Determination of Phosphor in Ta Powder through Induction Coupling Plasma Mass Spectrometer AITranslate
Abstract AITranslate
Description is made of the determination of trace impurity phosphor in Ta powder through ICP-MS. Based on the investigation into the testing condition, hydrofluoric acid-resistant inert feed system, shielded torch and cold plasma technology,phosphor concentration in Ta powder is determined by standard dosage method.
KeyWords AITranslate
1刘湘生.高纯银中痕量杂质的ICP—MS测定方法研究[J].分析试验室,2004,(23):293-293.
2戴特AR 李金英 译.电感耦合等离子体质谱分析的应用[M].北京:原子能出版社,1998.170.
3郝红梅.ICP—MS法测定铌酸锂中15种杂质元素[J].分析试验室,2004,(23):247-247.
1夏明星,郑欣,李中奎,王东辉,王峰.电容器用钽铌粉的研究进展[J].材料导报:纳米与新材料专辑,2009,23(2):109-111. 被引量:8
1王东新,李军义,孙本双,任晓,何季麟.钽粉制备新工艺研究进展[J].湖南有色金属,2011,27(3):34-37. 被引量:19
2杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17
3杨国启,孙宇,李仲香,陈学清,林辅坤,程越伟,雒国清.高压高比容钽粉的制备及性能表征[J].湖南有色金属,2017,33(2):43-47. 被引量:3
4李丽君,杨国启,梁宏源,马应会.KCl/NaCl中pH的测定[J].湖南有色金属,2017,33(5):71-73.
5杨国启,李仲香,李慧,马海燕,雒国清,赵春霞.高氮含量电容器级钽粉末的制备工艺研究[J].湖南有色金属,2018,34(5):50-52. 被引量:2
6潘齐凤,阳元江,刘桥,田东斌,刘一峰.超薄型钽浆阳极电容器的制备及性能分析[J].电子器件,2019,42(3):569-573. 被引量:3
7李丽君,雒国清,刘建伟,纪保军.降低钠还原钽粉中铁、镍质量分数的工艺探讨[J].宁夏工程技术,2020,19(3):223-225. 被引量:1
8李仲香,张健康,李慧,陈学清,张洪刚.烧结钽阳极块中氧含量对漏电流的影响[J].云南冶金,2021,50(5):59-63. 被引量:2
1唐德胜,刘英,童坚.磷钼酸铵-孔雀绿-PVA分光光度法测定钽粉中磷[J].分析试验室,2006,25(9):96-98. 被引量:3
2宋金华,戴和平,廖丹.电感耦合等离子质谱法测定钽粉中杂质[J].稀有金属与硬质合金,2012,40(2):68-71. 被引量:6
3ZHANG Han qi, YUAN Xiang lin, LIANG Feng, LIU Si pei, ZHAO Li wei and JIN Qin han ** (Department of Chemistry, Jilin University, Changchun, 130023).Determination of Elements of Groups Ⅲ A and Ⅳ A Using Microwave Plasma Torch Atomic Emission Spectrometry[J].高等学校化学研究:英文版,1997,0(2):34-40.
4张众,郝红梅.火焰原子发射光谱法测定钽粉中钾含量的研究[J].稀有金属与硬质合金,2014,42(5):65-67.
5张颖.电感耦合等离子体发射光谱法测定氟钽酸钾中十四种杂质元素[J].硬质合金,2002,19(2):107-111. 被引量:4
6Deng Mei YE,Jing Hong ZHAO,Han Qi ZHANG,Qin Han JIN(Department of Chemistry, Jilin University, Changchun, 130023).FLOW-INJECTION ON-LINE COLUMN PRECONCENTRATION IN MICROWAVE PLASMA TORCH ATOMIC EMISSION SPECTROMETRY[J].中国化学快报:英文版,1994,5(3):237-238.
7ZHANG Han-qi,YUAN Xiang-lin,YE Dong-mei,ZHAO Xiao-jun and JIN Qin-han (Department Of Chemistry, Jilin University, Changchun, 130023)ZHU Zhi-ping(Department of Chemistry, Northeast Normal University, Changchun, 130024).Determination of Carbon by Means of Microwave Plasma Torch Atomic Emission Spectrometry[J].高等学校化学研究:英文版,1996,0(1):32-36.
8纪新华,张春祥,王林,吴梅.测定钽中碳的红外吸收方法研究[J].原子能科学技术,2004,38(z1):179-181. 被引量:1
9朱艳.高频红外吸收法测定钽粉、铌粉和碳化钽中的碳[J].化学分析计量,2004,13(4):49-50. 被引量:6
10ZHAO Li wei, ZHANG Han qi ** , CAO Yan bo, YANG Wen jun, JIN Qun and JIN Qin han (Department of Chemistry, Jilin University, Changchun, 130023) FU Yao (Foundational Department, Jilin Architecture and Engineering College, Changchun, 130.Determination of Cd,Pb and Sr by Microwave Plasma Torch Atomic Emision Spectrometry Using an Electrothermal Vaporization Sample Introduction System[J].高等学校化学研究:英文版,1998,0(4):22-26.
Basic Information:
DOI:
Chinese Library Classification Number:O657.63[理学—分析化学]
Citation Information:
Description is made of the determination of trace impurity phosphor in Ta powder through ICP-MS. Based on the investigation into the testing condition, hydrofluoric acid-resistant inert feed system, shielded torch and cold plasma technology,phosphor concentration in Ta powder is determined by standard dosage method.
quote
| GB/T 7714-2015 | [1] LIU Shi-yi, YU Xiao-qing, WANG Jing, et al. Determination of Phosphor in Ta Powder through Induction Coupling Plasma Mass Spectrometer[J]. Rare Metals and Cemented Carbides, 2005(4): 35-37. |
| MLA | [1] LIU Shi-yi, et al., "Determination of Phosphor in Ta Powder through Induction Coupling Plasma Mass Spectrometer." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 35-37. |
| APA | [1] LIU Shi-yi, YU Xiao-qing, WANG Jing, & SONG Jin-hua. (2005). Determination of Phosphor in Ta Powder through Induction Coupling Plasma Mass Spectrometer. Rare Metals and Cemented Carbides(4), 35-37. |
| IEEE | [1] LIU Shi-yi, YU Xiao-qing, WANG Jing, and SONG Jin-hua, "Determination of Phosphor in Ta Powder through Induction Coupling Plasma Mass Spectrometer," Rare Metals and Cemented Carbides, no. 4, pp. 35-37, 2005. keywords: {Ta powder;phosphor;shielded torch;ICP-MS} |