The Effect of Sintering Temperature on Mechanical Property of Steel Bonded Cemented Carbide Cladding AITranslate
Abstract AITranslate
Steel-bonded cemented carbide powder mixture(TLMW50) processed by explosive compaction was successfully bonded to the surface of carbon steel through liquid phase sintering. In order to determinate the mechanical property of steel-bonded cemented carbide TLMW50 cladding, study is made of the effect of different sintering temperature at 1 335-1 350℃ on the hardness and bonding strength of the cladding through 3-point bending and hardness test. The test results showed that the hardness of TLMW50 cladding and bonding strength between TLMW50 cladding and carbon steel substrate was increased with the increase of the sintering temperature, a good metallurgical bonding condition in sinter interface and good mechanical property of the cladding were found at 1 350℃.
KeyWords AITranslate
1刘福田,李兆前,黄传真.金属陶瓷复合涂层技术[J].济南大学学报:自然科学版,2002,16(1):84-91. 被引量:31
2王盘鑫.粉末冶金学[M].冶金工业出版社,2003..
1赵一生,高志国,魏世忠,杨涤心.碳钢/钢结硬质合金覆层材料制备及界面分析[J].深圳职业技术学院学报,2009,8(3):67-70. 被引量:1
2赵一生,高志国,杨涤心,魏世忠.热处理对钢结硬质合金TLMW50中复式碳化物形态与分布的影响[J].湖南有色金属,2009,25(3):40-43. 被引量:1
1张煜,赵一生,高志国.钢结硬质合金的研究和发展现状[J].湖南有色金属,2010,26(5):39-41. 被引量:11
2赵一生,魏世忠,高志国.热处理态钢结硬质合金WC相析出微结构分析[J].工具技术,2011(1):31-33. 被引量:3
1高志国,杨涤心,魏世忠,龙锐.热处理对钢结硬质合金TLMW50覆层微观组织的影响[J].金属热处理,2006,31(3):62-64. 被引量:5
2高志国,杨涤心,魏世忠,龙锐.热处理后钢结硬质合金覆层中粘结相组织转变分析[J].硬质合金,2005,22(3):133-135. 被引量:1
3高志国,杨涤心,魏世忠,龙锐.烧结温度对钢结硬质合金覆层/碳素钢结合强度的影响[J].机械工程材料,2005,29(12):26-28. 被引量:1
4高志国,杨涤心,魏世忠,龙锐.热处理对TLMW50烧结覆层组织及磨粒磨损性能的影响[J].硬质合金,2006,23(2):69-74. 被引量:4
5王荣滨,刘翠兰.应用钢结硬质合金,提高模具使用寿命[J].硬质合金,1993,10(4):242-245. 被引量:1
6赵一生,高志国,杨涤心,魏世忠.热处理对钢结硬质合金TLMW50中复式碳化物形态与分布的影响[J].湖南有色金属,2009,25(3):40-43. 被引量:1
7张瓦利,刘薇,敖琪,王新建,吴建生.快淬粉爆炸压制Nd-Fe-B永磁体的性能与结构特征[J].理化检验:物理分册,2006,42(1):1-4.
8王荣滨.活塞销冷挤压凸模失效分析与选材试验[J].模具制造,2005,5(2):74-78.
9赵一生,魏世忠,高志国.热处理态钢结硬质合金WC相析出微结构分析[J].工具技术,2011(1):31-33. 被引量:3
10华寅初,战人瑞.爆炸处理提高43CrNi2MoV钢疲劳强度的试验研究[J].石油机械,1993,21(11):20-26. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]
Citation Information:
Steel-bonded cemented carbide powder mixture(TLMW50) processed by explosive compaction was successfully bonded to the surface of carbon steel through liquid phase sintering. In order to determinate the mechanical property of steel-bonded cemented carbide TLMW50 cladding, study is made of the effect of different sintering temperature at 1 335-1 350℃ on the hardness and bonding strength of the cladding through 3-point bending and hardness test. The test results showed that the hardness of TLMW50 cladding and bonding strength between TLMW50 cladding and carbon steel substrate was increased with the increase of the sintering temperature, a good metallurgical bonding condition in sinter interface and good mechanical property of the cladding were found at 1 350℃.
quote
| GB/T 7714-2015 | [1] GAO Zhi-guo, YANG Di-xin, WEI Shi-zhong, et al. The Effect of Sintering Temperature on Mechanical Property of Steel Bonded Cemented Carbide Cladding[J]. Rare Metals and Cemented Carbides, 2005(4): 23-27. |
| MLA | [1] GAO Zhi-guo, et al., "The Effect of Sintering Temperature on Mechanical Property of Steel Bonded Cemented Carbide Cladding." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 23-27. |
| APA | [1] GAO Zhi-guo, YANG Di-xin, WEI Shi-zhong, & LONG Rui. (2005). The Effect of Sintering Temperature on Mechanical Property of Steel Bonded Cemented Carbide Cladding. Rare Metals and Cemented Carbides(4), 23-27. |
| IEEE | [1] GAO Zhi-guo, YANG Di-xin, WEI Shi-zhong, and LONG Rui, "The Effect of Sintering Temperature on Mechanical Property of Steel Bonded Cemented Carbide Cladding," Rare Metals and Cemented Carbides, no. 4, pp. 23-27, 2005. keywords: {sintering temperature;steel- bonded cemented carbide;TLMW50 cladding;carbon steel;bonding strength;hardness} |