Preparation of Sub-micron Cemented Carbide by Hot-press Sintering of Ultrafine WC-Co Composite Powder AITranslate
Abstract AITranslate
Hot-press sintering process for cemented carbide preparation was investigated with ultrafine WC- Co composite powder prepared by in-situ reduction as the raw material. And the physical and mechanical properties of the samples were also analyzed. The results show that after ultrafine WC-Co composite pow ders with average particle size of about 300 nm,are sintered in hot-pressing furnace at 1 370℃ for 1.5 h, sub-micron WC-Co cemented carbide is obtained with average grain size of 600 nm,relative density of 99% and excellent comprehensive mechanical properties.
KeyWords AITranslate
1Mi S,Courtney T H. Synthesis of WC and WC-Co cer mets by mechanical alloying and subsequent hot isostatic pressing[J]. Scripta Materialia, 1998,38 (1) : 171-176.
2Berger S,Porat R, Rosen R. Nanocrystalline materials:a study of WC-based hard metals[J]. Progress in Materi- als Science,1997,42(1-4) :311-320.
3吴其山.超细WC-Co硬质合金研究综述[J].中国钨业,2005,20(6):35-40. 被引量:19
4Mc Candlish L E,Kear B H. Processing and properties of nanostructured WC- Co [ J ]. Nanostructured Materials, 1992,1 (2) : 119-124.
5Seegopaul P, McCandlish L E, Shinneman F M. Produc- tion capability and powder processing methods for nano- structured WC-Co powder[J]. International Journal of Refractory Metals and Hard Materials, 1997,15 ( 1 - 3 ) : 133-138.
6Ma X M, Gang J I. Nanostructured WC-Co alloy pre- pared by mechanical alloying[J]. Journal of Alloys and Compounds, 1996,245 : L30-42.
7Gao L,Kear B H. Synthesis of nanophase WC powder by a displacement reaction process[-J]. Nanostructured Materials, 1997,9 : 205-208.
8Spriggs G E. A history of fine grained hardmetal[J]. In- ternational Journal of Refractory Metals and Hard Mate- rials, 1995,13 : 241-255.
9Arato P, Bartha L, Porat R, et al. Solid or liquid phase sintering of nanocrystalline WC/Co hardmetals [J]. Nanostructured Materials, 1998,10:245-255.
10张启礼,孔立峰,高引慧.纳米WC-10Co硬质合金粉末的低压烧结[J].材料研究与应用,2007,1(1):31-33. 被引量:4
1羊求民,羊建高,苏伟,陈丽勇,陈颢,郭圣达.纳米/超细晶WC-Co类硬质合金的研究进展[J].稀有金属与硬质合金,2018,46(1):76-83. 被引量:18
1羊求民,唐彦渊,赖星任,张龙辉,邓登飞,李倩.Mo含量对烧结WC-CoCrCuFeNiMo_x硬质合金性能的影响[J].材料热处理学报,2018,39(11):46-51. 被引量:2
2刘觐,易志强,张琳,黄红华,谭敦强,陆磊.化学沉淀法制备超细仲钨酸铵粉末的研究[J].江西科学,2019,37(3):405-408. 被引量:2
3吴杰,王忠华,吕健.HVOF喷涂超细结构WC-12Co涂层磨粒磨损性能[J].稀有金属与硬质合金,2019,47(4):24-29.
4常龙飞,王伟,茹红强.球磨工艺对制备超细WC粉末的影响[J].材料与冶金学报,2019,18(3):207-212.
5祁志旭,陈兴媚.硬质合金刀具研究进展[J].材料研究与应用,2019,13(4):347-354. 被引量:7
6潘锋,刘家义,杜占,朱庆山.超细碳化钨制备过程及机理研究进展[J].化工学报,2021,72(11):5455-5467. 被引量:4
7全温灿,艾志龙,吴彤,史冠勇,豆志河.自蔓延高温合成制备碳化钨粉的热力学研究[J].江西冶金,2022,42(2):13-17.
