daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on the Influence of Sinter Pile Stuff on Recovery of Sm Metal during La Thermal Reduction of Sm_2O_3 AITranslate

School of Materials Science and Metallurgical Engineering, Inner Mongolia University of Science and Technology;School of Materials Science and Metallurgical Engineering, Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Research is made on the influence of sinter pile stuff on recovery of Sm metal during La thermal reduction of Sm2O3. The recovery of metal Sm in the different parts of the crucible were acquired by the chemistry analysis and hot weightness methods. The porosity of La slag in the differ part pot was measured by hydrostatic weighing,indicating the phenomenon of sinter pile stuff in the pot bottom during La thermal reduction of Sm2O3 ,Based on the test results the sinter pile stuff was analyzed according and optimization test was made with higher recovery.

KeyWords AITranslate

thermal reduction of La Sm2O3 La slag i sinter pile stuff Sm recovery

1王盘鑫.粉末冶金学[M].冶金工业出版社,2003..

1储爱民,姜银举.镧热还原氧化钐过程硅、铝杂质的行为探讨[J].硬质合金,2005,22(3):141-145. 被引量:2

2赵玉萍,储爱民,高春贵.镧热还原氧化钐过程温度梯度及压力梯度与钐收率关系的探讨[J].稀有金属与硬质合金,2008,36(2):19-22. 被引量:2

3成维,黄美松,王志坚,贾帅广,杨露辉.金属镧的制备方法及应用研究现状[J].稀有金属与硬质合金,2014,42(1):62-65. 被引量:7

4包香春,张秀艳,李建亭,李净岩.火焰原子吸收光谱法测定镧热还原稀土金属及熔盐电解稀土金属中锂含量[J].稀土,2020,41(5):93-98.

1崔有为,李杰,杜兆富.镧、铈改性沸石对污水除磷性能和机制的比较研究[J].中国稀土学报,2016,34(4):460-468. 被引量:16

2梁勇,邹瑜,刘玉城,黎永康,梁鑫,廖春发.碳酸钠焙烧-酸浸法从钙热还原稀土冶炼渣中提取稀土的研究[J].有色金属工程,2018,8(1):53-56. 被引量:3

3郝占忠,许林成.钐钆富集物直接还原蒸馏制备金属钐[J].有色金属:冶炼部分,2018(3):69-73.

4伍永福,薛凯,刘中兴,吴文远,边雪.LaCl_3·7H_2O脱水过程研究[J].稀有金属与硬质合金,2018,46(5):46-49.

5刘泽芳,刘永畅,巫圣喜,张贵清,曹佐英,曾理,关文娟,李青刚.草酸盐沉淀法制备不同形貌粒度的La2O3粉体[J].中国稀土学报,2020,38(6):798-807. 被引量:4

6熊志伟,刘爱民,刘玉宝,王旭,石忠宁.La_(2)O_(3)在LiF⁃NaF熔盐体系中的溶解行为[J].材料与冶金学报,2022,21(3):167-171.

7康佳,闫奇操,于兵,刘玉宝,陈国华,赵二雄,张全军,黄海涛.LaCl_(3)-KCl熔盐体系物化性质研究[J].有色金属科学与工程,2022,13(3):145-151. 被引量:1

8张先恒,赵二雄,苗旭晨,董岳阳.镧热还原法制备金属钐的研究[J].金属功能材料,2022,29(3):85-89.

9康佳,闫奇操,刘玉宝,于兵,赵二雄,张全军,黄海涛.熔盐电解法制备镧合金的研究进展[J].矿产综合利用,2022(6):110-115.

1储爱民,姜银举,赵玉萍.镧热还原氧化钐过程动力学控速环节的探索[J].江西有色金属,2005,19(2):26-27. 被引量:4

2赵玉萍,储爱民,高春贵.镧热还原氧化钐过程温度梯度及压力梯度与钐收率关系的探讨[J].稀有金属与硬质合金,2008,36(2):19-22. 被引量:2

3储爱民,姜银举.镧热还原氧化钐过程镧的表面富集现象探索[J].湖南有色金属,2005,21(5):22-23.

4储爱民,高春贵,蒋学智.镧热还原氧化钐过程镧的非平衡扩散的研究[J].有色金属:冶炼部分,2008(5):32-34. 被引量:2

5吕恩保,刘兴山.镧热和铈热还原法制取金属钐影响因素的研究[J].江西有色金属,1990,4(4):9-13. 被引量:11

6姜银举,储爱民.镧热还原氧化钐过程冶金动力学分析[J].稀土,2006,27(2):49-52. 被引量:9

7储爱民,姜银举.镧热还原氧化钐过程镧在镧渣表面的富集研究[J].稀有金属快报,2005,24(8):22-24. 被引量:2

8吴炳乾,张耀文.镧热还原铥镜镥富集物时杂质行为的讨论[J].江西有色金属,1997,11(2):34-37. 被引量:1

9静水矿业公司三季度铂族金属产量增加[J].中国金属通报,2009(44):13-13.

10姬长征(编译).静水矿业公司第二季度铂族金属产量下滑18.2%[J].中国贵金属,2010(8):76-77.

Basic Information:

DOI:

Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]

Citation Information:

Research is made on the influence of sinter pile stuff on recovery of Sm metal during La thermal reduction of Sm2O3. The recovery of metal Sm in the different parts of the crucible were acquired by the chemistry analysis and hot weightness methods. The porosity of La slag in the differ part pot was measured by hydrostatic weighing,indicating the phenomenon of sinter pile stuff in the pot bottom during La thermal reduction of Sm2O3 ,Based on the test results the sinter pile stuff was analyzed according and optimization test was made with higher recovery.

quote

GB/T 7714-2015 [1] JIANG Yin-ju, CHU Ai-min. Research on the Influence of Sinter Pile Stuff on Recovery of Sm Metal during La Thermal Reduction of Sm_2O_3[J]. Rare Metals and Cemented Carbides, 2005(4): 19-22.
MLA [1] JIANG Yin-ju, and CHU Ai-min. "Research on the Influence of Sinter Pile Stuff on Recovery of Sm Metal during La Thermal Reduction of Sm_2O_3." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 19-22.
APA [1] JIANG Yin-ju, & CHU Ai-min. (2005). Research on the Influence of Sinter Pile Stuff on Recovery of Sm Metal during La Thermal Reduction of Sm_2O_3. Rare Metals and Cemented Carbides(4), 19-22.
IEEE [1] JIANG Yin-ju and CHU Ai-min, "Research on the Influence of Sinter Pile Stuff on Recovery of Sm Metal during La Thermal Reduction of Sm_2O_3," Rare Metals and Cemented Carbides, no. 4, pp. 19-22, 2005. keywords: {thermal reduction of La;Sm2O3;La slag i sinter pile stuff;Sm recovery}