Application of Mathematic Method in the Spectrophotometric Analysis of Tungsten AITranslate

China Nonferrous Engineering Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Systematic description is made of the application of mathematic method in the spectrophotometric analysis of tungsten. And brief introduction is made to the testing principle, method and applicable range.

KeyWords AITranslate

tungsten spectrophotometric analysis mathematic method application

1沈立心,王东进,张汉辉,李琳,陈珠灵.偏最小二乘法同时分光光度测定W、Mo、Zr的研究[J].福州大学学报:自然科学版,1997,25(4):104-107. 被引量:2

2金继红,陈家玮,张永文.小波变换-偏最小二乘法用于钨、钼、钛的分光光度法同时测定[J].分析化学,2000,28(6):791-791. 被引量:16

3倪永年,陈晓东.主成份分析——分光光度法同时测定钨、钼、锡、钛四组份体系[J].分析化学,1990,18(7):618-622. 被引量:22

4陈同森,陈展光,何波,李志良.卡尔曼滤波分光光度法同时测定钛锡钼钨[J].中国有色金属学报,1997,7(1):52-55. 被引量:5

5沈洪达,王耀光,陈玉绶.平方根卡尔曼滤波分光光度法同时测定钼、钨和锡[J].冶金分析,1996,16(1):24-27. 被引量:7

6郑基甸,张在整,卓继伟.双络合体系K系数分光光度法同时测定钼(Ⅵ)与钨(Ⅵ)[J].福州大学学报:自然科学版,1990,18(4):99-103. 被引量:1

1段群章.铀的分光光度分析新进展[J].铀矿冶,1991,10(3):59-63. 被引量:2

2黄薇.锆的分光光度分析[J].枣庄师专学报,1991,8(4):57-60.

3刘先国,马聆音,王长庚.偏最小二乘法用于多组分的分光光度分析——钙锶钡的同时测定[J].岩矿测试,1992,11(4):293-298. 被引量:4

4段群章.铽的分光光度分析[J].铀矿冶,1995,14(2):118-123. 被引量:1

5苑海涛.分光光度分析测定钒的方法与应用进展[J].化工管理,2015(15):87-87. 被引量:1

6段群章.锂的分光光度和荧光分析新进展[J].铀矿冶,1993,12(4):256-259. 被引量:2

7姚泰煜.校正发射光谱分析干扰效应的数学方法[J].计算机与应用化学,1991,8(1):79-79. 被引量:1

8林彬.本尼地试剂区别醛酮的适用范围[J].实验室研究与探索,1991(3):95-96.

9庄长福,孙园园,王运方,石建慧,师宇华,师同顺.5-(4-烟酸酰亚胺基)苯基-10,15,20-三苯基卟啉及其锌配合物的合成及性质研究[J].化学学报,2010,68(22):2319-2324. 被引量:5

10张志红,黄毅.银杏叶提取物中黄酮类化合物的分光光度分析研究[J].分析试验室,2005,24(6):17-19. 被引量:17

Basic Information:

DOI:

Chinese Library Classification Number:O657.3[理学—分析化学]

Citation Information:

Systematic description is made of the application of mathematic method in the spectrophotometric analysis of tungsten. And brief introduction is made to the testing principle, method and applicable range.

quote

GB/T 7714-2015 [1] LI Bo. Application of Mathematic Method in the Spectrophotometric Analysis of Tungsten[J]. Rare Metals and Cemented Carbides, 2005(4): 32-34.
MLA [1] LI Bo. "Application of Mathematic Method in the Spectrophotometric Analysis of Tungsten." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 32-34.
APA [1] LI Bo. (2005). Application of Mathematic Method in the Spectrophotometric Analysis of Tungsten. Rare Metals and Cemented Carbides(4), 32-34.
IEEE [1] LI Bo, "Application of Mathematic Method in the Spectrophotometric Analysis of Tungsten," Rare Metals and Cemented Carbides, no. 4, pp. 32-34, 2005. keywords: {tungsten;spectrophotometric analysis;mathematic method;application}