Effects of Co and Cr_3C_2 on the Microstructure and Properties of Cemented Carbide AITranslate
Abstract AITranslate
Three kinds of cemented carbide materials with different Co and Cr3C2 content were prepared by powder metallurgy. The crystal grain size, hardness and bending strength of the materials were measured at room temperature. Metallographic microstructure and fracture morphology of the materials were observed under SEM. The results show that with the content of binder phase Co in cemented carbide increasing, the hardness of the material decreases, but the bending strength increases. Trace Cr3 Cz in the cemented carbide can refine crystal grain,and adding trace CraC2 into high-Co-content cemented carbide is a good way to ob- tain the material with excellent comprehensive performance of high hardness and high bending strength.
KeyWords AITranslate
1周建华,孙宝琦.钴相梯度分布硬质合金的研究[J].稀有金属与硬质合金,2002,30(2):11-14. 被引量:17
2居志兰,花国然,张华.硬质合金刀具材料的研究进展[J].稀有金属与硬质合金,2011,39(2):50-53. 被引量:10
3周建华.国内外新型复合硬质合金材料的发展动态[J].超硬材料工程,2009,21(2):33-39. 被引量:1
4陶国林,蒋显全,黄靖.硬质合金刀具材料发展现状与趋势[J].金属功能材料,2011,18(3):79-83. 被引量:34
5李力,栾道成,胡涛,张崇才.硬质合金刀具新技术研究进展[J].中国钨业,2010,25(1):45-49. 被引量:12
6Michael Sommerl. On the formation of very large WC crystals during sintering of ultrafine WC-Co alloys[J]. International Journal of Refractory Metals& Hard Ma- terials, 2002,20 : 41-55.
7杨世莹,贺子凯,黄鑫.添加剂对硬质合金性能的影响[J].粉末冶金工业,2005,15(6):22-25. 被引量:9
8ChoiK,Hwang N M,Kim D Y. Effect of VC addition on microstuetural evolution of WC-Co alloy:mechanism of grain growth inhibition [ J ]. Powder Metallurgy, 2000,43(2) :168-171.
1程剑兵,庞思勤,王西彬,张好强,曹瑞军.超细晶硬质合金刀具Co含量对其耐磨损性的影响[J].稀有金属与硬质合金,2015,43(3):57-62. 被引量:2
2秦琴,姜锦钦,吴宇莲,蹇松阳,王楠,李三雁,王正云.Co含量对超细YG类硬质合金结构及性能的影响[J].稀有金属与硬质合金,2021,49(3):75-79. 被引量:1
3陈振磊,喻琛,邵鸣宇.不同粘结相硬质合金的研究进展[J].机械研究与应用,2021,34(5):204-209. 被引量:2
4刘萍,瞿峻,温光华,陈响明,王社权.表层钴含量对基体/涂层界面组织结构和刀具切削性能的影响[J].硬质合金,2019,36(2):116-125. 被引量:4
1李之旭,范洪远,鲜广,赵海波,熊计.硬质合金基体对TiAlN/TiAlSiCrN/TiSiN多层涂层结构和机械性能的影响[J].硬质合金,2020,37(2):119-126. 被引量:1
2秦琴,姜锦钦,吴宇莲,蹇松阳,王楠,李三雁,王正云.Co含量对超细YG类硬质合金结构及性能的影响[J].稀有金属与硬质合金,2021,49(3):75-79. 被引量:1
3于洲,郑光明,程祥,刘焕宝,杨先海.高速铣削高温合金涂层刀具表面自组织结构研究[J].机床与液压,2021,49(20):32-35.
4谭君国,李季飞,叶谱生,张腾飞,王启民.高温渗碳对硬质合金涂层刀具高温力学性能及干式切削性能的影响[J].表面技术,2022,51(3):271-277. 被引量:1
5曹瑞军,李开深,李腾飞,何盛亚.金刚石含量对金刚石强化硬质合金耐磨性影响[J].硬质合金,2022,39(3):165-171. 被引量:1
6张云龙,牛楚涵,牛广津,张宇民,李启荣,高志杨,张唯一.La_(2)O_(3)掺杂量对WC-12Co硬质合金微观结构和硬度的影响[J].中国钨业,2022,37(2):53-59.
