The Latest Development of LiNil/3Co1/3Mnl/3O_2 Cathode Material for Lithium-ion Batteries AITranslate

School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest achievements and progress of LiNi1/3 their synthesis technology and doping and surface modific cific capacity,excellent cycle performance and lower cost. Col/3 Mnl/3 02 cathode materials are reviewed in ation,and these cathode materials have high spe- Their development trends are also forecasted.

KeyWords AITranslate

lithium-ion battery cathode material LiNil/3 Co1/3 Mnl/3O2 preparation method doping modifica-tion surface modification

1Ohzuku T, Makimura Y. Layered lithium insertion mate- rial of LiNi1/3Co1/3 Mn1/3 O2 for lithium-ion batteries [J]. Chem Lett, 2001, (7): 642-643.

2Ren H B,Wang Y R, Li D C,et a l. Characterizations on the structural and electrochemical properties of LiNi1/3 Mn1/3Co1/3O2 prepared by a wet-chemical process [J]. 2008,178(39-40) :1 969-1 974.

3胡传跃,郭军,杜勇,徐洪辉,贺跃辉.合成条件对氢氧化物共沉淀法制备锂离子电池层状正极材料Li[Ni_(1/3)Co_(1/3)Mn_(1/3)]O_2的影响(英文)[J].中国有色金属学报:英文版,2011,21(1):114-120. 被引量:6

4Deng C,Zhang S,Ma L,et al. Effects of precipitator on the morphological, structural and electrochemical charac- teristics of Li[Nil/3 Co1/3 Mn1/3 ] O2 prepared via carbon- ate eoprecipitation [J ]. Journal of Alloys and Com- pounds,2011, 509(4):1 322-1 327.

5Wen Jian-Wu, Zhang Da-Wei, Teng Yuan-Cheng, et al. One-step synthesis and improved electrochemical per- formance of Li(Ni1/3 Co1/3 Mn1/3 ) Oz by a modified radia- ted polymer gel method[J]. Electrochimica Acta, 2010, 55(7) :2 306-2 310.

6Seo H J,Yun C K. The characteristics of Ni-Co-Mn-O precursor and LiNi1/3 CO1/3 Mn1/3O2 cathode powders pre- pared by spray pyrolysis[J]. Ceram Int, 2009,35 : 1 205- 1 210.

7Xie Junlan, Huang Xiang, Zhu Zhibin, et al. Hydrother- mal synthesis of Li(Ni1/3 Co1/3 Mnl/3 ) O2 for lithium re- chargeable batteries[J]. Ceramics International, 2010,36 (8):2 485-2 487.

8Cheng Cuixia, Tan Long, H u Anzheng, et al. Synthesis of LiNi0.65Co0.25 Mn0.1 O2 as cathode material for lithium- ion batteries by rheological phase method [J]. Journal of Alloys and Compounds,2010,506(2):888-891.

9Abdelfattah Mahmoud, Ismael Saadoune, Jose Manuel Amarilla,et al. On the LiCo2/3 Ni1/6 Mn1/6 O2 positive e- lectrode material [J]. Electrochimica Acta, 2011, 56 (11):4 081-4 086.

10夏小勇,魏进平,叶茂,阎杰,卞锡奎.电解法制备锂离子电池正极材料LiCo_xNi_(1-x)O_2[J].应用化学,2003,20(10):928-931. 被引量:12

1禹筱元,余仕僖,周正添.锂离子电池LiNi_(1/3)Co_(1/3_Mn_(1/3)O_2正极材料的性能研究(Ⅰ)[J].广东化工,2008,35(4):26-29. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]

Citation Information:

The latest achievements and progress of LiNi1/3 their synthesis technology and doping and surface modific cific capacity,excellent cycle performance and lower cost. Col/3 Mnl/3 02 cathode materials are reviewed in ation,and these cathode materials have high spe- Their development trends are also forecasted.

quote

GB/T 7714-2015 [1] GUO Qing-shan, LIU Guo-qiang, TIAN Yan-wen, et al. The Latest Development of LiNil/3Co1/3Mnl/3O_2 Cathode Material for Lithium-ion Batteries[J]. Rare Metals and Cemented Carbides, 2012(3): 50-53.
MLA [1] GUO Qing-shan, et al., "The Latest Development of LiNil/3Co1/3Mnl/3O_2 Cathode Material for Lithium-ion Batteries." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 50-53.
APA [1] GUO Qing-shan, LIU Guo-qiang, TIAN Yan-wen, & WANG Qiang. (2012). The Latest Development of LiNil/3Co1/3Mnl/3O_2 Cathode Material for Lithium-ion Batteries. Rare Metals and Cemented Carbides(3), 50-53.
IEEE [1] GUO Qing-shan, LIU Guo-qiang, TIAN Yan-wen, and WANG Qiang, "The Latest Development of LiNil/3Co1/3Mnl/3O_2 Cathode Material for Lithium-ion Batteries," Rare Metals and Cemented Carbides, no. 3, pp. 50-53, 2012. keywords: {lithium-ion battery;cathode material;LiNil/3 Co1/3 Mnl/3O2;preparation method;doping modifica-tion;surface modification}