Temperature Field Simulation of Magnetic Abrasive Hot Pressing Process AITranslate

School of Mechanical Engineering, Taiyuan University of Technology;School of Mechanical Engineering, Taiyuan University of Technology;School of Mechanical Engineering, Taiyuan University of Technology;School of Mechanical Engineering, Taiyuan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on two-phase composite magnetic abrasive prepared from Fe powder and A12 03 powder, heat transfer model of its hot pressing process is built. Mould temperature field is analyzed by computer simulation,and then the hot pressing process is optimized. Simulation results show that furnace heating rate have a great effect on mould temperature field,and temperature field distribution of the abrasive in dif- ferent mould location is also different. In view of abrasive preparation efficiency and laboratory equipment requirements,the heating rate is determined to be 10~15 ~C/min at low temperature and 5~10 ~C/min at high temperature. And abrasive should be placed in z5 region of the mould,in order to reduce its axial tem- perature difference in the hot pressing forming process and improve its physical and mechanical properties.

KeyWords AITranslate

magnetic abrasive hot pressing sintering temperature field distribution computer simulation

1曾令可,张功元.陶瓷坯体烧成过程中温度场的三维有限元分析[J].材料研究学报,1994,8(3):245-252. 被引量:10

2许崇海,黄传真,邓建新,艾兴.多相复合陶瓷刀具材料热压过程的计算机模拟与工艺设计Ⅰ——温度场模拟与工艺设计[J].应用基础与工程科学学报,2000,8(1):44-51. 被引量:5

3素木洋一.硅酸盐手册[M].北京:轻工业出版社,1980.

4Kingery W D. The thermal conductivily of ceramic die- lectrics[J]. Progress in Ceramic Science, 1962,2: 181-186.

5周健.钼粉末温压成型过程的有限元数值模拟研究[D].西安:西北工业大学,2007.

1张龙,张晓敏,褚钟祥,彭松.粉末烧结的计算机模拟方法研究进展[J].重庆大学学报:自然科学版,2016,39(5):39-48. 被引量:1

2郭建伟,宋金鹏,高姣姣,吕明.热压烧结炉制备陶瓷刀具材料过程的温度场模拟[J].热加工工艺,2020,49(24):26-30.

1谢悦,宿晓如,冯春冬,罗冬梅.颗粒增强橡胶复合材料有效力学性能预测分析[J].兵器装备工程学报,2017,38(7):142-147. 被引量:4

1王军委,郑涛,陈红玲.磁性磨粒的热压烧结工艺参数研究[J].稀有金属与硬质合金,2012,40(5):66-69. 被引量:1

2孙健.420mm×1100mm板坯连铸结晶器吹氩对流场和温度场影响的数值模拟[J].特殊钢,2015,36(2):5-8. 被引量:2

3刘鲁宁,兰岳光,牛永红,彭继华,包云鹏.中间包控流装置对温度场影响的数值模拟研究[J].内蒙古科技大学学报,2009,28(3):209-212. 被引量:4

4季乐乐,贺东风.煤气成分和流量对钢包烘烤温度场影响的数值模拟[J].冶金能源,2014,33(3):12-16. 被引量:1

5李志希,范景莲,缪群.WC-10Co硬质合金热压工艺与晶粒抑制剂的研究[J].粉末冶金工业,2005,15(1):7-11. 被引量:2

6马新生,耿茂鹏,尧军平,饶磊,杨小军.电渣熔铸中渣池深度对渣池温度场影响的模拟研究[J].铸造技术,2005,26(12):1112-1115.

7武安华,曹文斌,李江涛,葛昌纯.热压工艺对SiC陶瓷结构及性能的影响[J].粉末冶金技术,2001,19(6):327-330. 被引量:5

8任忠.热压烧结金刚石制品工艺的特点及其优越性[J].超硬材料与工程,1995(1):20-21.

9胡坤太,仇圣桃,张慧,张兴中,干勇.连铸坯凝固晶粒组织的模拟[J].钢铁,2004(z1):542-545. 被引量:1

10兰岳光,邹宗树,王晓鸣.结晶器角部气隙厚度对方坯温度场影响的数值模拟[J].过程工程学报,2003,3(6):518-522. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF124.5[冶金工程—粉末冶金]

Citation Information:

Based on two-phase composite magnetic abrasive prepared from Fe powder and A12 03 powder, heat transfer model of its hot pressing process is built. Mould temperature field is analyzed by computer simulation,and then the hot pressing process is optimized. Simulation results show that furnace heating rate have a great effect on mould temperature field,and temperature field distribution of the abrasive in dif- ferent mould location is also different. In view of abrasive preparation efficiency and laboratory equipment requirements,the heating rate is determined to be 10~15 ~C/min at low temperature and 5~10 ~C/min at high temperature. And abrasive should be placed in z5 region of the mould,in order to reduce its axial tem- perature difference in the hot pressing forming process and improve its physical and mechanical properties.

quote

GB/T 7714-2015 [1] ZHENG Tao, WANG Jun-wei, CHEN Hong-ling, et al. Temperature Field Simulation of Magnetic Abrasive Hot Pressing Process[J]. Rare Metals and Cemented Carbides, 2012(3): 47-49.
MLA [1] ZHENG Tao, et al., "Temperature Field Simulation of Magnetic Abrasive Hot Pressing Process." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 47-49.
APA [1] ZHENG Tao, WANG Jun-wei, CHEN Hong-ling, & LI Wen-hui. (2012). Temperature Field Simulation of Magnetic Abrasive Hot Pressing Process. Rare Metals and Cemented Carbides(3), 47-49.
IEEE [1] ZHENG Tao, WANG Jun-wei, CHEN Hong-ling, and LI Wen-hui, "Temperature Field Simulation of Magnetic Abrasive Hot Pressing Process," Rare Metals and Cemented Carbides, no. 3, pp. 47-49, 2012. keywords: {magnetic abrasive;hot pressing sintering;temperature field distribution;computer simulation}