7李祥,郑光明,盖少磊,颜培,杨先海.PVD-AlTiN涂层刀具高速干铣削高温合金的磨损机理研究[J].工具技术,2023,57(1):25-29. 被引量:1
8胡启明,廖宇.贫碳WC-12%(Co+Ni)硬质合金微观组织与性能[J].硬质合金,2023,40(1):66-72.
9刘萍,瞿峻,温光华,陈响明,王社权.表层钴含量对基体/涂层界面组织结构和刀具切削性能的影响[J].硬质合金,2019,36(2):116-125. 被引量:4
1王洪福,芦琪,曾志强,王华昌.等离子喷焊方法与热锻模Ni60-Cr_3C_2覆层的制备[J].热加工工艺,2014,43(10):145-147. 被引量:2
2刘海雄,唐利平.Cr_3C_2对汽车模具埋弧堆焊修复层组织与性能的影响[J].热加工工艺,2016,45(5):227-229.
3陈健,弓满锋,刘伟,曾俊杰,伍尚华.添加TiC和Cr_3C_2对超细WC-8Co硬质合金微观结构和性能的影响[J].人工晶体学报,2015,44(5):1336-1341. 被引量:13
4余畅,朱宇,简险峰,刘瑞霞,赵会友.WC+Cr_3C_2增强铁基合金激光熔覆涂层磨损性能[J].金属热处理,2013,38(12):21-24. 被引量:6
5韩欣,王明智,梁宝岩.Sn做助剂机械合金化+热处理制备Ti_3AlC_2[J].稀有金属材料与工程,2010,39(A01):204-207. 被引量:4
6汪金文,刘宁,徐伟,胡巍巍,童延俊.Cr_3C_2对纳米Ti(C,N)基金属陶瓷组织和性能的影响[J].热处理,2011,26(2):14-19.
7郑金辉.Ti_3AlC_2增强铜基复合材料的摩擦磨损特性分析[J].兵器材料科学与工程,2016,39(2):103-105. 被引量:1
8王明智,梁宝岩,韩欣.机械诱发自蔓延反应合成Ti_3AlC_2的机理研究[J].燕山大学学报,2009,33(1):1-3. 被引量:7
9超音速火焰喷涂在电力系统中的应用研究[J].内蒙古电力技术,2008,26(4):15-15.
10李丽娅,易健宏,李爱坤,彭元东,夏庆林.Cr_3C_2含量和快淬速度对SmCo_(7-x)(Cr_3C_2)_x合金非晶化行为的影响(英文)[J].中国有色金属学报:英文版,2012,22(5):1118-1122.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Three kinds of cemented carbide materials with different Co and Cr3C2 content were prepared by powder metallurgy. The crystal grain size, hardness and bending strength of the materials were measured at room temperature. Metallographic microstructure and fracture morphology of the materials were observed under SEM. The results show that with the content of binder phase Co in cemented carbide increasing, the hardness of the material decreases, but the bending strength increases. Trace Cr3 Cz in the cemented carbide can refine crystal grain,and adding trace CraC2 into high-Co-content cemented carbide is a good way to ob- tain the material with excellent comprehensive performance of high hardness and high bending strength.
quote
| GB/T 7714-2015 | [1] YANG Xiao-fan, LI You-sheng, LI Ling-xiang, et al. Effects of Co and Cr_3C_2 on the Microstructure and Properties of Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2012(3): 54-57. |
| MLA | [1] YANG Xiao-fan, et al., "Effects of Co and Cr_3C_2 on the Microstructure and Properties of Cemented Carbide." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 54-57. |
| APA | [1] YANG Xiao-fan, LI You-sheng, LI Ling-xiang, LI Chao, & XU Zhi-long. (2012). Effects of Co and Cr_3C_2 on the Microstructure and Properties of Cemented Carbide. Rare Metals and Cemented Carbides(3), 54-57. |
| IEEE | [1] YANG Xiao-fan, LI You-sheng, LI Ling-xiang, LI Chao, and XU Zhi-long, "Effects of Co and Cr_3C_2 on the Microstructure and Properties of Cemented Carbide," Rare Metals and Cemented Carbides, no. 3, pp. 54-57, 2012. keywords: {cemented carbide;Co;Cra C2;crystal grain size;hardness;bending strength} |