daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on Connection and Interface Thermal Stress of W/Cu for Plasma Facing Components of Tokamak Unit AITranslate

Institute of Plasma, Chinese Academy of Sciences;Institute of Plasma, Chinese Academy of Sciences;Institute of Plasma, Chinese Academy of Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Discussion is focused on the following connection methods of W/Cu composite material for plasma facing components of Tokamak unit:electron beam welding,brazing, hot isostatic pressing,sintering and infiltration,vacuum plasma spray. Description is made of the heat load test under electron beam irradiation upon successful connection of PFM with heat sink material. Then stress solution and distribution of W/Cu material under heat load test is also discussed.

KeyWords AITranslate

Tokamak unit plasma facing components W/Cu material connection interface thermal stress

1冯海波,周玉,贾德昌.放电等离子烧结技术的原理及应用[J].材料科学与工艺,2003,11(3):327-331. 被引量:61

2凌云汉,周张键,李江涛,杨大正,葛昌纯.超高压梯度烧结法制备W/Cu功能梯度材料[J].中国有色金属学报,2001,11(4):576-581. 被引量:30

3谌启明,杨靖,单先裕,Jan Westerlund.热等静压技术的发展及应用[J].稀有金属与硬质合金,2003,31(2):33-38. 被引量:39

4凌云汉,白新德,李江涛,葛昌纯.W/Cu功能梯度材料的热应力优化设计[J].稀有金属材料与工程,2003,32(12):976-980. 被引量:21

5周张健,葛昌纯,李江涛.熔渗-焊接法制备W/Cu功能梯度材料的研究[J].金属学报,2000,36(6):655-658. 被引量:25

1郭双全,冯云彪,燕青芝,黎健.偏滤器中钨与异种材料的连接技术研究进展[J].焊接技术,2010,39(9):3-7. 被引量:12

2朱大焕,王坤,王先平,刘长松,方前锋,陈俊凌.偏滤器第一壁W/Cu FGM的热应力模拟与优化设计[J].稀有金属材料与工程,2011,40(9):1658-1661. 被引量:7

3黄华,姜明,马波,吴双,杨志坚,苟富均.钨等离子体平均离化度研究[J].核聚变与等离子体物理,2011,31(4):327-331. 被引量:1

4张俊,朱晓勇,罗来马,罗广南,程继贵,吴玉程.面向等离子体ODS-W复合材料的制备工艺[J].核聚变与等离子体物理,2014,34(4):348-354. 被引量:5

5刘晓,马纪敏,郭海兵.混合堆第一壁中子辐照损伤模拟[J].强激光与粒子束,2015,27(1):250-253. 被引量:3

6宋月鹏,孙祥鸣,李江涛,李倩,陈义祥,郭世斌,高东升.W/Cu梯度材料热应力分析及结构优化设计[J].稀有金属材料与工程,2015,44(3):603-607. 被引量:2

7赵永强,黄生洪,汪卫华.聚变堆第一壁连续W/Cu梯度材料的热工性能优化[J].核聚变与等离子体物理,2016,36(3):247-253. 被引量:1

1鲜铭权,任炬光,张艳丽,刘海兵,柯梦涛.MC模拟计算W-SiC辐射损伤研究[J].核电子学与探测技术,2022,42(6):950-955.

2王健,宋云涛,郭后扬,姚达毛,罗广南,许铁军.EAST偏滤器钨铜单体水冷模块参数优化[J].核聚变与等离子体物理,2013,33(1):72-77. 被引量:1

3闫安英,吴双,何启浩.氩和氪混合物不透明度研究[J].西南民族大学学报:自然科学版,2013,39(6):923-926.

4马运柱,王艳艳,刘文胜,蔡青山.扩散焊接钨/钒/钢体系的界面结构及力学性能[J].焊接学报,2013,34(12):17-20. 被引量:4

5李倩,宋月鹏,曲翠琴,孙祥鸣,凌云汉.高热负荷对钨铜材料工作应力分布影响的研究[J].热处理技术与装备,2013,34(6):37-41.

