only realizes the secondary resource utilization,but also produces no waste residue,saving the production costs and solving the problem of waste residue in environmental protection.The recovery and treatment method of Pr-Nd metal polished waste proposed by this process is simple and easy to operate and industrialize.
KeyWords AITranslate
1肖勇,陈月华,崔小震.稀土熔盐电解废料回收工艺研究[J].世界有色金属,2016,0(3):26-28. 被引量:5
2龚傲,李子良,吴选高,田磊.稀土熔盐电解渣中铁的分布状态与磁选除铁的工艺研究[J].江西冶金,2019,39(6):21-28. 被引量:6
3徐家聪,喻小强,吴选高,龚傲,徐志峰,田磊.氟化稀土熔盐电解渣硫酸浸出脱氟研究[J].有色金属科学与工程,2020,11(6):1-9. 被引量:5
1孙志勇,林栋,张芹.中国铁尾矿资源的综合利用途径[J].自然资源情报,2023(8):1-5.
2林安川,刘晓兰.含锌钢铁固废处理工艺流程概述及发展初探[J].昆明冶金高等专科学校学报,2023,39(2):1-9.
3虎兴茂,尚文祥,张军立,马青山,杨洪亮.铝电解净化收尘灰与废焦油协同利用工艺技术研究[J].绿色矿冶,2023,39(4):31-35.
4黄波,尹小林,赵海洋,张战锋.市政污泥作为水泥窑低碳能源的工业应用研究[J].中国资源综合利用,2023,41(8):24-27.
Basic Information:
DOI:
Chinese Library Classification Number:TF805.2[冶金工程—有色金属冶金]
Citation Information:
At room temperature(5~35 ℃),rare earths,fluorine and iron in Pr-Nd metal polished waste were recovered and recycled by screening,wet magnetic separation,acidification,oxalic acid precipitation and roasting.The obtained Pr-Nd oxide and Pr-Nd fluoride exhibit high purity,and the recovery rates of rare earths,fluorine,and iron are also high.The recovery rate of rare earths exceeds 96%,fluorine 90%,and iron 93%.The waste acid produced in the process of recovering the acid insolubles and the dust and washing water produced in the process of washing sieve oversize can be recycled in the treatment of the next batch.The whole process not only realizes the secondary resource utilization,but also produces no waste residue,saving the production costs and solving the problem of waste residue in environmental protection.The recovery and treatment method of Pr-Nd metal polished waste proposed by this process is simple and easy to operate and industrialize.
quote
| GB/T 7714-2015 | [1] ZHENG Yan-ling, QIU Xiao-Ying, GE Liu-sheng, et al. Research on the Recycling Process of Praseodymium-Neodymium Metal Polished Waste[J]. Rare Metals and Cemented Carbides, 2023(4): 8-12. |
| MLA | [1] ZHENG Yan-ling, et al., "Research on the Recycling Process of Praseodymium-Neodymium Metal Polished Waste." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 8-12. |
| APA | [1] ZHENG Yan-ling, QIU Xiao-Ying, GE Liu-sheng, & XIAO Li. (2023). Research on the Recycling Process of Praseodymium-Neodymium Metal Polished Waste. Rare Metals and Cemented Carbides(4), 8-12. |
| IEEE | [1] ZHENG Yan-ling, QIU Xiao-Ying, GE Liu-sheng, and XIAO Li, "Research on the Recycling Process of Praseodymium-Neodymium Metal Polished Waste," Rare Metals and Cemented Carbides, no. 4, pp. 8-12, 2023. keywords: {Pr-Nd metal polished waste;recovery;rare earth;Pr-Nd oxide;Pr-Nd fluoride;iron bead(pow-der)} |