Impact of La on Inclusions and Corrosion Resistance of Pure Steel AITranslate

School of Materials Science and Metallurgical Engineering, Inner Mongolia University of Science and Technology;School of Materials Science and Metallurgical Engineering, Inner Mongolia University of Science and Technology;School of Materials Science and Metallurgical Engineering, Inner Mongolia University of Science and Technology;School of Materials Science and Metallurgical Engineering, Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the impact of La on the corrosion resistance of pure steel through the observation of the morphology of RE inclusion in the pure steel, testing of electro-chemic corrosion EIS and polarization curve. The test results showed that addition of La into the pure steel can modify the inclusion and improve the morphology of the inclusion thus to improve the corrosion resistance of the pure steel.

KeyWords AITranslate

La pure steel RE inclusion corrosion

1张蕙文,毛裕文,孙明华,余宗森.稀土对钢耐大气腐蚀性能的影响[J].北京科技大学学报,1994,16(5):491-495. 被引量:26

2林勤,陈帮文,郭锋,郭英,孙学义,张志平.稀土改善09CuPTiRE耐候钢耐蚀性的作用机理[J].稀土,2003,24(5):26-28. 被引量:29

3江志强,夏向东,李建国,张力.稀土硅铁对16MnR钢在内蒙古天然碱苛化烧碱中腐蚀性能的影响[J].兵器材料科学与工程,2000(6):28-32. 被引量:5

4郭锋,林勤,张志平,陈冬火,高平祥,王跃华.稀土对碳锰钢耐蚀性能的影响[J].稀土,2003,24(5):29-32. 被引量:9

5蔡开科,张立峰,刘中柱.纯净钢生产技术及现状[J].河南冶金,2003,11(4):3-8. 被引量:16

6张学元,余刚,王凤平,杜元龙.Cl^-对API P105钢在含CO_2溶液中的电化学腐蚀行为的影响[J].高等学校化学学报,1999,20(7):1115-1118. 被引量:30

7岳丽杰,王龙妹,徐成海,朴秀玉.Cu-P耐候钢中稀土对夹杂物和耐蚀性的影响[J].东北大学学报:自然科学版,2004,25(12):1179-1182. 被引量:14

8江志强,夏向东,李建国,王来生.含稀土20钢焊接接头耐腐蚀性能的电化学研究[J].兵器材料科学与工程,1999,22(4):45-49. 被引量:3

1赵文广,诸帅豪.氧化钇对碳锰钢耐蚀性能的影响[J].稀土,2011,32(5):66-71. 被引量:1

2王迹,姜自莲,尚桂凡.LPC稀土改性ZG25CrNiMo后耐H_2S均匀腐蚀性能[J].腐蚀与防护,2013,34(5):426-429.

3亢业峰,查凯.冷却方式与稀土元素对低碳高铌钢组织与性能的影响[J].山东工业技术,2015(12):9-10.

4靳星.锆脱氧对船板EH36夹杂物和耐蚀性能的影响[J].连铸,2022,47(2):83-88. 被引量:2

1黄艺辉,陈守潇,林锦池,王艳良,赵德森.超细氧化钇材料的制备及其在包覆LiCoO_(2)材料中的应用[J].福建冶金,2022,51(3):32-35.

2房孟婷,袁华志,谢鑫,曾建华,仲红刚,翟启杰.重轨钢铸坯中MnS夹杂物的析出与长大[J].钢铁,2023,58(5):59-69. 被引量:1

3杨文魁,宋景凌,周旋,朱庆桂,李恒华,刘合萍,杨健.铝脱氧25Mn钢圆坯中夹杂物的分布规律[J].炼钢,2023,39(4):70-81.

1陈菁,纪胜如,陈惠敏,周小平,胡心彬,王永云,吴清泉,钟毅,赵昌旭.提高炉用ZGOCr23Ni13钢构件使用寿命的研究[J].热加工工艺,1997,26(3):41-43. 被引量:1

2秦紫瑞,赵军,钟蕊,尹大伟.改善电磁吸盘用钢的组织及性能的研究[J].铸造,1994,43(5):18-24.

3丁庆丰,陈颜堂,陈晓.含Zr低合金高强度钢中夹杂物的特性[J].钢铁研究,2004,32(3):34-37. 被引量:1

4肖峰,左素彦.稀土对钢中非金属夹杂物的影响[J].江西冶金,1998,18(5):1-3. 被引量:6

5贺俊光,文九巴,李旭东,郝庆国.Al-Zn-Sn-Ga阳极腐蚀过程的电化学阻抗谱[J].中国有色金属学报,2012,22(1):187-193. 被引量:25

6刘建平,李正奉,周晓湘.一种咪唑啉缓蚀剂在碳钢表面成膜的电化学研究[J].腐蚀科学与防护技术,2003,15(5):263-265. 被引量:19

7薛玉娜,任国琪,王荣.温度对J55钢铬铝合金化后电化学阻抗谱的影响[J].材料保护,2013,46(11):70-72. 被引量:2

8何岳,向嵩,石维,刘建敏,梁宇,陈朝轶.冷拔珠光体钢的组织演变对其点蚀行为的影响[J].金属学报,2016,52(12):1536-1544. 被引量:2

9杨昌柱,张敬东.碳钢在弱碱性钝化体系中的EIS谱研究[J].材料保护,1999,32(9):31-32. 被引量:2

10马景灵,文九巴,卢现稳,李元侦.铝合金阳极腐蚀过程的电化学阻抗谱研究[J].腐蚀与防护,2009,30(6):373-376. 被引量:17

Basic Information:

DOI:

Chinese Library Classification Number:TG142.13[金属学及工艺—金属材料]

Citation Information:

Study is made of the impact of La on the corrosion resistance of pure steel through the observation of the morphology of RE inclusion in the pure steel, testing of electro-chemic corrosion EIS and polarization curve. The test results showed that addition of La into the pure steel can modify the inclusion and improve the morphology of the inclusion thus to improve the corrosion resistance of the pure steel.

quote

GB/T 7714-2015 [1] JIANG Xue-zhi, WANG Bao-feng, LI Chun-long, et al. Impact of La on Inclusions and Corrosion Resistance of Pure Steel[J]. Rare Metals and Cemented Carbides, 2005(4): 28-31.
MLA [1] JIANG Xue-zhi, et al., "Impact of La on Inclusions and Corrosion Resistance of Pure Steel." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 28-31.
APA [1] JIANG Xue-zhi, WANG Bao-feng, LI Chun-long, & WANG Quan. (2005). Impact of La on Inclusions and Corrosion Resistance of Pure Steel. Rare Metals and Cemented Carbides(4), 28-31.
IEEE [1] JIANG Xue-zhi, WANG Bao-feng, LI Chun-long, and WANG Quan, "Impact of La on Inclusions and Corrosion Resistance of Pure Steel," Rare Metals and Cemented Carbides, no. 4, pp. 28-31, 2005. keywords: {La;pure steel;RE inclusion;corrosion}