6郭垚峰,范景莲,蒋冬福,刘涛.细晶W-Cu复合FGM制备及其显微组织特征[J].中南大学学报:自然科学版,2014,45(11):3762-3768. 被引量:1

7刘文胜,刘书华,马运柱,蔡青山,刘昊阳,余强,伍镭.基于镍基微晶钎料的钨/钢真空焊接接头的组织及性能[J].中国有色金属学报,2014,24(12):3051-3058. 被引量:9

8宋月鹏,孙祥鸣,李江涛,李倩,陈义祥,郭世斌,高东升.W/Cu梯度材料热应力分析及结构优化设计[J].稀有金属材料与工程,2015,44(3):603-607. 被引量:2

9李鹏,沈卫平,周雏蕾,徐士亮,王占朋,赵晓琳,张庆玲.具有金刚石/铜中间层W-RAFM模块的制备与评价[J].稀有金属材料与工程,2015,44(3):713-717.

10蒋冬福,范景莲,刘涛,田家敏.纳米复合W-Cu FGM的致密性及界面结合特征[J].粉末冶金材料科学与工程,2016,21(2):326-332.

1尚文静.热等静压(HIP)技术和设备的发展及应用[J].有色冶金设计与研究,2010,31(1):18-21. 被引量:25

2夏明星,张军良,郑欣,王东辉,白润,蔡小梅.Mo-Cu合金的研究进展[J].中国钼业,2013,37(4):34-37. 被引量:4

3王天国,梁启超,覃群.粉末冶金法制备Mo-Cu合金及其性能的研究[J].材料导报,2015,29(10):97-99. 被引量:6

4饶卫红,周瑞敏,张雪平,何林峰,陈永康,爱可可.表面活性剂对电子束制备纳米镍粉的影响[J].机械工程材料,2006,30(10):49-51.

5陈文革.热处理对自力型整体式W-Cu/QCr_(0.5)电触头材料组织与性能的影响[J].粉末冶金技术,2003,21(3):159-162.

6周敏,熊惟皓,姚振华,彭倩筠,黄玉柱.氧化物弥散增强低活化铁素体/马氏体9Cr钢的显微组织与拉伸性能[J].机械工程材料,2011,35(8):62-65.

7潘文强,何浩,李益民.Fe-2Ni/Fe-2Ni-xCr梯度功能材料的共烧结致密化行为和界面强度[J].粉末冶金材料科学与工程,2012,17(5):563-570. 被引量:2

8何忠.钼铜合金制作工艺探讨[J].电工合金,2000(2):4-6. 被引量:5

9谭兆强,李昆,侯海涛,李笃信.注射成形W-Cu及Mo-Cu研究进展[J].材料导报,2007,21(F11):207-209. 被引量:3

10刘如铁,李溪滨.颗粒增强铜基热沉复合材料的研制[J].材料科学与工程,2002,20(4):534-536. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TF146.41[冶金工程—冶金物理化学]

Citation Information:

Discussion is focused on the following connection methods of W/Cu composite material for plasma facing components of Tokamak unit:electron beam welding,brazing, hot isostatic pressing,sintering and infiltration,vacuum plasma spray. Description is made of the heat load test under electron beam irradiation upon successful connection of PFM with heat sink material. Then stress solution and distribution of W/Cu material under heat load test is also discussed.

quote

GB/T 7714-2015 [1] ZHONG Fa-li, CHEN Jun-ling, LI Jian-gang. Research on Connection and Interface Thermal Stress of W/Cu for Plasma Facing Components of Tokamak Unit[J]. Rare Metals and Cemented Carbides, 2005(4): 38-41.
MLA [1] ZHONG Fa-li, et al., "Research on Connection and Interface Thermal Stress of W/Cu for Plasma Facing Components of Tokamak Unit." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 38-41.
APA [1] ZHONG Fa-li, CHEN Jun-ling, & LI Jian-gang. (2005). Research on Connection and Interface Thermal Stress of W/Cu for Plasma Facing Components of Tokamak Unit. Rare Metals and Cemented Carbides(4), 38-41.
IEEE [1] ZHONG Fa-li, CHEN Jun-ling, and LI Jian-gang, "Research on Connection and Interface Thermal Stress of W/Cu for Plasma Facing Components of Tokamak Unit," Rare Metals and Cemented Carbides, no. 4, pp. 38-41, 2005. keywords: {Tokamak unit;plasma facing components;W/Cu material;connection;interface;thermal stress}