Experimental Study on Sb Removal from Ta-Nb Ore Decomposition Solution by Reduction with Magnesium Powder and Extraction with 2-Octanol AITranslate
Abstract AITranslate
In view of Sb valence,the extraction performance difference of 2-octanol for Sb(Ⅲ)and Sb(Ⅴ)was studied.It is verified that Sb(Ⅴ)extraction is easier with 2-octanol under the same extraction conditions.Based on the above results,Sb in Ta-Nb ore decomposition solution was reduced with a certain amount of magnesium powder,resulting in transformation of high valence state of Sb into low valence state of Sb and Sb separation from Ta and Nb.The experimental results show that to control Sb content within20×10^-6 in the product of niobium pentoxide,reduction conditions should be 10g/L magnesium powder dosage and 5hreaction duration.
KeyWords AITranslate
1韩建设,周勇.钽铌萃取分离工艺与设备进展[J].稀有金属与硬质合金,2004,32(2):15-20. 被引量:16
2张伟宁,李静,刘军.用分步沉积法去除Nb(OH)_5/Ta(OH)_5中Ti,Sb等金属杂质的工艺研究[J].宁夏工程技术,2002,1(3):216-217. 被引量:12
3Walter Bludssus, Uwe Bohmke, Karlheinz Reichert. Process for removing antimony from hydrofluoric acid solutions which contain Ta/Nb[P]. US Pat.. 5908489A, 1999-06-01.
4Havery Stewart, Edward Mosheim C. Process for separa- ting antimony from columbium solutions[P]. US Pat: 4518570,1985-05-21.
1梁昌明,张和鹏,郭永忠.MIBK萃取法从铌液中除锑制取高纯氧化铌的实验研究[J].稀有金属与硬质合金,2017,45(1):1-3. 被引量:4
2张何鹏,孙思聪,梅龙宝,梁粱.调整价态萃取-陶瓷膜过滤联合除锑制取超高纯氧化铌[J].有色金属科学与工程,2020,11(2):71-75. 被引量:1
1朱国荣.降低湿法制砷工艺液相锑浓度的实验研究[J].铜业工程,2019,0(3):46-48.
2张何鹏,孙思聪,梅龙宝,梁粱.调整价态萃取-陶瓷膜过滤联合除锑制取超高纯氧化铌[J].有色金属科学与工程,2020,11(2):71-75. 被引量:1
3鲁东,喻文斌,王诗海,张伟宁,郭洪范.结晶法和萃取法制备高纯氧化铌的研究[J].广州化工,2020,48(20):53-54. 被引量:1
4胡向平,李建新,杨斌,沈义梅,徐光以,许佩琪,荣幸,孟繁艳.Nb2O5原料对H-ZF类高折射率玻璃透过性能的影响因素[J].材料导报,2020,34(S02):138-141.
5王鹏,张军战,张颖,覃枫,杨明辉,陈红侠.催化剂对硅氧碳多孔陶瓷结构与性能的影响[J].稀有金属,2022,46(12):1573-1579.
1龙叔仲,谢忠.沸腾氯化从锡渣及钨钽铌矿富集铌钽综合回收钨、锡有价金属的研究[J].稀有金属,1991,15(5):333-338. 被引量:6
2胡益清,肖成西.从含铌钽的钛矿中回收铌钽[J].稀有金属与硬质合金,1993,21(1):29-32. 被引量:2
3赵明智,张劲.钛钽铌矿强化分解工艺的研究[J].稀有金属与硬质合金,2004,32(4):25-28. 被引量:2
4杨继红.低品位难分解钽铌矿加压酸分解工艺的试验研究[J].稀有金属与硬质合金,2013,41(3):4-7. 被引量:1
5李贺,王海北,王玉芳.复杂钼精矿湿法冶金工艺研究[J].有色金属:冶炼部分,2013(7):31-34. 被引量:6
6许亮,陈冬英,杨新华,常德民,周洁英,欧阳红.钨钽铌粗精矿碱分解液萃取试验研究[J].中国钨业,2014,29(1):48-51.
7周洁英,杨新华,洪侃,赖兰萍,陈冬英.从稀土分解液中连续去除铁、铝[J].湿法冶金,2016,35(6):513-516. 被引量:8
8何长仪,刘志明,张浩军.钽铌矿湿法冶炼含氟废气的治理[J].有色金属,1998,50(4):141-142. 被引量:14
9梁昌明,张和鹏,郭永忠.MIBK萃取法从铌液中除锑制取高纯氧化铌的实验研究[J].稀有金属与硬质合金,2017,45(1):1-3. 被引量:4
10周宏明,郑诗礼,张懿.KOH亚熔盐浸出低品位难分解钽铌矿的实验[J].过程工程学报,2003,3(5):459-463. 被引量:22
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
In view of Sb valence,the extraction performance difference of 2-octanol for Sb(Ⅲ)and Sb(Ⅴ)was studied.It is verified that Sb(Ⅴ)extraction is easier with 2-octanol under the same extraction conditions.Based on the above results,Sb in Ta-Nb ore decomposition solution was reduced with a certain amount of magnesium powder,resulting in transformation of high valence state of Sb into low valence state of Sb and Sb separation from Ta and Nb.The experimental results show that to control Sb content within20×10^-6 in the product of niobium pentoxide,reduction conditions should be 10g/L magnesium powder dosage and 5hreaction duration.
quote
| GB/T 7714-2015 | [1] HU Gen-huo, GUO Yong-zhong, SONG Jin-hua. Experimental Study on Sb Removal from Ta-Nb Ore Decomposition Solution by Reduction with Magnesium Powder and Extraction with 2-Octanol[J]. Rare Metals and Cemented Carbides, 2014(3): 12-14. |
| MLA | [1] HU Gen-huo, et al., "Experimental Study on Sb Removal from Ta-Nb Ore Decomposition Solution by Reduction with Magnesium Powder and Extraction with 2-Octanol." Rare Metals and Cemented Carbides, no. 3, 2014, pp. 12-14. |
| APA | [1] HU Gen-huo, GUO Yong-zhong, & SONG Jin-hua. (2014). Experimental Study on Sb Removal from Ta-Nb Ore Decomposition Solution by Reduction with Magnesium Powder and Extraction with 2-Octanol. Rare Metals and Cemented Carbides(3), 12-14. |
| IEEE | [1] HU Gen-huo, GUO Yong-zhong, and SONG Jin-hua, "Experimental Study on Sb Removal from Ta-Nb Ore Decomposition Solution by Reduction with Magnesium Powder and Extraction with 2-Octanol," Rare Metals and Cemented Carbides, no. 3, pp. 12-14, 2014. keywords: {Sb removal;reduction with magnesium powder;extraction with 2-octanol;Ta-Nb ore decomposition solution;Sb(Ⅲ);Sb(Ⅴ)} |