8杨诚辉,徐国钻,刘如铁,张龙辉,羊求民.不同氧化钨还原制备钨粉及其特性研究[J].稀有金属与硬质合金,2022,50(2):19-25. 被引量:1
9梁闯,王朝安,张志平,曲鹏.四氧化三钴碳含量对超细钴粉品质的影响[J].稀有金属与硬质合金,2022,50(2):79-84. 被引量:1
10罗鑫,洪源昆,吴佳逸,李绍轩,羊求民.超细硬质合金WC晶粒大小对其摩擦磨损性能的影响[J].稀有金属与硬质合金,2022,50(3):93-97.
1娄静,易健宏,鲍瑞,彭元东,张浩泽.碳含量对微波烧结亚微米硬质合金组织与性能的影响[J].中国钨业,2011,26(1):30-33. 被引量:4
2王玉香,文小强,周健.化学沉淀法制备超细WC-Co复合粉的研究[J].中国钨业,2012,27(6):24-27. 被引量:2
3王海滨,宋晓艳,刘雪梅,付军,魏崇斌,高杨.WC-Co复合粉的喷雾造粒及松装密度的影响因素[J].中国有色金属学报,2012,22(11):3241-3248. 被引量:5
4任秋凤,林忠杰.热等静压硬质合金的性能[J].硬质合金,1998,15(2):86-90. 被引量:2
5孙德玉.ZRY-100-20真空热压炉[J].工业加热,1995,24(4):20-22.
6刘雪梅,王海滨,宋晓艳,王西龙,李玉玺.VC添加量对纳米晶硬质合金的制备及性能影响[J].稀有金属材料与工程,2016,45(2):477-481. 被引量:10
7王西龙,宋晓艳,张哲旭,刘雪梅,刘兴伟,杨诚,李玉玺.以石墨烯为碳源的硬质合金制备与性能[J].稀有金属材料与工程,2016,45(12):3262-3266.
8B.H.格鲁什科夫,唐丹,李沐山.双峰结构的WC—Co硬质合金[J].国外难熔金属与硬质材料,1999,15(2):18-20. 被引量:1
9黄树涛,于骏一,姚英学,袁哲俊.金刚石薄膜与W、WC-6%Co基体间的界面结构研究[J].中国机械工程,2000,11(12):1398-1400. 被引量:2
10朱二涛,羊建高,邓军旺,郭圣达,谭兴龙,戴煜,张翔.不同钨源原料制备WC-Co复合粉的形貌研究[J].有色金属科学与工程,2014,5(6):38-46. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
Hot-press sintering process for cemented carbide preparation was investigated with ultrafine WC- Co composite powder prepared by in-situ reduction as the raw material. And the physical and mechanical properties of the samples were also analyzed. The results show that after ultrafine WC-Co composite pow ders with average particle size of about 300 nm,are sintered in hot-pressing furnace at 1 370℃ for 1.5 h, sub-micron WC-Co cemented carbide is obtained with average grain size of 600 nm,relative density of 99% and excellent comprehensive mechanical properties.
quote
| GB/T 7714-2015 | [1] ZHU Qi-kou, LIU Wen-bin, WANG Tie-jun, et al. Preparation of Sub-micron Cemented Carbide by Hot-press Sintering of Ultrafine WC-Co Composite Powder[J]. Rare Metals and Cemented Carbides, 2012(3): 58-62. |
| MLA | [1] ZHU Qi-kou, et al., "Preparation of Sub-micron Cemented Carbide by Hot-press Sintering of Ultrafine WC-Co Composite Powder." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 58-62. |
| APA | [1] ZHU Qi-kou, LIU Wen-bin, WANG Tie-jun, & SONG Xiao-yan. (2012). Preparation of Sub-micron Cemented Carbide by Hot-press Sintering of Ultrafine WC-Co Composite Powder. Rare Metals and Cemented Carbides(3), 58-62. |
| IEEE | [1] ZHU Qi-kou, LIU Wen-bin, WANG Tie-jun, and SONG Xiao-yan, "Preparation of Sub-micron Cemented Carbide by Hot-press Sintering of Ultrafine WC-Co Composite Powder," Rare Metals and Cemented Carbides, no. 3, pp. 58-62, 2012. keywords: {ultrafine WC-Co composite powder;hot-press sintering;sub-micron cemented carbide;mechanical property} |